Preparation method of complex modified montmorillonite

The invention discloses a preparation method of complex modified montmorillonite. The method adopting sodium montmorillonite as a raw material and a chelating agent diethylenetriamine as a modifier comprises the following steps: adding a diethylenetriamine solution into a sodium montmorillonite susp...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG ALONG, WANG FENGYUN, XU YING, XIA MINGZHU, YANG LEI, LEI WU, CHU YUTING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG ALONG
WANG FENGYUN
XU YING
XIA MINGZHU
YANG LEI
LEI WU
CHU YUTING
description The invention discloses a preparation method of complex modified montmorillonite. The method adopting sodium montmorillonite as a raw material and a chelating agent diethylenetriamine as a modifier comprises the following steps: adding a diethylenetriamine solution into a sodium montmorillonite suspension, stirring and reacting the diethylenetriamine solution and the sodium montmorillonite suspension under a 20-80 DEG C water bath condition for 2-24 h, carrying out suction filtration, and washing and drying the obtained reaction product to obtain the modified montmorillonite, wherein the moleof the diethylenetriamine is 80-120% of the cation exchange capacity of the sodium montmorillonite. The modified montmorillonite obtained through the method can effectively adsorb Pb (II), Cd (II) andother toxic heavy metal ions in an aqueous solution as an adsorbent, and has a high adsorption efficiency, the adsorption rate can reach 98.4% or more when the initial concentration of Pb ions is less than 100 mg/L, the modif
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN108686717A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN108686717A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN108686717A3</originalsourceid><addsrcrecordid>eNrjZDALKEotSCxKLMnMz1PITS3JyE9RyE9TSM7PLchJrVDIzU_JTMtMTQEy8kpy84syc3Ly8zJLUnkYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GBhZmFmbmhuaMxMWoA6N4uVQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of complex modified montmorillonite</title><source>esp@cenet</source><creator>WANG ALONG ; WANG FENGYUN ; XU YING ; XIA MINGZHU ; YANG LEI ; LEI WU ; CHU YUTING</creator><creatorcontrib>WANG ALONG ; WANG FENGYUN ; XU YING ; XIA MINGZHU ; YANG LEI ; LEI WU ; CHU YUTING</creatorcontrib><description>The invention discloses a preparation method of complex modified montmorillonite. The method adopting sodium montmorillonite as a raw material and a chelating agent diethylenetriamine as a modifier comprises the following steps: adding a diethylenetriamine solution into a sodium montmorillonite suspension, stirring and reacting the diethylenetriamine solution and the sodium montmorillonite suspension under a 20-80 DEG C water bath condition for 2-24 h, carrying out suction filtration, and washing and drying the obtained reaction product to obtain the modified montmorillonite, wherein the moleof the diethylenetriamine is 80-120% of the cation exchange capacity of the sodium montmorillonite. The modified montmorillonite obtained through the method can effectively adsorb Pb (II), Cd (II) andother toxic heavy metal ions in an aqueous solution as an adsorbent, and has a high adsorption efficiency, the adsorption rate can reach 98.4% or more when the initial concentration of Pb ions is less than 100 mg/L, the modif</description><language>chi ; eng</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181023&amp;DB=EPODOC&amp;CC=CN&amp;NR=108686717A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20181023&amp;DB=EPODOC&amp;CC=CN&amp;NR=108686717A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG ALONG</creatorcontrib><creatorcontrib>WANG FENGYUN</creatorcontrib><creatorcontrib>XU YING</creatorcontrib><creatorcontrib>XIA MINGZHU</creatorcontrib><creatorcontrib>YANG LEI</creatorcontrib><creatorcontrib>LEI WU</creatorcontrib><creatorcontrib>CHU YUTING</creatorcontrib><title>Preparation method of complex modified montmorillonite</title><description>The invention discloses a preparation method of complex modified montmorillonite. The method adopting sodium montmorillonite as a raw material and a chelating agent diethylenetriamine as a modifier comprises the following steps: adding a diethylenetriamine solution into a sodium montmorillonite suspension, stirring and reacting the diethylenetriamine solution and the sodium montmorillonite suspension under a 20-80 DEG C water bath condition for 2-24 h, carrying out suction filtration, and washing and drying the obtained reaction product to obtain the modified montmorillonite, wherein the moleof the diethylenetriamine is 80-120% of the cation exchange capacity of the sodium montmorillonite. The modified montmorillonite obtained through the method can effectively adsorb Pb (II), Cd (II) andother toxic heavy metal ions in an aqueous solution as an adsorbent, and has a high adsorption efficiency, the adsorption rate can reach 98.4% or more when the initial concentration of Pb ions is less than 100 mg/L, the modif</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDALKEotSCxKLMnMz1PITS3JyE9RyE9TSM7PLchJrVDIzU_JTMtMTQEy8kpy84syc3Ly8zJLUnkYWNMSc4pTeaE0N4Oim2uIs4duakF-fGpxQWJyal5qSbyzn6GBhZmFmbmhuaMxMWoA6N4uVQ</recordid><startdate>20181023</startdate><enddate>20181023</enddate><creator>WANG ALONG</creator><creator>WANG FENGYUN</creator><creator>XU YING</creator><creator>XIA MINGZHU</creator><creator>YANG LEI</creator><creator>LEI WU</creator><creator>CHU YUTING</creator><scope>EVB</scope></search><sort><creationdate>20181023</creationdate><title>Preparation method of complex modified montmorillonite</title><author>WANG ALONG ; WANG FENGYUN ; XU YING ; XIA MINGZHU ; YANG LEI ; LEI WU ; CHU YUTING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN108686717A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2018</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG ALONG</creatorcontrib><creatorcontrib>WANG FENGYUN</creatorcontrib><creatorcontrib>XU YING</creatorcontrib><creatorcontrib>XIA MINGZHU</creatorcontrib><creatorcontrib>YANG LEI</creatorcontrib><creatorcontrib>LEI WU</creatorcontrib><creatorcontrib>CHU YUTING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG ALONG</au><au>WANG FENGYUN</au><au>XU YING</au><au>XIA MINGZHU</au><au>YANG LEI</au><au>LEI WU</au><au>CHU YUTING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of complex modified montmorillonite</title><date>2018-10-23</date><risdate>2018</risdate><abstract>The invention discloses a preparation method of complex modified montmorillonite. The method adopting sodium montmorillonite as a raw material and a chelating agent diethylenetriamine as a modifier comprises the following steps: adding a diethylenetriamine solution into a sodium montmorillonite suspension, stirring and reacting the diethylenetriamine solution and the sodium montmorillonite suspension under a 20-80 DEG C water bath condition for 2-24 h, carrying out suction filtration, and washing and drying the obtained reaction product to obtain the modified montmorillonite, wherein the moleof the diethylenetriamine is 80-120% of the cation exchange capacity of the sodium montmorillonite. The modified montmorillonite obtained through the method can effectively adsorb Pb (II), Cd (II) andother toxic heavy metal ions in an aqueous solution as an adsorbent, and has a high adsorption efficiency, the adsorption rate can reach 98.4% or more when the initial concentration of Pb ions is less than 100 mg/L, the modif</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN108686717A
source esp@cenet
subjects CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
THEIR RELEVANT APPARATUS
TRANSPORTING
TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE
title Preparation method of complex modified montmorillonite
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T08%3A38%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20ALONG&rft.date=2018-10-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN108686717A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true