Alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery
The alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery uses 50% to 80% glycerol low melting point aqueous solution as electrolyte solvent, and adds sodium hydroxide andsodium stannate into cathode solution; the alkaline chloroaluminium mixed solvent sealed colloidal ba...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | CAO DAPING |
description | The alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery uses 50% to 80% glycerol low melting point aqueous solution as electrolyte solvent, and adds sodium hydroxide andsodium stannate into cathode solution; the alkaline chloroaluminium mixed solvent sealed colloidal battery is characterized in that the alkaline chloroaluminium mixed solvent is used as electrolyte solvent. Adding sodium perchlorate and sodium hydroxide into the anode solution; The cathode material is aluminum plate (rod, ring), and the anode material is graphite carbon black molded conductive plate (rod, ring). The cathodes of each group are insulated and sealed between the anodes, and the cathodes of the same group are separated from the anodes by an ion separator. The reaction of the discharge battery is 8Al + 3NaClO4+12H2O=8Al (HO) 3 (s) + 3NaCl: as shown in Figure 1.
本发明提出的碱性氯铝混合溶剂恒压密封胶体蓄电池,以50%至80%甘油低熔点水溶液为电解质溶剂,阴极液加入氢氧化钠,锡酸钠;阳极液加入高氯酸钠,氢氧化钠;阴极材料为铝板(棒、环),阳极材料为石墨碳黒成型导电板(棒、环);各组阴极、阳极间绝缘密封隔离,同组阴极与阳极间以离子隔膜分隔,放电电池 |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN109216782A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN109216782A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN109216782A3</originalsourceid><addsrcrecordid>eNqNyk0KwjAQQOFsXIh6h_EAgq3gz7IUxZUguC9jOsXgJBMyiejt7cIDuHpv8U3NteEnsgsE9sGSBLl4F1zx4N2belDhF4UMVoJmHCcmUi2JQAl5BFaYxfXIcMecKX3mZjIgKy1-nZnl6XhrzyuK0pFGtBQod-2lWh_qarvb183mH_MFbIU42g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery</title><source>esp@cenet</source><creator>CAO DAPING</creator><creatorcontrib>CAO DAPING</creatorcontrib><description>The alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery uses 50% to 80% glycerol low melting point aqueous solution as electrolyte solvent, and adds sodium hydroxide andsodium stannate into cathode solution; the alkaline chloroaluminium mixed solvent sealed colloidal battery is characterized in that the alkaline chloroaluminium mixed solvent is used as electrolyte solvent. Adding sodium perchlorate and sodium hydroxide into the anode solution; The cathode material is aluminum plate (rod, ring), and the anode material is graphite carbon black molded conductive plate (rod, ring). The cathodes of each group are insulated and sealed between the anodes, and the cathodes of the same group are separated from the anodes by an ion separator. The reaction of the discharge battery is 8Al + 3NaClO4+12H2O=8Al (HO) 3 (s) + 3NaCl: as shown in Figure 1.
本发明提出的碱性氯铝混合溶剂恒压密封胶体蓄电池,以50%至80%甘油低熔点水溶液为电解质溶剂,阴极液加入氢氧化钠,锡酸钠;阳极液加入高氯酸钠,氢氧化钠;阴极材料为铝板(棒、环),阳极材料为石墨碳黒成型导电板(棒、环);各组阴极、阳极间绝缘密封隔离,同组阴极与阳极间以离子隔膜分隔,放电电池</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20190115&DB=EPODOC&CC=CN&NR=109216782A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20190115&DB=EPODOC&CC=CN&NR=109216782A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CAO DAPING</creatorcontrib><title>Alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery</title><description>The alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery uses 50% to 80% glycerol low melting point aqueous solution as electrolyte solvent, and adds sodium hydroxide andsodium stannate into cathode solution; the alkaline chloroaluminium mixed solvent sealed colloidal battery is characterized in that the alkaline chloroaluminium mixed solvent is used as electrolyte solvent. Adding sodium perchlorate and sodium hydroxide into the anode solution; The cathode material is aluminum plate (rod, ring), and the anode material is graphite carbon black molded conductive plate (rod, ring). The cathodes of each group are insulated and sealed between the anodes, and the cathodes of the same group are separated from the anodes by an ion separator. The reaction of the discharge battery is 8Al + 3NaClO4+12H2O=8Al (HO) 3 (s) + 3NaCl: as shown in Figure 1.
本发明提出的碱性氯铝混合溶剂恒压密封胶体蓄电池,以50%至80%甘油低熔点水溶液为电解质溶剂,阴极液加入氢氧化钠,锡酸钠;阳极液加入高氯酸钠,氢氧化钠;阴极材料为铝板(棒、环),阳极材料为石墨碳黒成型导电板(棒、环);各组阴极、阳极间绝缘密封隔离,同组阴极与阳极间以离子隔膜分隔,放电电池</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyk0KwjAQQOFsXIh6h_EAgq3gz7IUxZUguC9jOsXgJBMyiejt7cIDuHpv8U3NteEnsgsE9sGSBLl4F1zx4N2belDhF4UMVoJmHCcmUi2JQAl5BFaYxfXIcMecKX3mZjIgKy1-nZnl6XhrzyuK0pFGtBQod-2lWh_qarvb183mH_MFbIU42g</recordid><startdate>20190115</startdate><enddate>20190115</enddate><creator>CAO DAPING</creator><scope>EVB</scope></search><sort><creationdate>20190115</creationdate><title>Alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery</title><author>CAO DAPING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN109216782A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>CAO DAPING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CAO DAPING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery</title><date>2019-01-15</date><risdate>2019</risdate><abstract>The alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery uses 50% to 80% glycerol low melting point aqueous solution as electrolyte solvent, and adds sodium hydroxide andsodium stannate into cathode solution; the alkaline chloroaluminium mixed solvent sealed colloidal battery is characterized in that the alkaline chloroaluminium mixed solvent is used as electrolyte solvent. Adding sodium perchlorate and sodium hydroxide into the anode solution; The cathode material is aluminum plate (rod, ring), and the anode material is graphite carbon black molded conductive plate (rod, ring). The cathodes of each group are insulated and sealed between the anodes, and the cathodes of the same group are separated from the anodes by an ion separator. The reaction of the discharge battery is 8Al + 3NaClO4+12H2O=8Al (HO) 3 (s) + 3NaCl: as shown in Figure 1.
本发明提出的碱性氯铝混合溶剂恒压密封胶体蓄电池,以50%至80%甘油低熔点水溶液为电解质溶剂,阴极液加入氢氧化钠,锡酸钠;阳极液加入高氯酸钠,氢氧化钠;阴极材料为铝板(棒、环),阳极材料为石墨碳黒成型导电板(棒、环);各组阴极、阳极间绝缘密封隔离,同组阴极与阳极间以离子隔膜分隔,放电电池</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN109216782A |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS ELECTRICITY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
title | Alkaline chloroaluminium mixed solvent constant pressure sealed colloidal battery |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T07%3A53%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CAO%20DAPING&rft.date=2019-01-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN109216782A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |