Preparation method of high-temperature nylon
The invention discloses a preparation method of high-temperature nylon, which comprises the following steps: (1) carrying out water-phase polymerization reaction, namely, proportionally adding binaryacid, diamine, a reaction assistant and deionized water into a high-pressure reaction kettle to obtai...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG XIANWEN HU SANYOU HUANG HUAPENG TAN LIN |
description | The invention discloses a preparation method of high-temperature nylon, which comprises the following steps: (1) carrying out water-phase polymerization reaction, namely, proportionally adding binaryacid, diamine, a reaction assistant and deionized water into a high-pressure reaction kettle to obtain a high-temperature nylon precursor; and (2) adding the high-temperature nylon precursor into a solid-phase polymerization reactor, exhausting air in the reactor, introducing an exhaust valve into water, carrying out liquid sealing, introducing inert gas, keeping the pressure in the reactor at normal pressure, raising the temperature in the reactor to 230-300 DEG C at a constant speed within a period of time, slowly reducing the vacuum in the reactor to 0-60Pa within a period of time after thereaction for a period of time, continuing the reaction for a period of time, and performing discharging to obtain the product. According to the preparation method, the high-temperature nylon precursor with specific relative v |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111303408A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111303408A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111303408A3</originalsourceid><addsrcrecordid>eNrjZNAJKEotSCxKLMnMz1PITS3JyE9RyE9TyMhMz9AtSc0tSAVKlRalKuRV5uTn8TCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_Q0NDYwNjEwMLR2Ni1AAAs5gqAw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of high-temperature nylon</title><source>esp@cenet</source><creator>WANG XIANWEN ; HU SANYOU ; HUANG HUAPENG ; TAN LIN</creator><creatorcontrib>WANG XIANWEN ; HU SANYOU ; HUANG HUAPENG ; TAN LIN</creatorcontrib><description>The invention discloses a preparation method of high-temperature nylon, which comprises the following steps: (1) carrying out water-phase polymerization reaction, namely, proportionally adding binaryacid, diamine, a reaction assistant and deionized water into a high-pressure reaction kettle to obtain a high-temperature nylon precursor; and (2) adding the high-temperature nylon precursor into a solid-phase polymerization reactor, exhausting air in the reactor, introducing an exhaust valve into water, carrying out liquid sealing, introducing inert gas, keeping the pressure in the reactor at normal pressure, raising the temperature in the reactor to 230-300 DEG C at a constant speed within a period of time, slowly reducing the vacuum in the reactor to 0-60Pa within a period of time after thereaction for a period of time, continuing the reaction for a period of time, and performing discharging to obtain the product. According to the preparation method, the high-temperature nylon precursor with specific relative v</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20200619&DB=EPODOC&CC=CN&NR=111303408A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20200619&DB=EPODOC&CC=CN&NR=111303408A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG XIANWEN</creatorcontrib><creatorcontrib>HU SANYOU</creatorcontrib><creatorcontrib>HUANG HUAPENG</creatorcontrib><creatorcontrib>TAN LIN</creatorcontrib><title>Preparation method of high-temperature nylon</title><description>The invention discloses a preparation method of high-temperature nylon, which comprises the following steps: (1) carrying out water-phase polymerization reaction, namely, proportionally adding binaryacid, diamine, a reaction assistant and deionized water into a high-pressure reaction kettle to obtain a high-temperature nylon precursor; and (2) adding the high-temperature nylon precursor into a solid-phase polymerization reactor, exhausting air in the reactor, introducing an exhaust valve into water, carrying out liquid sealing, introducing inert gas, keeping the pressure in the reactor at normal pressure, raising the temperature in the reactor to 230-300 DEG C at a constant speed within a period of time, slowly reducing the vacuum in the reactor to 0-60Pa within a period of time after thereaction for a period of time, continuing the reaction for a period of time, and performing discharging to obtain the product. According to the preparation method, the high-temperature nylon precursor with specific relative v</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNAJKEotSCxKLMnMz1PITS3JyE9RyE9TyMhMz9AtSc0tSAVKlRalKuRV5uTn8TCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_Q0NDYwNjEwMLR2Ni1AAAs5gqAw</recordid><startdate>20200619</startdate><enddate>20200619</enddate><creator>WANG XIANWEN</creator><creator>HU SANYOU</creator><creator>HUANG HUAPENG</creator><creator>TAN LIN</creator><scope>EVB</scope></search><sort><creationdate>20200619</creationdate><title>Preparation method of high-temperature nylon</title><author>WANG XIANWEN ; HU SANYOU ; HUANG HUAPENG ; TAN LIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111303408A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG XIANWEN</creatorcontrib><creatorcontrib>HU SANYOU</creatorcontrib><creatorcontrib>HUANG HUAPENG</creatorcontrib><creatorcontrib>TAN LIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG XIANWEN</au><au>HU SANYOU</au><au>HUANG HUAPENG</au><au>TAN LIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of high-temperature nylon</title><date>2020-06-19</date><risdate>2020</risdate><abstract>The invention discloses a preparation method of high-temperature nylon, which comprises the following steps: (1) carrying out water-phase polymerization reaction, namely, proportionally adding binaryacid, diamine, a reaction assistant and deionized water into a high-pressure reaction kettle to obtain a high-temperature nylon precursor; and (2) adding the high-temperature nylon precursor into a solid-phase polymerization reactor, exhausting air in the reactor, introducing an exhaust valve into water, carrying out liquid sealing, introducing inert gas, keeping the pressure in the reactor at normal pressure, raising the temperature in the reactor to 230-300 DEG C at a constant speed within a period of time, slowly reducing the vacuum in the reactor to 0-60Pa within a period of time after thereaction for a period of time, continuing the reaction for a period of time, and performing discharging to obtain the product. According to the preparation method, the high-temperature nylon precursor with specific relative v</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN111303408A |
source | esp@cenet |
subjects | CHEMISTRY COMPOSITIONS BASED THEREON MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP |
title | Preparation method of high-temperature nylon |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-25T09%3A27%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20XIANWEN&rft.date=2020-06-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111303408A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |