Preparation method of dextrin with thermal viscosity stability
The invention relates to the technical field of dextrin processing, in particular to a preparation method of dextrin with thermal viscosity stability. The preparation method comprises the following steps that first, starch acidizing treatment is conducted, specifically, starch is acidized through a...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHONG MINGXUE MO QUANTING FENG LIN LI YING WANG FUBIAO |
description | The invention relates to the technical field of dextrin processing, in particular to a preparation method of dextrin with thermal viscosity stability. The preparation method comprises the following steps that first, starch acidizing treatment is conducted, specifically, starch is acidized through a hydrochloric acid solution with the concentration being 6%-8%, thus the PH value of the starch is kept within the range of 2.0-2.2, and still standing for adsorption is conducted for two hours; second, pre-drying is conducted, specifically, the acidized starch is subjected to air flow drying to enable the moisture content of the starch to be decreased to 6% or below; and third, dextrin transformation is conducted, specifically, conduction oil is added into a jacket in a jacket reaction tank fora dextrinization reaction, the oil temperature of the jacket reaction tank is increased to 170 DEG C before the reaction, then the acidized starch treated in the second step is put into the jacket reaction tank, and trace hot |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110551225A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110551225A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110551225A3</originalsourceid><addsrcrecordid>eNrjZLALKEotSCxKLMnMz1PITS3JyE9RyE9TSEmtKCnKzFMozyzJUCjJSC3KTcxRKMssTs4vziypVCguSUzKzAGyeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGBqamhkZGpozExagCn-jE1</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of dextrin with thermal viscosity stability</title><source>esp@cenet</source><creator>ZHONG MINGXUE ; MO QUANTING ; FENG LIN ; LI YING ; WANG FUBIAO</creator><creatorcontrib>ZHONG MINGXUE ; MO QUANTING ; FENG LIN ; LI YING ; WANG FUBIAO</creatorcontrib><description>The invention relates to the technical field of dextrin processing, in particular to a preparation method of dextrin with thermal viscosity stability. The preparation method comprises the following steps that first, starch acidizing treatment is conducted, specifically, starch is acidized through a hydrochloric acid solution with the concentration being 6%-8%, thus the PH value of the starch is kept within the range of 2.0-2.2, and still standing for adsorption is conducted for two hours; second, pre-drying is conducted, specifically, the acidized starch is subjected to air flow drying to enable the moisture content of the starch to be decreased to 6% or below; and third, dextrin transformation is conducted, specifically, conduction oil is added into a jacket in a jacket reaction tank fora dextrinization reaction, the oil temperature of the jacket reaction tank is increased to 170 DEG C before the reaction, then the acidized starch treated in the second step is put into the jacket reaction tank, and trace hot</description><language>chi ; eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; DERIVATIVES THEREOF ; DYES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; POLYSACCHARIDES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20191210&DB=EPODOC&CC=CN&NR=110551225A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20191210&DB=EPODOC&CC=CN&NR=110551225A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHONG MINGXUE</creatorcontrib><creatorcontrib>MO QUANTING</creatorcontrib><creatorcontrib>FENG LIN</creatorcontrib><creatorcontrib>LI YING</creatorcontrib><creatorcontrib>WANG FUBIAO</creatorcontrib><title>Preparation method of dextrin with thermal viscosity stability</title><description>The invention relates to the technical field of dextrin processing, in particular to a preparation method of dextrin with thermal viscosity stability. The preparation method comprises the following steps that first, starch acidizing treatment is conducted, specifically, starch is acidized through a hydrochloric acid solution with the concentration being 6%-8%, thus the PH value of the starch is kept within the range of 2.0-2.2, and still standing for adsorption is conducted for two hours; second, pre-drying is conducted, specifically, the acidized starch is subjected to air flow drying to enable the moisture content of the starch to be decreased to 6% or below; and third, dextrin transformation is conducted, specifically, conduction oil is added into a jacket in a jacket reaction tank fora dextrinization reaction, the oil temperature of the jacket reaction tank is increased to 170 DEG C before the reaction, then the acidized starch treated in the second step is put into the jacket reaction tank, and trace hot</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>DERIVATIVES THEREOF</subject><subject>DYES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>POLYSACCHARIDES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLALKEotSCxKLMnMz1PITS3JyE9RyE9TSEmtKCnKzFMozyzJUCjJSC3KTcxRKMssTs4vziypVCguSUzKzAGyeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGBqamhkZGpozExagCn-jE1</recordid><startdate>20191210</startdate><enddate>20191210</enddate><creator>ZHONG MINGXUE</creator><creator>MO QUANTING</creator><creator>FENG LIN</creator><creator>LI YING</creator><creator>WANG FUBIAO</creator><scope>EVB</scope></search><sort><creationdate>20191210</creationdate><title>Preparation method of dextrin with thermal viscosity stability</title><author>ZHONG MINGXUE ; MO QUANTING ; FENG LIN ; LI YING ; WANG FUBIAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110551225A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>DERIVATIVES THEREOF</topic><topic>DYES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>POLYSACCHARIDES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHONG MINGXUE</creatorcontrib><creatorcontrib>MO QUANTING</creatorcontrib><creatorcontrib>FENG LIN</creatorcontrib><creatorcontrib>LI YING</creatorcontrib><creatorcontrib>WANG FUBIAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHONG MINGXUE</au><au>MO QUANTING</au><au>FENG LIN</au><au>LI YING</au><au>WANG FUBIAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of dextrin with thermal viscosity stability</title><date>2019-12-10</date><risdate>2019</risdate><abstract>The invention relates to the technical field of dextrin processing, in particular to a preparation method of dextrin with thermal viscosity stability. The preparation method comprises the following steps that first, starch acidizing treatment is conducted, specifically, starch is acidized through a hydrochloric acid solution with the concentration being 6%-8%, thus the PH value of the starch is kept within the range of 2.0-2.2, and still standing for adsorption is conducted for two hours; second, pre-drying is conducted, specifically, the acidized starch is subjected to air flow drying to enable the moisture content of the starch to be decreased to 6% or below; and third, dextrin transformation is conducted, specifically, conduction oil is added into a jacket in a jacket reaction tank fora dextrinization reaction, the oil temperature of the jacket reaction tank is increased to 170 DEG C before the reaction, then the acidized starch treated in the second step is put into the jacket reaction tank, and trace hot</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN110551225A |
source | esp@cenet |
subjects | ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ADHESIVES CHEMISTRY COMPOSITIONS BASED THEREON DERIVATIVES THEREOF DYES METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ORGANIC MACROMOLECULAR COMPOUNDS PAINTS POLISHES POLYSACCHARIDES THEIR PREPARATION OR CHEMICAL WORKING-UP USE OF MATERIALS AS ADHESIVES |
title | Preparation method of dextrin with thermal viscosity stability |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T21%3A33%3A32IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHONG%20MINGXUE&rft.date=2019-12-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110551225A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |