Mine slag-based aerated building block and preparation method thereof

The invention discloses a mine slag based aerated building block and a preparation method thereof. The method comprises the following steps: carrying out ball milling on mine slag, quick lime, basaltand water, screening with a 100 [mu]m sieve mesh to obtain a prefabricated material, adding cement an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JIANG WENNAN, GAO QIN, MENG MENG, YU YAWEN, MENG WEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JIANG WENNAN
GAO QIN
MENG MENG
YU YAWEN
MENG WEI
description The invention discloses a mine slag based aerated building block and a preparation method thereof. The method comprises the following steps: carrying out ball milling on mine slag, quick lime, basaltand water, screening with a 100 [mu]m sieve mesh to obtain a prefabricated material, adding cement and gypsum into the prefabricated material, and uniformly stirring to obtain slurry; stirring sodiumbentonite, ammonium bicarbonate powder, an emulsifier and water, performing spray drying, heating at 60-70 DEG C for 1-2 h, adding cationic starch and water, grinding, then performing activation at 105-115 DEG C for 20-30 min, drying, and screening with a 100-mesh sieve so as to obtain a cationic starch-bentonite complex; and uniformly mixing the slurry, the cationic starch-bentonite complex, a sulfonated melamine formaldehyde resin, lignin fibers and water, carrying out mold pouring at a pouring temperature of 40-45 DEG C, carrying out pre-curing for 20-40 min, demolding, cutting, and carrying out steam curing to obta
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111440005A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111440005A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111440005A3</originalsourceid><addsrcrecordid>eNrjZHD1zcxLVSjOSUzXTUosTk1RSEwtSiwB0kmlmTkpmXnpCkk5-cnZCol5KQoFRakFiUDZzPw8hdzUkoz8FIWSjNSi1Pw0HgbWtMSc4lReKM3NoOjmGuLsoZtakB-fWlyQmJyal1oS7-xnaGhoYmJgYGDqaEyMGgDJNjLd</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Mine slag-based aerated building block and preparation method thereof</title><source>esp@cenet</source><creator>JIANG WENNAN ; GAO QIN ; MENG MENG ; YU YAWEN ; MENG WEI</creator><creatorcontrib>JIANG WENNAN ; GAO QIN ; MENG MENG ; YU YAWEN ; MENG WEI</creatorcontrib><description>The invention discloses a mine slag based aerated building block and a preparation method thereof. The method comprises the following steps: carrying out ball milling on mine slag, quick lime, basaltand water, screening with a 100 [mu]m sieve mesh to obtain a prefabricated material, adding cement and gypsum into the prefabricated material, and uniformly stirring to obtain slurry; stirring sodiumbentonite, ammonium bicarbonate powder, an emulsifier and water, performing spray drying, heating at 60-70 DEG C for 1-2 h, adding cationic starch and water, grinding, then performing activation at 105-115 DEG C for 20-30 min, drying, and screening with a 100-mesh sieve so as to obtain a cationic starch-bentonite complex; and uniformly mixing the slurry, the cationic starch-bentonite complex, a sulfonated melamine formaldehyde resin, lignin fibers and water, carrying out mold pouring at a pouring temperature of 40-45 DEG C, carrying out pre-curing for 20-40 min, demolding, cutting, and carrying out steam curing to obta</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200724&amp;DB=EPODOC&amp;CC=CN&amp;NR=111440005A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200724&amp;DB=EPODOC&amp;CC=CN&amp;NR=111440005A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JIANG WENNAN</creatorcontrib><creatorcontrib>GAO QIN</creatorcontrib><creatorcontrib>MENG MENG</creatorcontrib><creatorcontrib>YU YAWEN</creatorcontrib><creatorcontrib>MENG WEI</creatorcontrib><title>Mine slag-based aerated building block and preparation method thereof</title><description>The invention discloses a mine slag based aerated building block and a preparation method thereof. The method comprises the following steps: carrying out ball milling on mine slag, quick lime, basaltand water, screening with a 100 [mu]m sieve mesh to obtain a prefabricated material, adding cement and gypsum into the prefabricated material, and uniformly stirring to obtain slurry; stirring sodiumbentonite, ammonium bicarbonate powder, an emulsifier and water, performing spray drying, heating at 60-70 DEG C for 1-2 h, adding cationic starch and water, grinding, then performing activation at 105-115 DEG C for 20-30 min, drying, and screening with a 100-mesh sieve so as to obtain a cationic starch-bentonite complex; and uniformly mixing the slurry, the cationic starch-bentonite complex, a sulfonated melamine formaldehyde resin, lignin fibers and water, carrying out mold pouring at a pouring temperature of 40-45 DEG C, carrying out pre-curing for 20-40 min, demolding, cutting, and carrying out steam curing to obta</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD1zcxLVSjOSUzXTUosTk1RSEwtSiwB0kmlmTkpmXnpCkk5-cnZCol5KQoFRakFiUDZzPw8hdzUkoz8FIWSjNSi1Pw0HgbWtMSc4lReKM3NoOjmGuLsoZtakB-fWlyQmJyal1oS7-xnaGhoYmJgYGDqaEyMGgDJNjLd</recordid><startdate>20200724</startdate><enddate>20200724</enddate><creator>JIANG WENNAN</creator><creator>GAO QIN</creator><creator>MENG MENG</creator><creator>YU YAWEN</creator><creator>MENG WEI</creator><scope>EVB</scope></search><sort><creationdate>20200724</creationdate><title>Mine slag-based aerated building block and preparation method thereof</title><author>JIANG WENNAN ; GAO QIN ; MENG MENG ; YU YAWEN ; MENG WEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111440005A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>JIANG WENNAN</creatorcontrib><creatorcontrib>GAO QIN</creatorcontrib><creatorcontrib>MENG MENG</creatorcontrib><creatorcontrib>YU YAWEN</creatorcontrib><creatorcontrib>MENG WEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JIANG WENNAN</au><au>GAO QIN</au><au>MENG MENG</au><au>YU YAWEN</au><au>MENG WEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Mine slag-based aerated building block and preparation method thereof</title><date>2020-07-24</date><risdate>2020</risdate><abstract>The invention discloses a mine slag based aerated building block and a preparation method thereof. The method comprises the following steps: carrying out ball milling on mine slag, quick lime, basaltand water, screening with a 100 [mu]m sieve mesh to obtain a prefabricated material, adding cement and gypsum into the prefabricated material, and uniformly stirring to obtain slurry; stirring sodiumbentonite, ammonium bicarbonate powder, an emulsifier and water, performing spray drying, heating at 60-70 DEG C for 1-2 h, adding cationic starch and water, grinding, then performing activation at 105-115 DEG C for 20-30 min, drying, and screening with a 100-mesh sieve so as to obtain a cationic starch-bentonite complex; and uniformly mixing the slurry, the cationic starch-bentonite complex, a sulfonated melamine formaldehyde resin, lignin fibers and water, carrying out mold pouring at a pouring temperature of 40-45 DEG C, carrying out pre-curing for 20-40 min, demolding, cutting, and carrying out steam curing to obta</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN111440005A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Mine slag-based aerated building block and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T19%3A21%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JIANG%20WENNAN&rft.date=2020-07-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111440005A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true