NEGATIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY

A negative electrode active material for a lithium ion secondary battery comprising silicon oxide particles having carbon present in a portion or the entirety of the surface thereof wherein the ratio(PSi/PSiO 2) of the X ray diffraction peak intensity at 2Theta = 27D to 29D originating from Si, rela...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NISHIDA TATSUYA, OHSAKI YOSHIE, YASUDA AKIRA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NISHIDA TATSUYA
OHSAKI YOSHIE
YASUDA AKIRA
description A negative electrode active material for a lithium ion secondary battery comprising silicon oxide particles having carbon present in a portion or the entirety of the surface thereof wherein the ratio(PSi/PSiO 2) of the X ray diffraction peak intensity at 2Theta = 27D to 29D originating from Si, relative to the X ray diffraction peak intensity at 2Theta=20D to 25D originating from SiO2, falls in the range of 1.0 to 2.6 when CuKAlpha radiation with a wavelength of 0.15406 nm is used as the beam source, and the aspect ratio represented by the ratio (S/L) between a long axis L and a short axis Sthereof, has a mean value that falls in the range of 0.45
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110462892A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110462892A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110462892A3</originalsourceid><addsrcrecordid>eNrjZJjr5-ruGOIZ5qrg6uPqHBLk7-Kq4OgMFvB1DHEN8nT0UXDzD1Lw8Qzx8Az1VfD091MIdnX293NxDIpUcHIMAaqJ1FHAYgoRuhz9XPAr4WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hoYGJmZGFpZGjsbEqAEAshNELQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>NEGATIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY</title><source>esp@cenet</source><creator>NISHIDA TATSUYA ; OHSAKI YOSHIE ; YASUDA AKIRA</creator><creatorcontrib>NISHIDA TATSUYA ; OHSAKI YOSHIE ; YASUDA AKIRA</creatorcontrib><description>A negative electrode active material for a lithium ion secondary battery comprising silicon oxide particles having carbon present in a portion or the entirety of the surface thereof wherein the ratio(PSi/PSiO 2) of the X ray diffraction peak intensity at 2Theta = 27D to 29D originating from Si, relative to the X ray diffraction peak intensity at 2Theta=20D to 25D originating from SiO2, falls in the range of 1.0 to 2.6 when CuKAlpha radiation with a wavelength of 0.15406 nm is used as the beam source, and the aspect ratio represented by the ratio (S/L) between a long axis L and a short axis Sthereof, has a mean value that falls in the range of 0.45&lt;=S/L&lt;=1. 一种锂离子二次电池用负极活性物质,其包含在表面的一部分或全部中存在碳的硅氧化物粒子,使用波长0.15406nm的CuKα射线作为射线源时,源自Si的2θ=27°~29°的X射线衍射峰强度相对于源自SiO的2θ=20°~25°的X射线衍射峰强度的比(P/P)为1.0~2.6的范围,由长径L与短径S的比(S/L)表示的纵横比的平均值处于0.45≤S/L≤1的范围。</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191115&amp;DB=EPODOC&amp;CC=CN&amp;NR=110462892A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191115&amp;DB=EPODOC&amp;CC=CN&amp;NR=110462892A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NISHIDA TATSUYA</creatorcontrib><creatorcontrib>OHSAKI YOSHIE</creatorcontrib><creatorcontrib>YASUDA AKIRA</creatorcontrib><title>NEGATIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY</title><description>A negative electrode active material for a lithium ion secondary battery comprising silicon oxide particles having carbon present in a portion or the entirety of the surface thereof wherein the ratio(PSi/PSiO 2) of the X ray diffraction peak intensity at 2Theta = 27D to 29D originating from Si, relative to the X ray diffraction peak intensity at 2Theta=20D to 25D originating from SiO2, falls in the range of 1.0 to 2.6 when CuKAlpha radiation with a wavelength of 0.15406 nm is used as the beam source, and the aspect ratio represented by the ratio (S/L) between a long axis L and a short axis Sthereof, has a mean value that falls in the range of 0.45&lt;=S/L&lt;=1. 一种锂离子二次电池用负极活性物质,其包含在表面的一部分或全部中存在碳的硅氧化物粒子,使用波长0.15406nm的CuKα射线作为射线源时,源自Si的2θ=27°~29°的X射线衍射峰强度相对于源自SiO的2θ=20°~25°的X射线衍射峰强度的比(P/P)为1.0~2.6的范围,由长径L与短径S的比(S/L)表示的纵横比的平均值处于0.45≤S/L≤1的范围。</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJjr5-ruGOIZ5qrg6uPqHBLk7-Kq4OgMFvB1DHEN8nT0UXDzD1Lw8Qzx8Az1VfD091MIdnX293NxDIpUcHIMAaqJ1FHAYgoRuhz9XPAr4WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hoYGJmZGFpZGjsbEqAEAshNELQ</recordid><startdate>20191115</startdate><enddate>20191115</enddate><creator>NISHIDA TATSUYA</creator><creator>OHSAKI YOSHIE</creator><creator>YASUDA AKIRA</creator><scope>EVB</scope></search><sort><creationdate>20191115</creationdate><title>NEGATIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY</title><author>NISHIDA TATSUYA ; OHSAKI YOSHIE ; YASUDA AKIRA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110462892A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>NISHIDA TATSUYA</creatorcontrib><creatorcontrib>OHSAKI YOSHIE</creatorcontrib><creatorcontrib>YASUDA AKIRA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NISHIDA TATSUYA</au><au>OHSAKI YOSHIE</au><au>YASUDA AKIRA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>NEGATIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY</title><date>2019-11-15</date><risdate>2019</risdate><abstract>A negative electrode active material for a lithium ion secondary battery comprising silicon oxide particles having carbon present in a portion or the entirety of the surface thereof wherein the ratio(PSi/PSiO 2) of the X ray diffraction peak intensity at 2Theta = 27D to 29D originating from Si, relative to the X ray diffraction peak intensity at 2Theta=20D to 25D originating from SiO2, falls in the range of 1.0 to 2.6 when CuKAlpha radiation with a wavelength of 0.15406 nm is used as the beam source, and the aspect ratio represented by the ratio (S/L) between a long axis L and a short axis Sthereof, has a mean value that falls in the range of 0.45&lt;=S/L&lt;=1. 一种锂离子二次电池用负极活性物质,其包含在表面的一部分或全部中存在碳的硅氧化物粒子,使用波长0.15406nm的CuKα射线作为射线源时,源自Si的2θ=27°~29°的X射线衍射峰强度相对于源自SiO的2θ=20°~25°的X射线衍射峰强度的比(P/P)为1.0~2.6的范围,由长径L与短径S的比(S/L)表示的纵横比的平均值处于0.45≤S/L≤1的范围。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN110462892A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title NEGATIVE ELECTRODE ACTIVE MATERIAL FOR LITHIUM ION SECONDARY BATTERY, NEGATIVE ELECTRODE FOR LITHIUM ION SECONDARY BATTERY, AND LITHIUM ION SECONDARY BATTERY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T20%3A34%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NISHIDA%20TATSUYA&rft.date=2019-11-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110462892A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true