Preparation method of dopamine modified graphene insensitive doped nitramine oxidant

The invention relates to a preparation method of a dopamine modified graphene insensitive doped nitramine oxidizing agent. The preparation method comprises the following steps: dissolving ammonium nitrate crystals in nearly saturated dimethyl sulfoxide DMSO to obtain a DMSO solution of the ammonium...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HUANG BINBIN, XUE ZHIHUA, HE WEI, LYU JIEYAO, YAN QILONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HUANG BINBIN
XUE ZHIHUA
HE WEI
LYU JIEYAO
YAN QILONG
description The invention relates to a preparation method of a dopamine modified graphene insensitive doped nitramine oxidizing agent. The preparation method comprises the following steps: dissolving ammonium nitrate crystals in nearly saturated dimethyl sulfoxide DMSO to obtain a DMSO solution of the ammonium nitrate crystals; adding a graphene oxide suspension into the DMSO solution, and adding a dopamine ethanol solution to obtain a mixed solution containing ammonium nitrate crystals, DA and the graphene oxide suspension; and dropwise adding H2O2 to obtain a mixed solution containing polydopamine PDA,so as to obtain the dopamine modified graphene insensitive doped nitramine oxidizing agent of a GO doped ammonium nitrate crystal energetic material taking PDA as an interface material. The preparation method has the beneficial effects that the safety risk in the operation process is reduced by introducing graphene oxide; and an ammonium nitrate energetic material with relatively high stability, namely, a graphene oxide d
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111285748A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111285748A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111285748A3</originalsourceid><addsrcrecordid>eNrjZAgJKEotSCxKLMnMz1PITS3JyE9RyE9TSMkvSMzNzEtVyM1PyUzLTE1RSC9KLMhIBYpk5hWn5hVnlmSWpYKUAaXyMkuKIKrzKzJTEvNKeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYjLQoJJ4Zz9DQ0MjC1NzEwtHY2LUAAD0QjmT</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of dopamine modified graphene insensitive doped nitramine oxidant</title><source>esp@cenet</source><creator>HUANG BINBIN ; XUE ZHIHUA ; HE WEI ; LYU JIEYAO ; YAN QILONG</creator><creatorcontrib>HUANG BINBIN ; XUE ZHIHUA ; HE WEI ; LYU JIEYAO ; YAN QILONG</creatorcontrib><description>The invention relates to a preparation method of a dopamine modified graphene insensitive doped nitramine oxidizing agent. The preparation method comprises the following steps: dissolving ammonium nitrate crystals in nearly saturated dimethyl sulfoxide DMSO to obtain a DMSO solution of the ammonium nitrate crystals; adding a graphene oxide suspension into the DMSO solution, and adding a dopamine ethanol solution to obtain a mixed solution containing ammonium nitrate crystals, DA and the graphene oxide suspension; and dropwise adding H2O2 to obtain a mixed solution containing polydopamine PDA,so as to obtain the dopamine modified graphene insensitive doped nitramine oxidizing agent of a GO doped ammonium nitrate crystal energetic material taking PDA as an interface material. The preparation method has the beneficial effects that the safety risk in the operation process is reduced by introducing graphene oxide; and an ammonium nitrate energetic material with relatively high stability, namely, a graphene oxide d</description><language>chi ; eng</language><subject>CHEMISTRY ; EXPLOSIVES ; EXPLOSIVES OR THERMIC COMPOSITIONS ; MANUFACTURE THEREOF ; MATCHES ; METALLURGY ; USE OF SINGLE SUBSTANCES AS EXPLOSIVES</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200616&amp;DB=EPODOC&amp;CC=CN&amp;NR=111285748A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200616&amp;DB=EPODOC&amp;CC=CN&amp;NR=111285748A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HUANG BINBIN</creatorcontrib><creatorcontrib>XUE ZHIHUA</creatorcontrib><creatorcontrib>HE WEI</creatorcontrib><creatorcontrib>LYU JIEYAO</creatorcontrib><creatorcontrib>YAN QILONG</creatorcontrib><title>Preparation method of dopamine modified graphene insensitive doped nitramine oxidant</title><description>The invention relates to a preparation method of a dopamine modified graphene insensitive doped nitramine oxidizing agent. The preparation method comprises the following steps: dissolving ammonium nitrate crystals in nearly saturated dimethyl sulfoxide DMSO to obtain a DMSO solution of the ammonium nitrate crystals; adding a graphene oxide suspension into the DMSO solution, and adding a dopamine ethanol solution to obtain a mixed solution containing ammonium nitrate crystals, DA and the graphene oxide suspension; and dropwise adding H2O2 to obtain a mixed solution containing polydopamine PDA,so as to obtain the dopamine modified graphene insensitive doped nitramine oxidizing agent of a GO doped ammonium nitrate crystal energetic material taking PDA as an interface material. The preparation method has the beneficial effects that the safety risk in the operation process is reduced by introducing graphene oxide; and an ammonium nitrate energetic material with relatively high stability, namely, a graphene oxide d</description><subject>CHEMISTRY</subject><subject>EXPLOSIVES</subject><subject>EXPLOSIVES OR THERMIC COMPOSITIONS</subject><subject>MANUFACTURE THEREOF</subject><subject>MATCHES</subject><subject>METALLURGY</subject><subject>USE OF SINGLE SUBSTANCES AS EXPLOSIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAgJKEotSCxKLMnMz1PITS3JyE9RyE9TSMkvSMzNzEtVyM1PyUzLTE1RSC9KLMhIBYpk5hWn5hVnlmSWpYKUAaXyMkuKIKrzKzJTEvNKeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYjLQoJJ4Zz9DQ0MjC1NzEwtHY2LUAAD0QjmT</recordid><startdate>20200616</startdate><enddate>20200616</enddate><creator>HUANG BINBIN</creator><creator>XUE ZHIHUA</creator><creator>HE WEI</creator><creator>LYU JIEYAO</creator><creator>YAN QILONG</creator><scope>EVB</scope></search><sort><creationdate>20200616</creationdate><title>Preparation method of dopamine modified graphene insensitive doped nitramine oxidant</title><author>HUANG BINBIN ; XUE ZHIHUA ; HE WEI ; LYU JIEYAO ; YAN QILONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111285748A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>CHEMISTRY</topic><topic>EXPLOSIVES</topic><topic>EXPLOSIVES OR THERMIC COMPOSITIONS</topic><topic>MANUFACTURE THEREOF</topic><topic>MATCHES</topic><topic>METALLURGY</topic><topic>USE OF SINGLE SUBSTANCES AS EXPLOSIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>HUANG BINBIN</creatorcontrib><creatorcontrib>XUE ZHIHUA</creatorcontrib><creatorcontrib>HE WEI</creatorcontrib><creatorcontrib>LYU JIEYAO</creatorcontrib><creatorcontrib>YAN QILONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HUANG BINBIN</au><au>XUE ZHIHUA</au><au>HE WEI</au><au>LYU JIEYAO</au><au>YAN QILONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of dopamine modified graphene insensitive doped nitramine oxidant</title><date>2020-06-16</date><risdate>2020</risdate><abstract>The invention relates to a preparation method of a dopamine modified graphene insensitive doped nitramine oxidizing agent. The preparation method comprises the following steps: dissolving ammonium nitrate crystals in nearly saturated dimethyl sulfoxide DMSO to obtain a DMSO solution of the ammonium nitrate crystals; adding a graphene oxide suspension into the DMSO solution, and adding a dopamine ethanol solution to obtain a mixed solution containing ammonium nitrate crystals, DA and the graphene oxide suspension; and dropwise adding H2O2 to obtain a mixed solution containing polydopamine PDA,so as to obtain the dopamine modified graphene insensitive doped nitramine oxidizing agent of a GO doped ammonium nitrate crystal energetic material taking PDA as an interface material. The preparation method has the beneficial effects that the safety risk in the operation process is reduced by introducing graphene oxide; and an ammonium nitrate energetic material with relatively high stability, namely, a graphene oxide d</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN111285748A
source esp@cenet
subjects CHEMISTRY
EXPLOSIVES
EXPLOSIVES OR THERMIC COMPOSITIONS
MANUFACTURE THEREOF
MATCHES
METALLURGY
USE OF SINGLE SUBSTANCES AS EXPLOSIVES
title Preparation method of dopamine modified graphene insensitive doped nitramine oxidant
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-11T03%3A14%3A05IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HUANG%20BINBIN&rft.date=2020-06-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111285748A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true