Method for preparing stoneware archaized brick from multi-source ceramic solid wastes

The invention discloses a method for preparing a stoneware archaized brick from multi-source ceramic solid wastes. A green body is prepared from the following main raw materials in percentage by weight: 5 to 10 percent of glazed slag, 20 to 40 percent of sewage mud, 10 to 60 percent of Longshan red...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DING YINGMEI, LIU HAIGUANG, ZENG FANPING, LIANG YAOLONG, CAI SANLIANG, LIANG TONGCAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DING YINGMEI
LIU HAIGUANG
ZENG FANPING
LIANG YAOLONG
CAI SANLIANG
LIANG TONGCAN
description The invention discloses a method for preparing a stoneware archaized brick from multi-source ceramic solid wastes. A green body is prepared from the following main raw materials in percentage by weight: 5 to 10 percent of glazed slag, 20 to 40 percent of sewage mud, 10 to 60 percent of Longshan red sand, 5 to 20 percent of Xiongda stone flour and 10 to 20 percent of estuary black mud; the one-timefiring temperature of the green body is 1175 to 1215 DEG C, and the firing period is 50 to 65 minutes. A large amount of residual stacked wastes in a ceramic factory and low-quality minerals with a low price are taken as raw materials of the archaized brick, and the production cost is obviously lower than that of common ceramic tiles on the market. Meanwhile, due to sufficient stock of wastes andlow-quality raw materials, fluctuation in the production process is reduced, the superior product rate is increased, and the production cost of the archaized brick is successfully reduced. The sale price range is wide, the ma
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111792914A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111792914A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111792914A3</originalsourceid><addsrcrecordid>eNqNyjEOgkAQBVAaC6PeYTwAxaqJoTREY6OV1mRcPrARmM3MEhJPb-MBrF7zltnzhtRJTY0oRUVkDWNLlmTEzApi9R2HD2p6afBvalQGGqY-hdxkUg_yUB6CJ5M-1DSzJdg6WzTcGzY_V9n2cn6U1xxRKlhkjxGpKu_OuWOxK9zhtP_nfAETozmj</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing stoneware archaized brick from multi-source ceramic solid wastes</title><source>esp@cenet</source><creator>DING YINGMEI ; LIU HAIGUANG ; ZENG FANPING ; LIANG YAOLONG ; CAI SANLIANG ; LIANG TONGCAN</creator><creatorcontrib>DING YINGMEI ; LIU HAIGUANG ; ZENG FANPING ; LIANG YAOLONG ; CAI SANLIANG ; LIANG TONGCAN</creatorcontrib><description>The invention discloses a method for preparing a stoneware archaized brick from multi-source ceramic solid wastes. A green body is prepared from the following main raw materials in percentage by weight: 5 to 10 percent of glazed slag, 20 to 40 percent of sewage mud, 10 to 60 percent of Longshan red sand, 5 to 20 percent of Xiongda stone flour and 10 to 20 percent of estuary black mud; the one-timefiring temperature of the green body is 1175 to 1215 DEG C, and the firing period is 50 to 65 minutes. A large amount of residual stacked wastes in a ceramic factory and low-quality minerals with a low price are taken as raw materials of the archaized brick, and the production cost is obviously lower than that of common ceramic tiles on the market. Meanwhile, due to sufficient stock of wastes andlow-quality raw materials, fluctuation in the production process is reduced, the superior product rate is increased, and the production cost of the archaized brick is successfully reduced. The sale price range is wide, the ma</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; LIME, MAGNESIA ; METALLURGY ; MINERAL OR SLAG WOOL ; REFRACTORIES ; SLAG ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS ; TREATMENT OF NATURAL STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201020&amp;DB=EPODOC&amp;CC=CN&amp;NR=111792914A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20201020&amp;DB=EPODOC&amp;CC=CN&amp;NR=111792914A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DING YINGMEI</creatorcontrib><creatorcontrib>LIU HAIGUANG</creatorcontrib><creatorcontrib>ZENG FANPING</creatorcontrib><creatorcontrib>LIANG YAOLONG</creatorcontrib><creatorcontrib>CAI SANLIANG</creatorcontrib><creatorcontrib>LIANG TONGCAN</creatorcontrib><title>Method for preparing stoneware archaized brick from multi-source ceramic solid wastes</title><description>The invention discloses a method for preparing a stoneware archaized brick from multi-source ceramic solid wastes. A green body is prepared from the following main raw materials in percentage by weight: 5 to 10 percent of glazed slag, 20 to 40 percent of sewage mud, 10 to 60 percent of Longshan red sand, 5 to 20 percent of Xiongda stone flour and 10 to 20 percent of estuary black mud; the one-timefiring temperature of the green body is 1175 to 1215 DEG C, and the firing period is 50 to 65 minutes. A large amount of residual stacked wastes in a ceramic factory and low-quality minerals with a low price are taken as raw materials of the archaized brick, and the production cost is obviously lower than that of common ceramic tiles on the market. Meanwhile, due to sufficient stock of wastes andlow-quality raw materials, fluctuation in the production process is reduced, the superior product rate is increased, and the production cost of the archaized brick is successfully reduced. The sale price range is wide, the ma</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEOgkAQBVAaC6PeYTwAxaqJoTREY6OV1mRcPrARmM3MEhJPb-MBrF7zltnzhtRJTY0oRUVkDWNLlmTEzApi9R2HD2p6afBvalQGGqY-hdxkUg_yUB6CJ5M-1DSzJdg6WzTcGzY_V9n2cn6U1xxRKlhkjxGpKu_OuWOxK9zhtP_nfAETozmj</recordid><startdate>20201020</startdate><enddate>20201020</enddate><creator>DING YINGMEI</creator><creator>LIU HAIGUANG</creator><creator>ZENG FANPING</creator><creator>LIANG YAOLONG</creator><creator>CAI SANLIANG</creator><creator>LIANG TONGCAN</creator><scope>EVB</scope></search><sort><creationdate>20201020</creationdate><title>Method for preparing stoneware archaized brick from multi-source ceramic solid wastes</title><author>DING YINGMEI ; LIU HAIGUANG ; ZENG FANPING ; LIANG YAOLONG ; CAI SANLIANG ; LIANG TONGCAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111792914A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>DING YINGMEI</creatorcontrib><creatorcontrib>LIU HAIGUANG</creatorcontrib><creatorcontrib>ZENG FANPING</creatorcontrib><creatorcontrib>LIANG YAOLONG</creatorcontrib><creatorcontrib>CAI SANLIANG</creatorcontrib><creatorcontrib>LIANG TONGCAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DING YINGMEI</au><au>LIU HAIGUANG</au><au>ZENG FANPING</au><au>LIANG YAOLONG</au><au>CAI SANLIANG</au><au>LIANG TONGCAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing stoneware archaized brick from multi-source ceramic solid wastes</title><date>2020-10-20</date><risdate>2020</risdate><abstract>The invention discloses a method for preparing a stoneware archaized brick from multi-source ceramic solid wastes. A green body is prepared from the following main raw materials in percentage by weight: 5 to 10 percent of glazed slag, 20 to 40 percent of sewage mud, 10 to 60 percent of Longshan red sand, 5 to 20 percent of Xiongda stone flour and 10 to 20 percent of estuary black mud; the one-timefiring temperature of the green body is 1175 to 1215 DEG C, and the firing period is 50 to 65 minutes. A large amount of residual stacked wastes in a ceramic factory and low-quality minerals with a low price are taken as raw materials of the archaized brick, and the production cost is obviously lower than that of common ceramic tiles on the market. Meanwhile, due to sufficient stock of wastes andlow-quality raw materials, fluctuation in the production process is reduced, the superior product rate is increased, and the production cost of the archaized brick is successfully reduced. The sale price range is wide, the ma</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN111792914A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
LIME, MAGNESIA
METALLURGY
MINERAL OR SLAG WOOL
REFRACTORIES
SLAG
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
TREATMENT OF NATURAL STONE
title Method for preparing stoneware archaized brick from multi-source ceramic solid wastes
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T22%3A04%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DING%20YINGMEI&rft.date=2020-10-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111792914A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true