High-Bs low-power-consumption manganese-zinc ferrite material and preparation method thereof

The invention relates to the technical field of ferrite material preparation, in particular to a high-Bs low-power-consumption manganese-zinc ferrite material and a preparation method thereof. The high-Bs low-power-consumption manganese-zinc ferrite material comprises main components and auxiliary c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: XU SHILIANG, KONG ZHIQIANG, HAN WEIDONG, DING CHANGLONG, GAO ZHONGGUO, WANG YONG, LIU TAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator XU SHILIANG
KONG ZHIQIANG
HAN WEIDONG
DING CHANGLONG
GAO ZHONGGUO
WANG YONG
LIU TAO
description The invention relates to the technical field of ferrite material preparation, in particular to a high-Bs low-power-consumption manganese-zinc ferrite material and a preparation method thereof. The high-Bs low-power-consumption manganese-zinc ferrite material comprises main components and auxiliary components, wherein the main components comprise, by mole, 54 to 55 mol% of Fe2O3, 40 to 41 mol% of Mn3O4 and 4.5 to 5.5 mol% of ZnO; the auxiliary components are prepared from the following main components in percentage by weight: 150 to 200 ppm of SiO2, 100 to 150 ppm of P2O5, 500 to 800 ppm of CaO, 300 to 400 ppm of ZrO2 and 400 to 500 ppm of Nb2O5. The high-Bs low-power-consumption manganese-zinc ferrite material is prepared on the basis that no NiO is added, the production cost is greatly reduced, meanwhile, a unique sintering process is adopted, SiO2 and P2O5 are used as sintering accelerators, the sintering density, magnetic conductivity and Bs of the product are effectively improved,and the power consumption
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110655396A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110655396A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110655396A3</originalsourceid><addsrcrecordid>eNqNyjEKwkAQRuE0FqLeYT3AgiEkYKlBSWVlKYQh-ZNdSGaW2ZWAp1fQA1g9eHzr7NH40dlzNJMsNsgCtZ1wfM4heWEzE4_EiLAvz50ZoOoTPjtBPU2GuDdBEUjp65Gc9CY5KGTYZquBpojdr5tsf73c68YiSIsYqAMjtfUtzw9VWRbH6lT8Y97o_Dxb</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High-Bs low-power-consumption manganese-zinc ferrite material and preparation method thereof</title><source>esp@cenet</source><creator>XU SHILIANG ; KONG ZHIQIANG ; HAN WEIDONG ; DING CHANGLONG ; GAO ZHONGGUO ; WANG YONG ; LIU TAO</creator><creatorcontrib>XU SHILIANG ; KONG ZHIQIANG ; HAN WEIDONG ; DING CHANGLONG ; GAO ZHONGGUO ; WANG YONG ; LIU TAO</creatorcontrib><description>The invention relates to the technical field of ferrite material preparation, in particular to a high-Bs low-power-consumption manganese-zinc ferrite material and a preparation method thereof. The high-Bs low-power-consumption manganese-zinc ferrite material comprises main components and auxiliary components, wherein the main components comprise, by mole, 54 to 55 mol% of Fe2O3, 40 to 41 mol% of Mn3O4 and 4.5 to 5.5 mol% of ZnO; the auxiliary components are prepared from the following main components in percentage by weight: 150 to 200 ppm of SiO2, 100 to 150 ppm of P2O5, 500 to 800 ppm of CaO, 300 to 400 ppm of ZrO2 and 400 to 500 ppm of Nb2O5. The high-Bs low-power-consumption manganese-zinc ferrite material is prepared on the basis that no NiO is added, the production cost is greatly reduced, meanwhile, a unique sintering process is adopted, SiO2 and P2O5 are used as sintering accelerators, the sintering density, magnetic conductivity and Bs of the product are effectively improved,and the power consumption</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; BASIC ELECTRIC ELEMENTS ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; ELECTRICITY ; INDUCTANCES ; LIME, MAGNESIA ; MAGNETS ; METALLURGY ; REFRACTORIES ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; SLAG ; TRANSFORMERS ; TREATMENT OF NATURAL STONE</subject><creationdate>2020</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200107&amp;DB=EPODOC&amp;CC=CN&amp;NR=110655396A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20200107&amp;DB=EPODOC&amp;CC=CN&amp;NR=110655396A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>XU SHILIANG</creatorcontrib><creatorcontrib>KONG ZHIQIANG</creatorcontrib><creatorcontrib>HAN WEIDONG</creatorcontrib><creatorcontrib>DING CHANGLONG</creatorcontrib><creatorcontrib>GAO ZHONGGUO</creatorcontrib><creatorcontrib>WANG YONG</creatorcontrib><creatorcontrib>LIU TAO</creatorcontrib><title>High-Bs low-power-consumption manganese-zinc ferrite material and preparation method thereof</title><description>The invention relates to the technical field of ferrite material preparation, in particular to a high-Bs low-power-consumption manganese-zinc ferrite material and a preparation method thereof. The high-Bs low-power-consumption manganese-zinc ferrite material comprises main components and auxiliary components, wherein the main components comprise, by mole, 54 to 55 mol% of Fe2O3, 40 to 41 mol% of Mn3O4 and 4.5 to 5.5 mol% of ZnO; the auxiliary components are prepared from the following main components in percentage by weight: 150 to 200 ppm of SiO2, 100 to 150 ppm of P2O5, 500 to 800 ppm of CaO, 300 to 400 ppm of ZrO2 and 400 to 500 ppm of Nb2O5. The high-Bs low-power-consumption manganese-zinc ferrite material is prepared on the basis that no NiO is added, the production cost is greatly reduced, meanwhile, a unique sintering process is adopted, SiO2 and P2O5 are used as sintering accelerators, the sintering density, magnetic conductivity and Bs of the product are effectively improved,and the power consumption</description><subject>ARTIFICIAL STONE</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>ELECTRICITY</subject><subject>INDUCTANCES</subject><subject>LIME, MAGNESIA</subject><subject>MAGNETS</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>SLAG</subject><subject>TRANSFORMERS</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2020</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEKwkAQRuE0FqLeYT3AgiEkYKlBSWVlKYQh-ZNdSGaW2ZWAp1fQA1g9eHzr7NH40dlzNJMsNsgCtZ1wfM4heWEzE4_EiLAvz50ZoOoTPjtBPU2GuDdBEUjp65Gc9CY5KGTYZquBpojdr5tsf73c68YiSIsYqAMjtfUtzw9VWRbH6lT8Y97o_Dxb</recordid><startdate>20200107</startdate><enddate>20200107</enddate><creator>XU SHILIANG</creator><creator>KONG ZHIQIANG</creator><creator>HAN WEIDONG</creator><creator>DING CHANGLONG</creator><creator>GAO ZHONGGUO</creator><creator>WANG YONG</creator><creator>LIU TAO</creator><scope>EVB</scope></search><sort><creationdate>20200107</creationdate><title>High-Bs low-power-consumption manganese-zinc ferrite material and preparation method thereof</title><author>XU SHILIANG ; KONG ZHIQIANG ; HAN WEIDONG ; DING CHANGLONG ; GAO ZHONGGUO ; WANG YONG ; LIU TAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110655396A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2020</creationdate><topic>ARTIFICIAL STONE</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>ELECTRICITY</topic><topic>INDUCTANCES</topic><topic>LIME, MAGNESIA</topic><topic>MAGNETS</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>SLAG</topic><topic>TRANSFORMERS</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>XU SHILIANG</creatorcontrib><creatorcontrib>KONG ZHIQIANG</creatorcontrib><creatorcontrib>HAN WEIDONG</creatorcontrib><creatorcontrib>DING CHANGLONG</creatorcontrib><creatorcontrib>GAO ZHONGGUO</creatorcontrib><creatorcontrib>WANG YONG</creatorcontrib><creatorcontrib>LIU TAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>XU SHILIANG</au><au>KONG ZHIQIANG</au><au>HAN WEIDONG</au><au>DING CHANGLONG</au><au>GAO ZHONGGUO</au><au>WANG YONG</au><au>LIU TAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High-Bs low-power-consumption manganese-zinc ferrite material and preparation method thereof</title><date>2020-01-07</date><risdate>2020</risdate><abstract>The invention relates to the technical field of ferrite material preparation, in particular to a high-Bs low-power-consumption manganese-zinc ferrite material and a preparation method thereof. The high-Bs low-power-consumption manganese-zinc ferrite material comprises main components and auxiliary components, wherein the main components comprise, by mole, 54 to 55 mol% of Fe2O3, 40 to 41 mol% of Mn3O4 and 4.5 to 5.5 mol% of ZnO; the auxiliary components are prepared from the following main components in percentage by weight: 150 to 200 ppm of SiO2, 100 to 150 ppm of P2O5, 500 to 800 ppm of CaO, 300 to 400 ppm of ZrO2 and 400 to 500 ppm of Nb2O5. The high-Bs low-power-consumption manganese-zinc ferrite material is prepared on the basis that no NiO is added, the production cost is greatly reduced, meanwhile, a unique sintering process is adopted, SiO2 and P2O5 are used as sintering accelerators, the sintering density, magnetic conductivity and Bs of the product are effectively improved,and the power consumption</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN110655396A
source esp@cenet
subjects ARTIFICIAL STONE
BASIC ELECTRIC ELEMENTS
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
ELECTRICITY
INDUCTANCES
LIME, MAGNESIA
MAGNETS
METALLURGY
REFRACTORIES
SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
SLAG
TRANSFORMERS
TREATMENT OF NATURAL STONE
title High-Bs low-power-consumption manganese-zinc ferrite material and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T06%3A45%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=XU%20SHILIANG&rft.date=2020-01-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110655396A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true