Preparation method of silicon nitride rich in fiber morphology

The invention discloses a preparation method of silicon nitride rich in fiber morphology. The preparation method includes weighing 5 wt% of Fe powder and 3 wt% of NH4Cl powder and adding them to Si powder to obtain a powder mixture, subjecting the power mixture to ball milling and mixing uniformly,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG SENJING, YI XUEMEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG SENJING
YI XUEMEI
description The invention discloses a preparation method of silicon nitride rich in fiber morphology. The preparation method includes weighing 5 wt% of Fe powder and 3 wt% of NH4Cl powder and adding them to Si powder to obtain a powder mixture, subjecting the power mixture to ball milling and mixing uniformly, placing the mixture in a high-temperature tube furnace, vacuumizing and introducing nitrogen gas, powering on to heat the mixture to 1300 DEG C and holding the temperature for 4 hours, after finishing reaction, reducing temperature of the furnace to the room temperature, and finally collecting a silicon nitride product. The added Fe powder and NH4Cl powder react to produce a reducing atmosphere containing hydrogen gas, which facilitates gasification of Si powder and catalysis of fibrous siliconnitride; the prepared silicon nitride powder has rich fiber and long length. The preparation method is easy, needs low cost, low energy consumption, short reaction time and simple source of raw materials, and is suitable for
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN109264677A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN109264677A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN109264677A3</originalsourceid><addsrcrecordid>eNrjZLALKEotSCxKLMnMz1PITS3JyE9RyE9TKM7MyUwGiuRllhRlpqQqFGUmZyhk5imkZSalFink5hcVZOTn5KdX8jCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_QwNLIzMTM3NzR2Ni1AAAbfowyQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of silicon nitride rich in fiber morphology</title><source>esp@cenet</source><creator>ZHANG SENJING ; YI XUEMEI</creator><creatorcontrib>ZHANG SENJING ; YI XUEMEI</creatorcontrib><description>The invention discloses a preparation method of silicon nitride rich in fiber morphology. The preparation method includes weighing 5 wt% of Fe powder and 3 wt% of NH4Cl powder and adding them to Si powder to obtain a powder mixture, subjecting the power mixture to ball milling and mixing uniformly, placing the mixture in a high-temperature tube furnace, vacuumizing and introducing nitrogen gas, powering on to heat the mixture to 1300 DEG C and holding the temperature for 4 hours, after finishing reaction, reducing temperature of the furnace to the room temperature, and finally collecting a silicon nitride product. The added Fe powder and NH4Cl powder react to produce a reducing atmosphere containing hydrogen gas, which facilitates gasification of Si powder and catalysis of fibrous siliconnitride; the prepared silicon nitride powder has rich fiber and long length. The preparation method is easy, needs low cost, low energy consumption, short reaction time and simple source of raw materials, and is suitable for</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190125&amp;DB=EPODOC&amp;CC=CN&amp;NR=109264677A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190125&amp;DB=EPODOC&amp;CC=CN&amp;NR=109264677A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG SENJING</creatorcontrib><creatorcontrib>YI XUEMEI</creatorcontrib><title>Preparation method of silicon nitride rich in fiber morphology</title><description>The invention discloses a preparation method of silicon nitride rich in fiber morphology. The preparation method includes weighing 5 wt% of Fe powder and 3 wt% of NH4Cl powder and adding them to Si powder to obtain a powder mixture, subjecting the power mixture to ball milling and mixing uniformly, placing the mixture in a high-temperature tube furnace, vacuumizing and introducing nitrogen gas, powering on to heat the mixture to 1300 DEG C and holding the temperature for 4 hours, after finishing reaction, reducing temperature of the furnace to the room temperature, and finally collecting a silicon nitride product. The added Fe powder and NH4Cl powder react to produce a reducing atmosphere containing hydrogen gas, which facilitates gasification of Si powder and catalysis of fibrous siliconnitride; the prepared silicon nitride powder has rich fiber and long length. The preparation method is easy, needs low cost, low energy consumption, short reaction time and simple source of raw materials, and is suitable for</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLALKEotSCxKLMnMz1PITS3JyE9RyE9TKM7MyUwGiuRllhRlpqQqFGUmZyhk5imkZSalFink5hcVZOTn5KdX8jCwpiXmFKfyQmluBkU31xBnD93Ugvz41OKCxOTUvNSSeGc_QwNLIzMTM3NzR2Ni1AAAbfowyQ</recordid><startdate>20190125</startdate><enddate>20190125</enddate><creator>ZHANG SENJING</creator><creator>YI XUEMEI</creator><scope>EVB</scope></search><sort><creationdate>20190125</creationdate><title>Preparation method of silicon nitride rich in fiber morphology</title><author>ZHANG SENJING ; YI XUEMEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN109264677A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG SENJING</creatorcontrib><creatorcontrib>YI XUEMEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG SENJING</au><au>YI XUEMEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of silicon nitride rich in fiber morphology</title><date>2019-01-25</date><risdate>2019</risdate><abstract>The invention discloses a preparation method of silicon nitride rich in fiber morphology. The preparation method includes weighing 5 wt% of Fe powder and 3 wt% of NH4Cl powder and adding them to Si powder to obtain a powder mixture, subjecting the power mixture to ball milling and mixing uniformly, placing the mixture in a high-temperature tube furnace, vacuumizing and introducing nitrogen gas, powering on to heat the mixture to 1300 DEG C and holding the temperature for 4 hours, after finishing reaction, reducing temperature of the furnace to the room temperature, and finally collecting a silicon nitride product. The added Fe powder and NH4Cl powder react to produce a reducing atmosphere containing hydrogen gas, which facilitates gasification of Si powder and catalysis of fibrous siliconnitride; the prepared silicon nitride powder has rich fiber and long length. The preparation method is easy, needs low cost, low energy consumption, short reaction time and simple source of raw materials, and is suitable for</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN109264677A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title Preparation method of silicon nitride rich in fiber morphology
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-29T15%3A23%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20SENJING&rft.date=2019-01-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN109264677A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true