PRODUCTION METHOD FOR LITHIUM METAL COMPLEX OXIDE

A production method for a lithium metal complex oxide is for producing a lithium metal complex oxide that contains at least nickel and that can be used for doping with lithium ions and removal of lithium ions, and the method comprises the steps: a mixing step for mixing a metal complex compound cont...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KAGEURA JUN-ICHI, KOBAYASHI RYOTA, DOUMAE KYOUSUKE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KAGEURA JUN-ICHI
KOBAYASHI RYOTA
DOUMAE KYOUSUKE
description A production method for a lithium metal complex oxide is for producing a lithium metal complex oxide that contains at least nickel and that can be used for doping with lithium ions and removal of lithium ions, and the method comprises the steps: a mixing step for mixing a metal complex compound containing at least nickel with a lithium compound to obtain a mixture; a firing step for firing the mixture in an oxygen-containing atmosphere to obtain a fired product; a washing step for washing the fired product to obtain a washed product; and a thermal treatment step for subjecting the washed product to a thermal treatment, wherein, in the mixing step, the mixing is performed such that the ratio (molar ratio) of the number of moles of lithium in the lithium compound to the total number of molesof metal elements in the metal complex compound exceeds one, and the thermal treatment step is performed at a temperature increase rate of 100 DEG C/hr or more and at a maintained temperature of morethan 550 DEG C but not mo
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110461770A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110461770A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110461770A3</originalsourceid><addsrcrecordid>eNrjZDAMCPJ3CXUO8fT3U_B1DfHwd1Fw8w9S8PEM8fAM9QUJOfooOPv7Bvi4Rij4R3i6uPIwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDAxMzQ3NzA0djYtQAAGF-Jp0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCTION METHOD FOR LITHIUM METAL COMPLEX OXIDE</title><source>esp@cenet</source><creator>KAGEURA JUN-ICHI ; KOBAYASHI RYOTA ; DOUMAE KYOUSUKE</creator><creatorcontrib>KAGEURA JUN-ICHI ; KOBAYASHI RYOTA ; DOUMAE KYOUSUKE</creatorcontrib><description>A production method for a lithium metal complex oxide is for producing a lithium metal complex oxide that contains at least nickel and that can be used for doping with lithium ions and removal of lithium ions, and the method comprises the steps: a mixing step for mixing a metal complex compound containing at least nickel with a lithium compound to obtain a mixture; a firing step for firing the mixture in an oxygen-containing atmosphere to obtain a fired product; a washing step for washing the fired product to obtain a washed product; and a thermal treatment step for subjecting the washed product to a thermal treatment, wherein, in the mixing step, the mixing is performed such that the ratio (molar ratio) of the number of moles of lithium in the lithium compound to the total number of molesof metal elements in the metal complex compound exceeds one, and the thermal treatment step is performed at a temperature increase rate of 100 DEG C/hr or more and at a maintained temperature of morethan 550 DEG C but not mo</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191115&amp;DB=EPODOC&amp;CC=CN&amp;NR=110461770A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191115&amp;DB=EPODOC&amp;CC=CN&amp;NR=110461770A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KAGEURA JUN-ICHI</creatorcontrib><creatorcontrib>KOBAYASHI RYOTA</creatorcontrib><creatorcontrib>DOUMAE KYOUSUKE</creatorcontrib><title>PRODUCTION METHOD FOR LITHIUM METAL COMPLEX OXIDE</title><description>A production method for a lithium metal complex oxide is for producing a lithium metal complex oxide that contains at least nickel and that can be used for doping with lithium ions and removal of lithium ions, and the method comprises the steps: a mixing step for mixing a metal complex compound containing at least nickel with a lithium compound to obtain a mixture; a firing step for firing the mixture in an oxygen-containing atmosphere to obtain a fired product; a washing step for washing the fired product to obtain a washed product; and a thermal treatment step for subjecting the washed product to a thermal treatment, wherein, in the mixing step, the mixing is performed such that the ratio (molar ratio) of the number of moles of lithium in the lithium compound to the total number of molesof metal elements in the metal complex compound exceeds one, and the thermal treatment step is performed at a temperature increase rate of 100 DEG C/hr or more and at a maintained temperature of morethan 550 DEG C but not mo</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAMCPJ3CXUO8fT3U_B1DfHwd1Fw8w9S8PEM8fAM9QUJOfooOPv7Bvi4Rij4R3i6uPIwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDAxMzQ3NzA0djYtQAAGF-Jp0</recordid><startdate>20191115</startdate><enddate>20191115</enddate><creator>KAGEURA JUN-ICHI</creator><creator>KOBAYASHI RYOTA</creator><creator>DOUMAE KYOUSUKE</creator><scope>EVB</scope></search><sort><creationdate>20191115</creationdate><title>PRODUCTION METHOD FOR LITHIUM METAL COMPLEX OXIDE</title><author>KAGEURA JUN-ICHI ; KOBAYASHI RYOTA ; DOUMAE KYOUSUKE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110461770A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>KAGEURA JUN-ICHI</creatorcontrib><creatorcontrib>KOBAYASHI RYOTA</creatorcontrib><creatorcontrib>DOUMAE KYOUSUKE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KAGEURA JUN-ICHI</au><au>KOBAYASHI RYOTA</au><au>DOUMAE KYOUSUKE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCTION METHOD FOR LITHIUM METAL COMPLEX OXIDE</title><date>2019-11-15</date><risdate>2019</risdate><abstract>A production method for a lithium metal complex oxide is for producing a lithium metal complex oxide that contains at least nickel and that can be used for doping with lithium ions and removal of lithium ions, and the method comprises the steps: a mixing step for mixing a metal complex compound containing at least nickel with a lithium compound to obtain a mixture; a firing step for firing the mixture in an oxygen-containing atmosphere to obtain a fired product; a washing step for washing the fired product to obtain a washed product; and a thermal treatment step for subjecting the washed product to a thermal treatment, wherein, in the mixing step, the mixing is performed such that the ratio (molar ratio) of the number of moles of lithium in the lithium compound to the total number of molesof metal elements in the metal complex compound exceeds one, and the thermal treatment step is performed at a temperature increase rate of 100 DEG C/hr or more and at a maintained temperature of morethan 550 DEG C but not mo</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN110461770A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
ELECTRICITY
INORGANIC CHEMISTRY
METALLURGY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title PRODUCTION METHOD FOR LITHIUM METAL COMPLEX OXIDE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T19%3A04%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KAGEURA%20JUN-ICHI&rft.date=2019-11-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110461770A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true