Curing device of anti-relaxation coating of alkali metal gas chamber

The invention relates to a curing device of an anti-relaxation coating of an alkali metal gas chamber. An alkali metal gas chamber main body and an alkali metal gas chamber tail pipe are respectivelyarranged on a lower shell at high temperature and an upper shell at low temperature, when the anti-re...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FANG JIANCHENG, HAN BANGCHENG, LI LIN, SHANG HUINING, QUAN WEI, LU JIXI, ZHOU BINQUAN, CHI HAOTIAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FANG JIANCHENG
HAN BANGCHENG
LI LIN
SHANG HUINING
QUAN WEI
LU JIXI
ZHOU BINQUAN
CHI HAOTIAN
description The invention relates to a curing device of an anti-relaxation coating of an alkali metal gas chamber. An alkali metal gas chamber main body and an alkali metal gas chamber tail pipe are respectivelyarranged on a lower shell at high temperature and an upper shell at low temperature, when the anti-relaxation coating is cured, alkali metal atoms which are attached to the alkali metal gas chamber main body can preferably interact with the anti-relaxation coating at the curing temperature provided by a heating device in the lower shell so as to generate the stable anti-relaxation coating, and thegasified alkali metal atoms are coagulated and attached to the cold alkali metal gas chamber tail pipe at last due to the temperature gradient between the lower shell and the upper shell, so that theanti-relaxation coating does not have defects, and the coverage rate of the anti-relaxation coating is increased. 本发明所述的一种碱金属气室内抗弛豫涂层的固化装置,将碱金属气室主体与碱金属气室尾管分别设于温度较高的下层壳体和温度较低的上层壳体,在抗弛豫涂层固化时,附着于所述碱金属气室主体的碱金属原子在下层壳体内的加热装置提供的固化温度作
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN111013969A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN111013969A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN111013969A3</originalsourceid><addsrcrecordid>eNrjZHBxLi3KzEtXSEkty0xOVchPU0jMK8nULUrNSaxILMnMz1NIzgfSQBUgqZzsxJxMhdzUksQchfTEYoXkjMTcpNQiHgbWtMSc4lReKM3NoOjmGuLsoZtakB-fWlyQmJyal1oS7-xnaGhoYGhsaWbpaEyMGgB8YjJO</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Curing device of anti-relaxation coating of alkali metal gas chamber</title><source>esp@cenet</source><creator>FANG JIANCHENG ; HAN BANGCHENG ; LI LIN ; SHANG HUINING ; QUAN WEI ; LU JIXI ; ZHOU BINQUAN ; CHI HAOTIAN</creator><creatorcontrib>FANG JIANCHENG ; HAN BANGCHENG ; LI LIN ; SHANG HUINING ; QUAN WEI ; LU JIXI ; ZHOU BINQUAN ; CHI HAOTIAN</creatorcontrib><description>The invention relates to a curing device of an anti-relaxation coating of an alkali metal gas chamber. An alkali metal gas chamber main body and an alkali metal gas chamber tail pipe are respectivelyarranged on a lower shell at high temperature and an upper shell at low temperature, when the anti-relaxation coating is cured, alkali metal atoms which are attached to the alkali metal gas chamber main body can preferably interact with the anti-relaxation coating at the curing temperature provided by a heating device in the lower shell so as to generate the stable anti-relaxation coating, and thegasified alkali metal atoms are coagulated and attached to the cold alkali metal gas chamber tail pipe at last due to the temperature gradient between the lower shell and the upper shell, so that theanti-relaxation coating does not have defects, and the coverage rate of the anti-relaxation coating is increased. 本发明所述的一种碱金属气室内抗弛豫涂层的固化装置,将碱金属气室主体与碱金属气室尾管分别设于温度较高的下层壳体和温度较低的上层壳体,在抗弛豫涂层固化时,附着于所述碱金属气室主体的碱金属原子在下层壳体内的加热装置提供的固化温度作</description><language>chi ; eng</language><subject>APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL ; PERFORMING OPERATIONS ; PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL ; SPRAYING OR ATOMISING IN GENERAL ; TRANSPORTING</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200417&amp;DB=EPODOC&amp;CC=CN&amp;NR=111013969A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25553,76306</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200417&amp;DB=EPODOC&amp;CC=CN&amp;NR=111013969A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FANG JIANCHENG</creatorcontrib><creatorcontrib>HAN BANGCHENG</creatorcontrib><creatorcontrib>LI LIN</creatorcontrib><creatorcontrib>SHANG HUINING</creatorcontrib><creatorcontrib>QUAN WEI</creatorcontrib><creatorcontrib>LU JIXI</creatorcontrib><creatorcontrib>ZHOU BINQUAN</creatorcontrib><creatorcontrib>CHI HAOTIAN</creatorcontrib><title>Curing device of anti-relaxation coating of alkali metal gas chamber</title><description>The invention relates to a curing device of an anti-relaxation coating of an alkali metal gas chamber. An alkali metal gas chamber main body and an alkali metal gas chamber tail pipe are respectivelyarranged on a lower shell at high temperature and an upper shell at low temperature, when the anti-relaxation coating is cured, alkali metal atoms which are attached to the alkali metal gas chamber main body can preferably interact with the anti-relaxation coating at the curing temperature provided by a heating device in the lower shell so as to generate the stable anti-relaxation coating, and thegasified alkali metal atoms are coagulated and attached to the cold alkali metal gas chamber tail pipe at last due to the temperature gradient between the lower shell and the upper shell, so that theanti-relaxation coating does not have defects, and the coverage rate of the anti-relaxation coating is increased. 本发明所述的一种碱金属气室内抗弛豫涂层的固化装置,将碱金属气室主体与碱金属气室尾管分别设于温度较高的下层壳体和温度较低的上层壳体,在抗弛豫涂层固化时,附着于所述碱金属气室主体的碱金属原子在下层壳体内的加热装置提供的固化温度作</description><subject>APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL</subject><subject>SPRAYING OR ATOMISING IN GENERAL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHBxLi3KzEtXSEkty0xOVchPU0jMK8nULUrNSaxILMnMz1NIzgfSQBUgqZzsxJxMhdzUksQchfTEYoXkjMTcpNQiHgbWtMSc4lReKM3NoOjmGuLsoZtakB-fWlyQmJyal1oS7-xnaGhoYGhsaWbpaEyMGgB8YjJO</recordid><startdate>20200417</startdate><enddate>20200417</enddate><creator>FANG JIANCHENG</creator><creator>HAN BANGCHENG</creator><creator>LI LIN</creator><creator>SHANG HUINING</creator><creator>QUAN WEI</creator><creator>LU JIXI</creator><creator>ZHOU BINQUAN</creator><creator>CHI HAOTIAN</creator><scope>EVB</scope></search><sort><creationdate>20200417</creationdate><title>Curing device of anti-relaxation coating of alkali metal gas chamber</title><author>FANG JIANCHENG ; HAN BANGCHENG ; LI LIN ; SHANG HUINING ; QUAN WEI ; LU JIXI ; ZHOU BINQUAN ; CHI HAOTIAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN111013969A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL</topic><topic>SPRAYING OR ATOMISING IN GENERAL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>FANG JIANCHENG</creatorcontrib><creatorcontrib>HAN BANGCHENG</creatorcontrib><creatorcontrib>LI LIN</creatorcontrib><creatorcontrib>SHANG HUINING</creatorcontrib><creatorcontrib>QUAN WEI</creatorcontrib><creatorcontrib>LU JIXI</creatorcontrib><creatorcontrib>ZHOU BINQUAN</creatorcontrib><creatorcontrib>CHI HAOTIAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FANG JIANCHENG</au><au>HAN BANGCHENG</au><au>LI LIN</au><au>SHANG HUINING</au><au>QUAN WEI</au><au>LU JIXI</au><au>ZHOU BINQUAN</au><au>CHI HAOTIAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Curing device of anti-relaxation coating of alkali metal gas chamber</title><date>2020-04-17</date><risdate>2020</risdate><abstract>The invention relates to a curing device of an anti-relaxation coating of an alkali metal gas chamber. An alkali metal gas chamber main body and an alkali metal gas chamber tail pipe are respectivelyarranged on a lower shell at high temperature and an upper shell at low temperature, when the anti-relaxation coating is cured, alkali metal atoms which are attached to the alkali metal gas chamber main body can preferably interact with the anti-relaxation coating at the curing temperature provided by a heating device in the lower shell so as to generate the stable anti-relaxation coating, and thegasified alkali metal atoms are coagulated and attached to the cold alkali metal gas chamber tail pipe at last due to the temperature gradient between the lower shell and the upper shell, so that theanti-relaxation coating does not have defects, and the coverage rate of the anti-relaxation coating is increased. 本发明所述的一种碱金属气室内抗弛豫涂层的固化装置,将碱金属气室主体与碱金属气室尾管分别设于温度较高的下层壳体和温度较低的上层壳体,在抗弛豫涂层固化时,附着于所述碱金属气室主体的碱金属原子在下层壳体内的加热装置提供的固化温度作</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN111013969A
source esp@cenet
subjects APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
PERFORMING OPERATIONS
PROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TOSURFACES, IN GENERAL
SPRAYING OR ATOMISING IN GENERAL
TRANSPORTING
title Curing device of anti-relaxation coating of alkali metal gas chamber
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T07%3A55%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FANG%20JIANCHENG&rft.date=2020-04-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN111013969A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true