Comprehensive recovery method for copper smelted slag
The invention provides a comprehensive recovery method for copper smelted slag. The method comprises the following steps: carrying out reductive fuming and settlement on the smelted slag by using a CRfurnace to recover valuable metals in the smelted slag comprehensively; and making harmless slag, wh...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LIANG SHUAIBIAO RU HONGSHUN LI BING ZHOU GANG LI FENG JIANG JIMU LU ZHIFANG LI MIN LU JINZHONG LIU KAI WEI KEJIAN LI DONGBO LIU CHENG CAO KEFEI YAN JIE ZHANG HAIXIN |
description | The invention provides a comprehensive recovery method for copper smelted slag. The method comprises the following steps: carrying out reductive fuming and settlement on the smelted slag by using a CRfurnace to recover valuable metals in the smelted slag comprehensively; and making harmless slag, wherein the CR furnace comprises a cavity which comprises a reductive fuming cavity and a settlementcavity communicating to each other; the step of recovering the valuable metals in the recovered smelted slag comprises the following steps: carrying out reductive fuming treatment on the smelted slagin the reductive fuming cavity to obtain value metal soot and reduced slag; and settling the reduced slag in the settlement cavity to obtain copper matte and harmless slag; or settling the smelted slag in the settlement cavity to obtain copper matte and settled slag; and carrying out reductive fuming treatment on the settled slag in the reductive fuming cavity to obtain valuable metal soot and harmless slag. According to th |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN108611499A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN108611499A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN108611499A3</originalsourceid><addsrcrecordid>eNrjZDB1zs8tKErNSM0rzixLVShKTc4vSy2qVMhNLcnIT1FIyy9SSM4vKEgtUijOTc0pSU1RKM5JTOdhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoYGFmaGhiaWlo7GxKgBAJtALZc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Comprehensive recovery method for copper smelted slag</title><source>esp@cenet</source><creator>LIANG SHUAIBIAO ; RU HONGSHUN ; LI BING ; ZHOU GANG ; LI FENG ; JIANG JIMU ; LU ZHIFANG ; LI MIN ; LU JINZHONG ; LIU KAI ; WEI KEJIAN ; LI DONGBO ; LIU CHENG ; CAO KEFEI ; YAN JIE ; ZHANG HAIXIN</creator><creatorcontrib>LIANG SHUAIBIAO ; RU HONGSHUN ; LI BING ; ZHOU GANG ; LI FENG ; JIANG JIMU ; LU ZHIFANG ; LI MIN ; LU JINZHONG ; LIU KAI ; WEI KEJIAN ; LI DONGBO ; LIU CHENG ; CAO KEFEI ; YAN JIE ; ZHANG HAIXIN</creatorcontrib><description>The invention provides a comprehensive recovery method for copper smelted slag. The method comprises the following steps: carrying out reductive fuming and settlement on the smelted slag by using a CRfurnace to recover valuable metals in the smelted slag comprehensively; and making harmless slag, wherein the CR furnace comprises a cavity which comprises a reductive fuming cavity and a settlementcavity communicating to each other; the step of recovering the valuable metals in the recovered smelted slag comprises the following steps: carrying out reductive fuming treatment on the smelted slagin the reductive fuming cavity to obtain value metal soot and reduced slag; and settling the reduced slag in the settlement cavity to obtain copper matte and harmless slag; or settling the smelted slag in the settlement cavity to obtain copper matte and settled slag; and carrying out reductive fuming treatment on the settled slag in the reductive fuming cavity to obtain valuable metal soot and harmless slag. According to th</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20181002&DB=EPODOC&CC=CN&NR=108611499A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20181002&DB=EPODOC&CC=CN&NR=108611499A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIANG SHUAIBIAO</creatorcontrib><creatorcontrib>RU HONGSHUN</creatorcontrib><creatorcontrib>LI BING</creatorcontrib><creatorcontrib>ZHOU GANG</creatorcontrib><creatorcontrib>LI FENG</creatorcontrib><creatorcontrib>JIANG JIMU</creatorcontrib><creatorcontrib>LU ZHIFANG</creatorcontrib><creatorcontrib>LI MIN</creatorcontrib><creatorcontrib>LU JINZHONG</creatorcontrib><creatorcontrib>LIU KAI</creatorcontrib><creatorcontrib>WEI KEJIAN</creatorcontrib><creatorcontrib>LI DONGBO</creatorcontrib><creatorcontrib>LIU CHENG</creatorcontrib><creatorcontrib>CAO KEFEI</creatorcontrib><creatorcontrib>YAN JIE</creatorcontrib><creatorcontrib>ZHANG HAIXIN</creatorcontrib><title>Comprehensive recovery method for copper smelted slag</title><description>The invention provides a comprehensive recovery method for copper smelted slag. The method comprises the following steps: carrying out reductive fuming and settlement on the smelted slag by using a CRfurnace to recover valuable metals in the smelted slag comprehensively; and making harmless slag, wherein the CR furnace comprises a cavity which comprises a reductive fuming cavity and a settlementcavity communicating to each other; the step of recovering the valuable metals in the recovered smelted slag comprises the following steps: carrying out reductive fuming treatment on the smelted slagin the reductive fuming cavity to obtain value metal soot and reduced slag; and settling the reduced slag in the settlement cavity to obtain copper matte and harmless slag; or settling the smelted slag in the settlement cavity to obtain copper matte and settled slag; and carrying out reductive fuming treatment on the settled slag in the reductive fuming cavity to obtain valuable metal soot and harmless slag. According to th</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB1zs8tKErNSM0rzixLVShKTc4vSy2qVMhNLcnIT1FIyy9SSM4vKEgtUijOTc0pSU1RKM5JTOdhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoYGFmaGhiaWlo7GxKgBAJtALZc</recordid><startdate>20181002</startdate><enddate>20181002</enddate><creator>LIANG SHUAIBIAO</creator><creator>RU HONGSHUN</creator><creator>LI BING</creator><creator>ZHOU GANG</creator><creator>LI FENG</creator><creator>JIANG JIMU</creator><creator>LU ZHIFANG</creator><creator>LI MIN</creator><creator>LU JINZHONG</creator><creator>LIU KAI</creator><creator>WEI KEJIAN</creator><creator>LI DONGBO</creator><creator>LIU CHENG</creator><creator>CAO KEFEI</creator><creator>YAN JIE</creator><creator>ZHANG HAIXIN</creator><scope>EVB</scope></search><sort><creationdate>20181002</creationdate><title>Comprehensive recovery method for copper smelted slag</title><author>LIANG SHUAIBIAO ; RU HONGSHUN ; LI BING ; ZHOU GANG ; LI FENG ; JIANG JIMU ; LU ZHIFANG ; LI MIN ; LU JINZHONG ; LIU KAI ; WEI KEJIAN ; LI DONGBO ; LIU CHENG ; CAO KEFEI ; YAN JIE ; ZHANG HAIXIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN108611499A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2018</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LIANG SHUAIBIAO</creatorcontrib><creatorcontrib>RU HONGSHUN</creatorcontrib><creatorcontrib>LI BING</creatorcontrib><creatorcontrib>ZHOU GANG</creatorcontrib><creatorcontrib>LI FENG</creatorcontrib><creatorcontrib>JIANG JIMU</creatorcontrib><creatorcontrib>LU ZHIFANG</creatorcontrib><creatorcontrib>LI MIN</creatorcontrib><creatorcontrib>LU JINZHONG</creatorcontrib><creatorcontrib>LIU KAI</creatorcontrib><creatorcontrib>WEI KEJIAN</creatorcontrib><creatorcontrib>LI DONGBO</creatorcontrib><creatorcontrib>LIU CHENG</creatorcontrib><creatorcontrib>CAO KEFEI</creatorcontrib><creatorcontrib>YAN JIE</creatorcontrib><creatorcontrib>ZHANG HAIXIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIANG SHUAIBIAO</au><au>RU HONGSHUN</au><au>LI BING</au><au>ZHOU GANG</au><au>LI FENG</au><au>JIANG JIMU</au><au>LU ZHIFANG</au><au>LI MIN</au><au>LU JINZHONG</au><au>LIU KAI</au><au>WEI KEJIAN</au><au>LI DONGBO</au><au>LIU CHENG</au><au>CAO KEFEI</au><au>YAN JIE</au><au>ZHANG HAIXIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Comprehensive recovery method for copper smelted slag</title><date>2018-10-02</date><risdate>2018</risdate><abstract>The invention provides a comprehensive recovery method for copper smelted slag. The method comprises the following steps: carrying out reductive fuming and settlement on the smelted slag by using a CRfurnace to recover valuable metals in the smelted slag comprehensively; and making harmless slag, wherein the CR furnace comprises a cavity which comprises a reductive fuming cavity and a settlementcavity communicating to each other; the step of recovering the valuable metals in the recovered smelted slag comprises the following steps: carrying out reductive fuming treatment on the smelted slagin the reductive fuming cavity to obtain value metal soot and reduced slag; and settling the reduced slag in the settlement cavity to obtain copper matte and harmless slag; or settling the smelted slag in the settlement cavity to obtain copper matte and settled slag; and carrying out reductive fuming treatment on the settled slag in the reductive fuming cavity to obtain valuable metal soot and harmless slag. According to th</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN108611499A |
source | esp@cenet |
subjects | CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Comprehensive recovery method for copper smelted slag |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T00%3A25%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIANG%20SHUAIBIAO&rft.date=2018-10-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN108611499A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |