Preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder

The invention provides a preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder. The preparation method comprises the following steps of: (1) weighing luminumoxide dispersion-strengthened copper powder of which the particle size is smaller than 75 microns an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAN ZHIQIAO, WANG SHUNCHENG, LIU ZHENPENG, FU NAIKE, CHEN FENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAN ZHIQIAO
WANG SHUNCHENG
LIU ZHENPENG
FU NAIKE
CHEN FENG
description The invention provides a preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder. The preparation method comprises the following steps of: (1) weighing luminumoxide dispersion-strengthened copper powder of which the particle size is smaller than 75 microns and metal powder of which the particle size is smaller than 45 microns according to a mass ratio, andmixing for 4 h to 8 h; (2) processing the mixed powder for 0.5 h to 4 h at the temperature of 600 DEG C to 900 DEG C in hydrogen atmosphere; (3) crushing the obtained material until the particle sizeof the material is smaller than or equal to 180 microns, and screening the material to form powder which is within four different particle size ranges including 180-150 microns, 15-75 microns, 75-45microns and smaller than 45 microns; and (4) processing the powder for 1 h to 3 h at the temperature of 450 DEG C to 650 DEG C in the hydrogen atmosphere, cooling to room temperature to obtain the aluminum oxide dispersion-stren
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN109530705A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN109530705A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN109530705A3</originalsourceid><addsrcrecordid>eNqNjEsKAjEQRGfjQtQ7tAcIRIZBXMqguBIX7sc43XECSTrkg3p7I3gAV8UrXtW8uV0iBRVVNuzBUZ4YgTUoW5zxxQG_DBKgSYFiqo5IOZJ_5Ik8IYwcai_uKlVAo3X5OnVt-Q2Bn0hx2cy0solWv1w06-Ph2p8EBR4oBTXWpzz0543cda3cym7f_uN8AFp7PmU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder</title><source>esp@cenet</source><creator>YAN ZHIQIAO ; WANG SHUNCHENG ; LIU ZHENPENG ; FU NAIKE ; CHEN FENG</creator><creatorcontrib>YAN ZHIQIAO ; WANG SHUNCHENG ; LIU ZHENPENG ; FU NAIKE ; CHEN FENG</creatorcontrib><description>The invention provides a preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder. The preparation method comprises the following steps of: (1) weighing luminumoxide dispersion-strengthened copper powder of which the particle size is smaller than 75 microns and metal powder of which the particle size is smaller than 45 microns according to a mass ratio, andmixing for 4 h to 8 h; (2) processing the mixed powder for 0.5 h to 4 h at the temperature of 600 DEG C to 900 DEG C in hydrogen atmosphere; (3) crushing the obtained material until the particle sizeof the material is smaller than or equal to 180 microns, and screening the material to form powder which is within four different particle size ranges including 180-150 microns, 15-75 microns, 75-45microns and smaller than 45 microns; and (4) processing the powder for 1 h to 3 h at the temperature of 450 DEG C to 650 DEG C in the hydrogen atmosphere, cooling to room temperature to obtain the aluminum oxide dispersion-stren</description><language>chi ; eng</language><subject>CASTING ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING ; WORKING METALLIC POWDER</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190329&amp;DB=EPODOC&amp;CC=CN&amp;NR=109530705A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190329&amp;DB=EPODOC&amp;CC=CN&amp;NR=109530705A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAN ZHIQIAO</creatorcontrib><creatorcontrib>WANG SHUNCHENG</creatorcontrib><creatorcontrib>LIU ZHENPENG</creatorcontrib><creatorcontrib>FU NAIKE</creatorcontrib><creatorcontrib>CHEN FENG</creatorcontrib><title>Preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder</title><description>The invention provides a preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder. The preparation method comprises the following steps of: (1) weighing luminumoxide dispersion-strengthened copper powder of which the particle size is smaller than 75 microns and metal powder of which the particle size is smaller than 45 microns according to a mass ratio, andmixing for 4 h to 8 h; (2) processing the mixed powder for 0.5 h to 4 h at the temperature of 600 DEG C to 900 DEG C in hydrogen atmosphere; (3) crushing the obtained material until the particle sizeof the material is smaller than or equal to 180 microns, and screening the material to form powder which is within four different particle size ranges including 180-150 microns, 15-75 microns, 75-45microns and smaller than 45 microns; and (4) processing the powder for 1 h to 3 h at the temperature of 450 DEG C to 650 DEG C in the hydrogen atmosphere, cooling to room temperature to obtain the aluminum oxide dispersion-stren</description><subject>CASTING</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEsKAjEQRGfjQtQ7tAcIRIZBXMqguBIX7sc43XECSTrkg3p7I3gAV8UrXtW8uV0iBRVVNuzBUZ4YgTUoW5zxxQG_DBKgSYFiqo5IOZJ_5Ik8IYwcai_uKlVAo3X5OnVt-Q2Bn0hx2cy0solWv1w06-Ph2p8EBR4oBTXWpzz0543cda3cym7f_uN8AFp7PmU</recordid><startdate>20190329</startdate><enddate>20190329</enddate><creator>YAN ZHIQIAO</creator><creator>WANG SHUNCHENG</creator><creator>LIU ZHENPENG</creator><creator>FU NAIKE</creator><creator>CHEN FENG</creator><scope>EVB</scope></search><sort><creationdate>20190329</creationdate><title>Preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder</title><author>YAN ZHIQIAO ; WANG SHUNCHENG ; LIU ZHENPENG ; FU NAIKE ; CHEN FENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN109530705A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>CASTING</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>YAN ZHIQIAO</creatorcontrib><creatorcontrib>WANG SHUNCHENG</creatorcontrib><creatorcontrib>LIU ZHENPENG</creatorcontrib><creatorcontrib>FU NAIKE</creatorcontrib><creatorcontrib>CHEN FENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAN ZHIQIAO</au><au>WANG SHUNCHENG</au><au>LIU ZHENPENG</au><au>FU NAIKE</au><au>CHEN FENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder</title><date>2019-03-29</date><risdate>2019</risdate><abstract>The invention provides a preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder. The preparation method comprises the following steps of: (1) weighing luminumoxide dispersion-strengthened copper powder of which the particle size is smaller than 75 microns and metal powder of which the particle size is smaller than 45 microns according to a mass ratio, andmixing for 4 h to 8 h; (2) processing the mixed powder for 0.5 h to 4 h at the temperature of 600 DEG C to 900 DEG C in hydrogen atmosphere; (3) crushing the obtained material until the particle sizeof the material is smaller than or equal to 180 microns, and screening the material to form powder which is within four different particle size ranges including 180-150 microns, 15-75 microns, 75-45microns and smaller than 45 microns; and (4) processing the powder for 1 h to 3 h at the temperature of 450 DEG C to 650 DEG C in the hydrogen atmosphere, cooling to room temperature to obtain the aluminum oxide dispersion-stren</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN109530705A
source esp@cenet
subjects CASTING
MAKING METALLIC POWDER
MANUFACTURE OF ARTICLES FROM METALLIC POWDER
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
WORKING METALLIC POWDER
title Preparation method of aluminum oxide dispersion-strengthened copper-based diffusion alloy powder
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T15%3A26%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAN%20ZHIQIAO&rft.date=2019-03-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN109530705A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true