Preparation method of porous carbon-loaded manganese dioxide nano material

The invention discloses a preparation method of a porous carbon-loaded manganese dioxide nano material. The method comprises the following steps of performing grinding on porous carbon and potassium permanganate according to the mass ratio of 1:4 to 1:16, and dispersing in water, adding concentrated...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KONG YUYU, DIAO GUOWANG, LI XUSEN, ZHANG WANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KONG YUYU
DIAO GUOWANG
LI XUSEN
ZHANG WANG
description The invention discloses a preparation method of a porous carbon-loaded manganese dioxide nano material. The method comprises the following steps of performing grinding on porous carbon and potassium permanganate according to the mass ratio of 1:4 to 1:16, and dispersing in water, adding concentrated sulfuric acid, carrying out stirring and uniformly mixing, and then carrying out water bath heatingreaction to obtain the porous carbon-loaded manganese dioxide nano material. The method disclosed by the invention is simple and feasible, the physical properties of the synthesized nano material arerelatively stable, and the specific capacitance can reach 337 F/g; and when the nano material is used as a supercapacitor material, relatively high electrochemical performance is shown. 本发明公开了一种多孔碳负载二氧化锰纳米材料的制备方法。所述方法将多孔碳和高锰酸钾按质量比为1:4~1:16研磨,分散于水中,并加入浓硫酸搅拌混合均匀后,水浴加热反应得到多孔碳负载二氧化锰纳米材料。本发明方法简便易行,合成的纳米材料的物理性质较为稳定,比电容可达337F/g,作为超级电容器材料具有较好的电化学性能。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110176363A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110176363A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110176363A3</originalsourceid><addsrcrecordid>eNqNyjEKAjEQRuE0FqLeYTzAgiGw1rIoYiEW9su4-dcNZGdCEsHja-EBrB58vKW53DISZ65BhWbUST3pSEmzvgoNnB8qTVT28DSzPFlQQD7oO3iQsOiXK3LguDaLkWPB5teV2Z6O9-7cIGmPkniAoPbd1dqd3beudQf3z_MBQ1w1Rw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of porous carbon-loaded manganese dioxide nano material</title><source>esp@cenet</source><creator>KONG YUYU ; DIAO GUOWANG ; LI XUSEN ; ZHANG WANG</creator><creatorcontrib>KONG YUYU ; DIAO GUOWANG ; LI XUSEN ; ZHANG WANG</creatorcontrib><description>The invention discloses a preparation method of a porous carbon-loaded manganese dioxide nano material. The method comprises the following steps of performing grinding on porous carbon and potassium permanganate according to the mass ratio of 1:4 to 1:16, and dispersing in water, adding concentrated sulfuric acid, carrying out stirring and uniformly mixing, and then carrying out water bath heatingreaction to obtain the porous carbon-loaded manganese dioxide nano material. The method disclosed by the invention is simple and feasible, the physical properties of the synthesized nano material arerelatively stable, and the specific capacitance can reach 337 F/g; and when the nano material is used as a supercapacitor material, relatively high electrochemical performance is shown. 本发明公开了一种多孔碳负载二氧化锰纳米材料的制备方法。所述方法将多孔碳和高锰酸钾按质量比为1:4~1:16研磨,分散于水中,并加入浓硫酸搅拌混合均匀后,水浴加热反应得到多孔碳负载二氧化锰纳米材料。本发明方法简便易行,合成的纳米材料的物理性质较为稳定,比电容可达337F/g,作为超级电容器材料具有较好的电化学性能。</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; CAPACITORS ; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE ; ELECTRICITY ; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES ; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES ; NANOTECHNOLOGY ; PERFORMING OPERATIONS ; SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES ; TRANSPORTING</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190827&amp;DB=EPODOC&amp;CC=CN&amp;NR=110176363A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190827&amp;DB=EPODOC&amp;CC=CN&amp;NR=110176363A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KONG YUYU</creatorcontrib><creatorcontrib>DIAO GUOWANG</creatorcontrib><creatorcontrib>LI XUSEN</creatorcontrib><creatorcontrib>ZHANG WANG</creatorcontrib><title>Preparation method of porous carbon-loaded manganese dioxide nano material</title><description>The invention discloses a preparation method of a porous carbon-loaded manganese dioxide nano material. The method comprises the following steps of performing grinding on porous carbon and potassium permanganate according to the mass ratio of 1:4 to 1:16, and dispersing in water, adding concentrated sulfuric acid, carrying out stirring and uniformly mixing, and then carrying out water bath heatingreaction to obtain the porous carbon-loaded manganese dioxide nano material. The method disclosed by the invention is simple and feasible, the physical properties of the synthesized nano material arerelatively stable, and the specific capacitance can reach 337 F/g; and when the nano material is used as a supercapacitor material, relatively high electrochemical performance is shown. 本发明公开了一种多孔碳负载二氧化锰纳米材料的制备方法。所述方法将多孔碳和高锰酸钾按质量比为1:4~1:16研磨,分散于水中,并加入浓硫酸搅拌混合均匀后,水浴加热反应得到多孔碳负载二氧化锰纳米材料。本发明方法简便易行,合成的纳米材料的物理性质较为稳定,比电容可达337F/g,作为超级电容器材料具有较好的电化学性能。</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CAPACITORS</subject><subject>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</subject><subject>ELECTRICITY</subject><subject>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</subject><subject>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</subject><subject>NANOTECHNOLOGY</subject><subject>PERFORMING OPERATIONS</subject><subject>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEKAjEQRuE0FqLeYTzAgiGw1rIoYiEW9su4-dcNZGdCEsHja-EBrB58vKW53DISZ65BhWbUST3pSEmzvgoNnB8qTVT28DSzPFlQQD7oO3iQsOiXK3LguDaLkWPB5teV2Z6O9-7cIGmPkniAoPbd1dqd3beudQf3z_MBQ1w1Rw</recordid><startdate>20190827</startdate><enddate>20190827</enddate><creator>KONG YUYU</creator><creator>DIAO GUOWANG</creator><creator>LI XUSEN</creator><creator>ZHANG WANG</creator><scope>EVB</scope></search><sort><creationdate>20190827</creationdate><title>Preparation method of porous carbon-loaded manganese dioxide nano material</title><author>KONG YUYU ; DIAO GUOWANG ; LI XUSEN ; ZHANG WANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110176363A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CAPACITORS</topic><topic>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</topic><topic>ELECTRICITY</topic><topic>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</topic><topic>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</topic><topic>NANOTECHNOLOGY</topic><topic>PERFORMING OPERATIONS</topic><topic>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>KONG YUYU</creatorcontrib><creatorcontrib>DIAO GUOWANG</creatorcontrib><creatorcontrib>LI XUSEN</creatorcontrib><creatorcontrib>ZHANG WANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KONG YUYU</au><au>DIAO GUOWANG</au><au>LI XUSEN</au><au>ZHANG WANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of porous carbon-loaded manganese dioxide nano material</title><date>2019-08-27</date><risdate>2019</risdate><abstract>The invention discloses a preparation method of a porous carbon-loaded manganese dioxide nano material. The method comprises the following steps of performing grinding on porous carbon and potassium permanganate according to the mass ratio of 1:4 to 1:16, and dispersing in water, adding concentrated sulfuric acid, carrying out stirring and uniformly mixing, and then carrying out water bath heatingreaction to obtain the porous carbon-loaded manganese dioxide nano material. The method disclosed by the invention is simple and feasible, the physical properties of the synthesized nano material arerelatively stable, and the specific capacitance can reach 337 F/g; and when the nano material is used as a supercapacitor material, relatively high electrochemical performance is shown. 本发明公开了一种多孔碳负载二氧化锰纳米材料的制备方法。所述方法将多孔碳和高锰酸钾按质量比为1:4~1:16研磨,分散于水中,并加入浓硫酸搅拌混合均匀后,水浴加热反应得到多孔碳负载二氧化锰纳米材料。本发明方法简便易行,合成的纳米材料的物理性质较为稳定,比电容可达337F/g,作为超级电容器材料具有较好的电化学性能。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN110176363A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CAPACITORS
CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE
ELECTRICITY
MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES
NANOTECHNOLOGY
PERFORMING OPERATIONS
SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES
TRANSPORTING
title Preparation method of porous carbon-loaded manganese dioxide nano material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-05T09%3A05%3A27IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KONG%20YUYU&rft.date=2019-08-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110176363A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true