Method for preparing high-purity spherical instant boric acid by induction of organic molecules

The invention belongs to the technical field of inorganic functional materials and provides a method for preparing high-purity spherical instant boric acid by induction of organic molecules. The high-purity spherical boric acid with no aggregation is prepared by: dissolving analytically pure boric a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TIAN PENG, PANG HONGCHANG, LIN YUAN, YE JUNWEI, NING GUILING, ZHU PEIHAN, CHENG JUN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TIAN PENG
PANG HONGCHANG
LIN YUAN
YE JUNWEI
NING GUILING
ZHU PEIHAN
CHENG JUN
description The invention belongs to the technical field of inorganic functional materials and provides a method for preparing high-purity spherical instant boric acid by induction of organic molecules. The high-purity spherical boric acid with no aggregation is prepared by: dissolving analytically pure boric acid or industrial boric acid in a hot solvent which is a mixture of water with a lower alcohol, ketone, ether or acid with carbon number of less than 4, cooling the boric acid solution based on the solubility and surface free energy control principle, adjusting exposed crystal face of boric acid crystal and morphology of aggregated particles by inducing crystallization via organic molecules so that recrystallized boric acid microspheres are separated from the oversaturated solution, carrying outsuction filtering, and drying. Instant spherical boric acid powder prepared via the method is simple to operate, the technical conditions are easy to control, consuming a surfactant or aid is not required, material utilizati
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN110054196A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN110054196A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN110054196A3</originalsourceid><addsrcrecordid>eNqNijsOwjAQBd1QIOAOywEiJeIjUaIIRAMVvbVx1vFKxmvZTpHb44IDUD3NzFsr_aTiZAQrCWKiiInDBI4n18Q5cVkgR0eJDXrgkAuGAoNUBjQ8wrBUO86msAQQC5ImDDV-xJOZPeWtWln0mXa_3aj9_fbuHw1F0ZQjGgpUdP_qurY9HbvL-Xr45_MFoiU9Kw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing high-purity spherical instant boric acid by induction of organic molecules</title><source>esp@cenet</source><creator>TIAN PENG ; PANG HONGCHANG ; LIN YUAN ; YE JUNWEI ; NING GUILING ; ZHU PEIHAN ; CHENG JUN</creator><creatorcontrib>TIAN PENG ; PANG HONGCHANG ; LIN YUAN ; YE JUNWEI ; NING GUILING ; ZHU PEIHAN ; CHENG JUN</creatorcontrib><description>The invention belongs to the technical field of inorganic functional materials and provides a method for preparing high-purity spherical instant boric acid by induction of organic molecules. The high-purity spherical boric acid with no aggregation is prepared by: dissolving analytically pure boric acid or industrial boric acid in a hot solvent which is a mixture of water with a lower alcohol, ketone, ether or acid with carbon number of less than 4, cooling the boric acid solution based on the solubility and surface free energy control principle, adjusting exposed crystal face of boric acid crystal and morphology of aggregated particles by inducing crystallization via organic molecules so that recrystallized boric acid microspheres are separated from the oversaturated solution, carrying outsuction filtering, and drying. Instant spherical boric acid powder prepared via the method is simple to operate, the technical conditions are easy to control, consuming a surfactant or aid is not required, material utilizati</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190726&amp;DB=EPODOC&amp;CC=CN&amp;NR=110054196A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190726&amp;DB=EPODOC&amp;CC=CN&amp;NR=110054196A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TIAN PENG</creatorcontrib><creatorcontrib>PANG HONGCHANG</creatorcontrib><creatorcontrib>LIN YUAN</creatorcontrib><creatorcontrib>YE JUNWEI</creatorcontrib><creatorcontrib>NING GUILING</creatorcontrib><creatorcontrib>ZHU PEIHAN</creatorcontrib><creatorcontrib>CHENG JUN</creatorcontrib><title>Method for preparing high-purity spherical instant boric acid by induction of organic molecules</title><description>The invention belongs to the technical field of inorganic functional materials and provides a method for preparing high-purity spherical instant boric acid by induction of organic molecules. The high-purity spherical boric acid with no aggregation is prepared by: dissolving analytically pure boric acid or industrial boric acid in a hot solvent which is a mixture of water with a lower alcohol, ketone, ether or acid with carbon number of less than 4, cooling the boric acid solution based on the solubility and surface free energy control principle, adjusting exposed crystal face of boric acid crystal and morphology of aggregated particles by inducing crystallization via organic molecules so that recrystallized boric acid microspheres are separated from the oversaturated solution, carrying outsuction filtering, and drying. Instant spherical boric acid powder prepared via the method is simple to operate, the technical conditions are easy to control, consuming a surfactant or aid is not required, material utilizati</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNijsOwjAQBd1QIOAOywEiJeIjUaIIRAMVvbVx1vFKxmvZTpHb44IDUD3NzFsr_aTiZAQrCWKiiInDBI4n18Q5cVkgR0eJDXrgkAuGAoNUBjQ8wrBUO86msAQQC5ImDDV-xJOZPeWtWln0mXa_3aj9_fbuHw1F0ZQjGgpUdP_qurY9HbvL-Xr45_MFoiU9Kw</recordid><startdate>20190726</startdate><enddate>20190726</enddate><creator>TIAN PENG</creator><creator>PANG HONGCHANG</creator><creator>LIN YUAN</creator><creator>YE JUNWEI</creator><creator>NING GUILING</creator><creator>ZHU PEIHAN</creator><creator>CHENG JUN</creator><scope>EVB</scope></search><sort><creationdate>20190726</creationdate><title>Method for preparing high-purity spherical instant boric acid by induction of organic molecules</title><author>TIAN PENG ; PANG HONGCHANG ; LIN YUAN ; YE JUNWEI ; NING GUILING ; ZHU PEIHAN ; CHENG JUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN110054196A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>TIAN PENG</creatorcontrib><creatorcontrib>PANG HONGCHANG</creatorcontrib><creatorcontrib>LIN YUAN</creatorcontrib><creatorcontrib>YE JUNWEI</creatorcontrib><creatorcontrib>NING GUILING</creatorcontrib><creatorcontrib>ZHU PEIHAN</creatorcontrib><creatorcontrib>CHENG JUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TIAN PENG</au><au>PANG HONGCHANG</au><au>LIN YUAN</au><au>YE JUNWEI</au><au>NING GUILING</au><au>ZHU PEIHAN</au><au>CHENG JUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing high-purity spherical instant boric acid by induction of organic molecules</title><date>2019-07-26</date><risdate>2019</risdate><abstract>The invention belongs to the technical field of inorganic functional materials and provides a method for preparing high-purity spherical instant boric acid by induction of organic molecules. The high-purity spherical boric acid with no aggregation is prepared by: dissolving analytically pure boric acid or industrial boric acid in a hot solvent which is a mixture of water with a lower alcohol, ketone, ether or acid with carbon number of less than 4, cooling the boric acid solution based on the solubility and surface free energy control principle, adjusting exposed crystal face of boric acid crystal and morphology of aggregated particles by inducing crystallization via organic molecules so that recrystallized boric acid microspheres are separated from the oversaturated solution, carrying outsuction filtering, and drying. Instant spherical boric acid powder prepared via the method is simple to operate, the technical conditions are easy to control, consuming a surfactant or aid is not required, material utilizati</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN110054196A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title Method for preparing high-purity spherical instant boric acid by induction of organic molecules
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T21%3A50%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TIAN%20PENG&rft.date=2019-07-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN110054196A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true