Supercritical fluid material mixing method for superfine-granularity ceramic abrasive tool

A supercritical fluid material mixing method for a superfine-granularity ceramic abrasive tool comprises the following steps that (1) according to weight percentage, 25%-50% of abrasive materials, 4%-26% of ceramic binding agent and 1-25% of wetting agent are fed into a high-pressure kettle, and the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU BIN, LI HENAN, XI YAOHUI, WANG ZHIQI, WANG CHAOFU
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU BIN
LI HENAN
XI YAOHUI
WANG ZHIQI
WANG CHAOFU
description A supercritical fluid material mixing method for a superfine-granularity ceramic abrasive tool comprises the following steps that (1) according to weight percentage, 25%-50% of abrasive materials, 4%-26% of ceramic binding agent and 1-25% of wetting agent are fed into a high-pressure kettle, and the high-pressure kettle is sealed; (2) carbon dioxide is fed into the high-pressure kettle, the pressure is adjusted to 72.8 atm, the temperature is adjusted to 31.1 DEG C and above, the carbon dioxide is made to reach the supercritical state, and stirring is conducted for 1-3 h. Researches are conducted for solving the problem that in the superfine abrasive tool preparing process, since the surface energy of powder is high, agglomeration is quite prone to happen, the supercritical liquid carbon dioxide which is quite high in penetration capacity is utilized to fully infiltrate gaps of agglomerated bodies, the purpose of weakening the binding force between particles is achieved, the problem that in the superfine abra
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN109483420A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN109483420A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN109483420A3</originalsourceid><addsrcrecordid>eNqNizsKwkAQQNNYiHqH8QCBaFKYUoJiZaOVTRg3s3Fgf8zuit7eCB7A6vHgvXlxu-RAooQTKzSgTeYBLCYSntTyi90IltLDD6C9QPzmmh2Vo6DLBqfzDYoELSvAu2DkJ0Hy3iyLmUYTafXjolgfD9fuVFLwPcWAihylvjtvqrbZ1c222tf_NB-qmzv_</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Supercritical fluid material mixing method for superfine-granularity ceramic abrasive tool</title><source>esp@cenet</source><creator>LIU BIN ; LI HENAN ; XI YAOHUI ; WANG ZHIQI ; WANG CHAOFU</creator><creatorcontrib>LIU BIN ; LI HENAN ; XI YAOHUI ; WANG ZHIQI ; WANG CHAOFU</creatorcontrib><description>A supercritical fluid material mixing method for a superfine-granularity ceramic abrasive tool comprises the following steps that (1) according to weight percentage, 25%-50% of abrasive materials, 4%-26% of ceramic binding agent and 1-25% of wetting agent are fed into a high-pressure kettle, and the high-pressure kettle is sealed; (2) carbon dioxide is fed into the high-pressure kettle, the pressure is adjusted to 72.8 atm, the temperature is adjusted to 31.1 DEG C and above, the carbon dioxide is made to reach the supercritical state, and stirring is conducted for 1-3 h. Researches are conducted for solving the problem that in the superfine abrasive tool preparing process, since the surface energy of powder is high, agglomeration is quite prone to happen, the supercritical liquid carbon dioxide which is quite high in penetration capacity is utilized to fully infiltrate gaps of agglomerated bodies, the purpose of weakening the binding force between particles is achieved, the problem that in the superfine abra</description><language>chi ; eng</language><subject>GRINDING ; PERFORMING OPERATIONS ; POLISHING ; TOOLS FOR GRINDING, BUFFING, OR SHARPENING ; TRANSPORTING</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190319&amp;DB=EPODOC&amp;CC=CN&amp;NR=109483420A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190319&amp;DB=EPODOC&amp;CC=CN&amp;NR=109483420A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU BIN</creatorcontrib><creatorcontrib>LI HENAN</creatorcontrib><creatorcontrib>XI YAOHUI</creatorcontrib><creatorcontrib>WANG ZHIQI</creatorcontrib><creatorcontrib>WANG CHAOFU</creatorcontrib><title>Supercritical fluid material mixing method for superfine-granularity ceramic abrasive tool</title><description>A supercritical fluid material mixing method for a superfine-granularity ceramic abrasive tool comprises the following steps that (1) according to weight percentage, 25%-50% of abrasive materials, 4%-26% of ceramic binding agent and 1-25% of wetting agent are fed into a high-pressure kettle, and the high-pressure kettle is sealed; (2) carbon dioxide is fed into the high-pressure kettle, the pressure is adjusted to 72.8 atm, the temperature is adjusted to 31.1 DEG C and above, the carbon dioxide is made to reach the supercritical state, and stirring is conducted for 1-3 h. Researches are conducted for solving the problem that in the superfine abrasive tool preparing process, since the surface energy of powder is high, agglomeration is quite prone to happen, the supercritical liquid carbon dioxide which is quite high in penetration capacity is utilized to fully infiltrate gaps of agglomerated bodies, the purpose of weakening the binding force between particles is achieved, the problem that in the superfine abra</description><subject>GRINDING</subject><subject>PERFORMING OPERATIONS</subject><subject>POLISHING</subject><subject>TOOLS FOR GRINDING, BUFFING, OR SHARPENING</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNizsKwkAQQNNYiHqH8QCBaFKYUoJiZaOVTRg3s3Fgf8zuit7eCB7A6vHgvXlxu-RAooQTKzSgTeYBLCYSntTyi90IltLDD6C9QPzmmh2Vo6DLBqfzDYoELSvAu2DkJ0Hy3iyLmUYTafXjolgfD9fuVFLwPcWAihylvjtvqrbZ1c222tf_NB-qmzv_</recordid><startdate>20190319</startdate><enddate>20190319</enddate><creator>LIU BIN</creator><creator>LI HENAN</creator><creator>XI YAOHUI</creator><creator>WANG ZHIQI</creator><creator>WANG CHAOFU</creator><scope>EVB</scope></search><sort><creationdate>20190319</creationdate><title>Supercritical fluid material mixing method for superfine-granularity ceramic abrasive tool</title><author>LIU BIN ; LI HENAN ; XI YAOHUI ; WANG ZHIQI ; WANG CHAOFU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN109483420A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>GRINDING</topic><topic>PERFORMING OPERATIONS</topic><topic>POLISHING</topic><topic>TOOLS FOR GRINDING, BUFFING, OR SHARPENING</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU BIN</creatorcontrib><creatorcontrib>LI HENAN</creatorcontrib><creatorcontrib>XI YAOHUI</creatorcontrib><creatorcontrib>WANG ZHIQI</creatorcontrib><creatorcontrib>WANG CHAOFU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU BIN</au><au>LI HENAN</au><au>XI YAOHUI</au><au>WANG ZHIQI</au><au>WANG CHAOFU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Supercritical fluid material mixing method for superfine-granularity ceramic abrasive tool</title><date>2019-03-19</date><risdate>2019</risdate><abstract>A supercritical fluid material mixing method for a superfine-granularity ceramic abrasive tool comprises the following steps that (1) according to weight percentage, 25%-50% of abrasive materials, 4%-26% of ceramic binding agent and 1-25% of wetting agent are fed into a high-pressure kettle, and the high-pressure kettle is sealed; (2) carbon dioxide is fed into the high-pressure kettle, the pressure is adjusted to 72.8 atm, the temperature is adjusted to 31.1 DEG C and above, the carbon dioxide is made to reach the supercritical state, and stirring is conducted for 1-3 h. Researches are conducted for solving the problem that in the superfine abrasive tool preparing process, since the surface energy of powder is high, agglomeration is quite prone to happen, the supercritical liquid carbon dioxide which is quite high in penetration capacity is utilized to fully infiltrate gaps of agglomerated bodies, the purpose of weakening the binding force between particles is achieved, the problem that in the superfine abra</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN109483420A
source esp@cenet
subjects GRINDING
PERFORMING OPERATIONS
POLISHING
TOOLS FOR GRINDING, BUFFING, OR SHARPENING
TRANSPORTING
title Supercritical fluid material mixing method for superfine-granularity ceramic abrasive tool
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T11%3A35%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20BIN&rft.date=2019-03-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN109483420A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true