Environmental-friendly plastering mortar and preparation method thereof

The invention discloses environmental-friendly plastering mortar and a preparation method thereof and relates to the technical field of building mortar. According to the technical scheme, the environmental-friendly plastering mortar is characterized by comprising the following components in parts by...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FU ZHIBIN, RAN JIZHONG, ZHANG HAILONG, TAN MIANZHI, DI YAODONG, CHEN ZHENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FU ZHIBIN
RAN JIZHONG
ZHANG HAILONG
TAN MIANZHI
DI YAODONG
CHEN ZHENG
description The invention discloses environmental-friendly plastering mortar and a preparation method thereof and relates to the technical field of building mortar. According to the technical scheme, the environmental-friendly plastering mortar is characterized by comprising the following components in parts by weight: 240-260 parts of cement, 65-75 parts of coal ash, 1050-1100 parts of a fine aggregate, 250-270 parts of water, 3-5 parts of a plastic retaining agent and 1-3 parts of a thickening time control agent. With the combination of the plastic retaining agent and the thickening time control agent with other raw materials, original properties of wet-mixed plastering mortar can be maintained for a long time, and the plastering mortar has very good water retention and stability, and has operability time up to 30 hours. 本发明公开了一种环保型抹灰砂浆及其制备方法,涉及建筑砂浆技术领域,其技术方案要点是一种环保型抹灰砂浆,以重量份数计,包括如下组分:水泥240-260份、粉煤灰65-75份、细骨料1050-1100份、水250-270份、保塑剂3-5份以及调凝剂1-3份。本发明通过保塑剂与调凝剂与其他原料的配合,可以使得湿拌抹灰砂浆可以在较长时间内保持原本的性能,具有很好的保水性以及稳定性,其可操作时间可达30h。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110627450A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110627450A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110627450A3</originalsourceid><addsrcrecordid>eNqNyjsOwjAMANAsDAi4gzlApZbvjKoCExN7ZRGnjZTYkWMhcXsWDsD0lrd0t4HfUYUzsWFqgkZinz5QElYjjTxBFjVUQPZQlAoqWhSGTDaLB5tJScLaLQKmSpufK7e9Ds_-3lCRkWrBFzHZ2D-6rj3tzodje9n_c77tdDTi</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Environmental-friendly plastering mortar and preparation method thereof</title><source>esp@cenet</source><creator>FU ZHIBIN ; RAN JIZHONG ; ZHANG HAILONG ; TAN MIANZHI ; DI YAODONG ; CHEN ZHENG</creator><creatorcontrib>FU ZHIBIN ; RAN JIZHONG ; ZHANG HAILONG ; TAN MIANZHI ; DI YAODONG ; CHEN ZHENG</creatorcontrib><description>The invention discloses environmental-friendly plastering mortar and a preparation method thereof and relates to the technical field of building mortar. According to the technical scheme, the environmental-friendly plastering mortar is characterized by comprising the following components in parts by weight: 240-260 parts of cement, 65-75 parts of coal ash, 1050-1100 parts of a fine aggregate, 250-270 parts of water, 3-5 parts of a plastic retaining agent and 1-3 parts of a thickening time control agent. With the combination of the plastic retaining agent and the thickening time control agent with other raw materials, original properties of wet-mixed plastering mortar can be maintained for a long time, and the plastering mortar has very good water retention and stability, and has operability time up to 30 hours. 本发明公开了一种环保型抹灰砂浆及其制备方法,涉及建筑砂浆技术领域,其技术方案要点是一种环保型抹灰砂浆,以重量份数计,包括如下组分:水泥240-260份、粉煤灰65-75份、细骨料1050-1100份、水250-270份、保塑剂3-5份以及调凝剂1-3份。本发明通过保塑剂与调凝剂与其他原料的配合,可以使得湿拌抹灰砂浆可以在较长时间内保持原本的性能,具有很好的保水性以及稳定性,其可操作时间可达30h。</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191231&amp;DB=EPODOC&amp;CC=CN&amp;NR=110627450A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191231&amp;DB=EPODOC&amp;CC=CN&amp;NR=110627450A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FU ZHIBIN</creatorcontrib><creatorcontrib>RAN JIZHONG</creatorcontrib><creatorcontrib>ZHANG HAILONG</creatorcontrib><creatorcontrib>TAN MIANZHI</creatorcontrib><creatorcontrib>DI YAODONG</creatorcontrib><creatorcontrib>CHEN ZHENG</creatorcontrib><title>Environmental-friendly plastering mortar and preparation method thereof</title><description>The invention discloses environmental-friendly plastering mortar and a preparation method thereof and relates to the technical field of building mortar. According to the technical scheme, the environmental-friendly plastering mortar is characterized by comprising the following components in parts by weight: 240-260 parts of cement, 65-75 parts of coal ash, 1050-1100 parts of a fine aggregate, 250-270 parts of water, 3-5 parts of a plastic retaining agent and 1-3 parts of a thickening time control agent. With the combination of the plastic retaining agent and the thickening time control agent with other raw materials, original properties of wet-mixed plastering mortar can be maintained for a long time, and the plastering mortar has very good water retention and stability, and has operability time up to 30 hours. 本发明公开了一种环保型抹灰砂浆及其制备方法,涉及建筑砂浆技术领域,其技术方案要点是一种环保型抹灰砂浆,以重量份数计,包括如下组分:水泥240-260份、粉煤灰65-75份、细骨料1050-1100份、水250-270份、保塑剂3-5份以及调凝剂1-3份。本发明通过保塑剂与调凝剂与其他原料的配合,可以使得湿拌抹灰砂浆可以在较长时间内保持原本的性能,具有很好的保水性以及稳定性,其可操作时间可达30h。</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjsOwjAMANAsDAi4gzlApZbvjKoCExN7ZRGnjZTYkWMhcXsWDsD0lrd0t4HfUYUzsWFqgkZinz5QElYjjTxBFjVUQPZQlAoqWhSGTDaLB5tJScLaLQKmSpufK7e9Ds_-3lCRkWrBFzHZ2D-6rj3tzodje9n_c77tdDTi</recordid><startdate>20191231</startdate><enddate>20191231</enddate><creator>FU ZHIBIN</creator><creator>RAN JIZHONG</creator><creator>ZHANG HAILONG</creator><creator>TAN MIANZHI</creator><creator>DI YAODONG</creator><creator>CHEN ZHENG</creator><scope>EVB</scope></search><sort><creationdate>20191231</creationdate><title>Environmental-friendly plastering mortar and preparation method thereof</title><author>FU ZHIBIN ; RAN JIZHONG ; ZHANG HAILONG ; TAN MIANZHI ; DI YAODONG ; CHEN ZHENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110627450A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>FU ZHIBIN</creatorcontrib><creatorcontrib>RAN JIZHONG</creatorcontrib><creatorcontrib>ZHANG HAILONG</creatorcontrib><creatorcontrib>TAN MIANZHI</creatorcontrib><creatorcontrib>DI YAODONG</creatorcontrib><creatorcontrib>CHEN ZHENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FU ZHIBIN</au><au>RAN JIZHONG</au><au>ZHANG HAILONG</au><au>TAN MIANZHI</au><au>DI YAODONG</au><au>CHEN ZHENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Environmental-friendly plastering mortar and preparation method thereof</title><date>2019-12-31</date><risdate>2019</risdate><abstract>The invention discloses environmental-friendly plastering mortar and a preparation method thereof and relates to the technical field of building mortar. According to the technical scheme, the environmental-friendly plastering mortar is characterized by comprising the following components in parts by weight: 240-260 parts of cement, 65-75 parts of coal ash, 1050-1100 parts of a fine aggregate, 250-270 parts of water, 3-5 parts of a plastic retaining agent and 1-3 parts of a thickening time control agent. With the combination of the plastic retaining agent and the thickening time control agent with other raw materials, original properties of wet-mixed plastering mortar can be maintained for a long time, and the plastering mortar has very good water retention and stability, and has operability time up to 30 hours. 本发明公开了一种环保型抹灰砂浆及其制备方法,涉及建筑砂浆技术领域,其技术方案要点是一种环保型抹灰砂浆,以重量份数计,包括如下组分:水泥240-260份、粉煤灰65-75份、细骨料1050-1100份、水250-270份、保塑剂3-5份以及调凝剂1-3份。本发明通过保塑剂与调凝剂与其他原料的配合,可以使得湿拌抹灰砂浆可以在较长时间内保持原本的性能,具有很好的保水性以及稳定性,其可操作时间可达30h。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN110627450A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Environmental-friendly plastering mortar and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T21%3A29%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FU%20ZHIBIN&rft.date=2019-12-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110627450A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true