Processing method of tempered glass subjected to bending deformation

The invention discloses a processing method of tempered glass subjected to bending deformation. The processing method of the tempered glass subjected to bending deformation includes the following steps that S1, the tempered glass subjected to bending deformation is provided; S2, the tempered glass i...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WU YUFENG, LI CHENGLONG, CAI HANYE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WU YUFENG
LI CHENGLONG
CAI HANYE
description The invention discloses a processing method of tempered glass subjected to bending deformation. The processing method of the tempered glass subjected to bending deformation includes the following steps that S1, the tempered glass subjected to bending deformation is provided; S2, the tempered glass is washed; S3, an acid solution is adopted to soak and process the tempered glass, so that the tempered layer on the surface of the tempered glass is removed; S4, the surface of the tempered glass is polished. According to the processing method of the tempered glass subjected to bending deformation,the acid solution is adopted to soak and process the tempered glass, the tempered layer on the surface of the tempered glass is removed, stress is released, and therefore the stresses on the two facesof the tempered glass are balanced; the processed tempered glass can be subjected to cutting, tempering and the like again, so that defective products of the tempered glass subjected to bending deformation are recycled, and t
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN109133660A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN109133660A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN109133660A3</originalsourceid><addsrcrecordid>eNrjZHAJKMpPTi0uzsxLV8hNLcnIT1HIT1MoSc0tSC1KTVFIz0ksLlYoLk3KSk0uAfJL8hWSUvNSQKpTUtPyi3ITSzLz83gYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GBpaGxsZmZgaMxMWoA1_gzEw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Processing method of tempered glass subjected to bending deformation</title><source>esp@cenet</source><creator>WU YUFENG ; LI CHENGLONG ; CAI HANYE</creator><creatorcontrib>WU YUFENG ; LI CHENGLONG ; CAI HANYE</creatorcontrib><description>The invention discloses a processing method of tempered glass subjected to bending deformation. The processing method of the tempered glass subjected to bending deformation includes the following steps that S1, the tempered glass subjected to bending deformation is provided; S2, the tempered glass is washed; S3, an acid solution is adopted to soak and process the tempered glass, so that the tempered layer on the surface of the tempered glass is removed; S4, the surface of the tempered glass is polished. According to the processing method of the tempered glass subjected to bending deformation,the acid solution is adopted to soak and process the tempered glass, the tempered layer on the surface of the tempered glass is removed, stress is released, and therefore the stresses on the two facesof the tempered glass are balanced; the processed tempered glass can be subjected to cutting, tempering and the like again, so that defective products of the tempered glass subjected to bending deformation are recycled, and t</description><language>chi ; eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190104&amp;DB=EPODOC&amp;CC=CN&amp;NR=109133660A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190104&amp;DB=EPODOC&amp;CC=CN&amp;NR=109133660A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WU YUFENG</creatorcontrib><creatorcontrib>LI CHENGLONG</creatorcontrib><creatorcontrib>CAI HANYE</creatorcontrib><title>Processing method of tempered glass subjected to bending deformation</title><description>The invention discloses a processing method of tempered glass subjected to bending deformation. The processing method of the tempered glass subjected to bending deformation includes the following steps that S1, the tempered glass subjected to bending deformation is provided; S2, the tempered glass is washed; S3, an acid solution is adopted to soak and process the tempered glass, so that the tempered layer on the surface of the tempered glass is removed; S4, the surface of the tempered glass is polished. According to the processing method of the tempered glass subjected to bending deformation,the acid solution is adopted to soak and process the tempered glass, the tempered layer on the surface of the tempered glass is removed, stress is released, and therefore the stresses on the two facesof the tempered glass are balanced; the processed tempered glass can be subjected to cutting, tempering and the like again, so that defective products of the tempered glass subjected to bending deformation are recycled, and t</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAJKMpPTi0uzsxLV8hNLcnIT1HIT1MoSc0tSC1KTVFIz0ksLlYoLk3KSk0uAfJL8hWSUvNSQKpTUtPyi3ITSzLz83gYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GBpaGxsZmZgaMxMWoA1_gzEw</recordid><startdate>20190104</startdate><enddate>20190104</enddate><creator>WU YUFENG</creator><creator>LI CHENGLONG</creator><creator>CAI HANYE</creator><scope>EVB</scope></search><sort><creationdate>20190104</creationdate><title>Processing method of tempered glass subjected to bending deformation</title><author>WU YUFENG ; LI CHENGLONG ; CAI HANYE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN109133660A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2019</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>WU YUFENG</creatorcontrib><creatorcontrib>LI CHENGLONG</creatorcontrib><creatorcontrib>CAI HANYE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WU YUFENG</au><au>LI CHENGLONG</au><au>CAI HANYE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Processing method of tempered glass subjected to bending deformation</title><date>2019-01-04</date><risdate>2019</risdate><abstract>The invention discloses a processing method of tempered glass subjected to bending deformation. The processing method of the tempered glass subjected to bending deformation includes the following steps that S1, the tempered glass subjected to bending deformation is provided; S2, the tempered glass is washed; S3, an acid solution is adopted to soak and process the tempered glass, so that the tempered layer on the surface of the tempered glass is removed; S4, the surface of the tempered glass is polished. According to the processing method of the tempered glass subjected to bending deformation,the acid solution is adopted to soak and process the tempered glass, the tempered layer on the surface of the tempered glass is removed, stress is released, and therefore the stresses on the two facesof the tempered glass are balanced; the processed tempered glass can be subjected to cutting, tempering and the like again, so that defective products of the tempered glass subjected to bending deformation are recycled, and t</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN109133660A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title Processing method of tempered glass subjected to bending deformation
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T19%3A16%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WU%20YUFENG&rft.date=2019-01-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN109133660A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true