Construction method for crystallizing of sandstone ground stone materials

The invention discloses a construction method for crystallizing of sandstone ground stone materials. The construction method comprises the steps that (1) white cement is smeared on the bottom faces ofthe sandstone stone materials, the sandstone stone materials are laid on the ground, and a gap betwe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG JIAN, YANG LIANG, GENG XIAOCHAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG JIAN
YANG LIANG
GENG XIAOCHAO
description The invention discloses a construction method for crystallizing of sandstone ground stone materials. The construction method comprises the steps that (1) white cement is smeared on the bottom faces ofthe sandstone stone materials, the sandstone stone materials are laid on the ground, and a gap between every two adjacent sandstone stone materials is 3-5 mm; (2) protective agents are smeared on thesurfaces of the sandstone stone materials, after the protective agents are absorbed by the sandstone stone materials, waterproof films are laid on the surfaces of the sandstone stone materials in a covering mode, and natural air drying is conducted for at least 10 days; (3) hollowing positions of the sandstone stone materials are subjected to potting treatment; (4) the edges of the sandstone stone materials are cut, and thus the gap between every two adjacent sandstone stone materials is 3-5 mm; and (5) the gap between every two adjacent sandstone stone materials is subjected to caulking treatment through marble glue.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN108487582A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN108487582A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN108487582A3</originalsourceid><addsrcrecordid>eNrjZPB0zs8rLikqTS7JzM9TyE0tychPUUjLL1JILqosLknMycmsysxLV8hPUyhOzEspLsnPS1VIL8ovzUtRgHByE0tSizITc4p5GFjTgFQqL5TmZlB0cw1x9tBNLciPTy0uSExOzUstiXf2MzSwMLEwN7UwcjQmRg0AZ2Y1xg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Construction method for crystallizing of sandstone ground stone materials</title><source>esp@cenet</source><creator>WANG JIAN ; YANG LIANG ; GENG XIAOCHAO</creator><creatorcontrib>WANG JIAN ; YANG LIANG ; GENG XIAOCHAO</creatorcontrib><description>The invention discloses a construction method for crystallizing of sandstone ground stone materials. The construction method comprises the steps that (1) white cement is smeared on the bottom faces ofthe sandstone stone materials, the sandstone stone materials are laid on the ground, and a gap between every two adjacent sandstone stone materials is 3-5 mm; (2) protective agents are smeared on thesurfaces of the sandstone stone materials, after the protective agents are absorbed by the sandstone stone materials, waterproof films are laid on the surfaces of the sandstone stone materials in a covering mode, and natural air drying is conducted for at least 10 days; (3) hollowing positions of the sandstone stone materials are subjected to potting treatment; (4) the edges of the sandstone stone materials are cut, and thus the gap between every two adjacent sandstone stone materials is 3-5 mm; and (5) the gap between every two adjacent sandstone stone materials is subjected to caulking treatment through marble glue.</description><language>chi ; eng</language><subject>BUILDING ; FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS ; FIXED CONSTRUCTIONS</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180904&amp;DB=EPODOC&amp;CC=CN&amp;NR=108487582A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180904&amp;DB=EPODOC&amp;CC=CN&amp;NR=108487582A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG JIAN</creatorcontrib><creatorcontrib>YANG LIANG</creatorcontrib><creatorcontrib>GENG XIAOCHAO</creatorcontrib><title>Construction method for crystallizing of sandstone ground stone materials</title><description>The invention discloses a construction method for crystallizing of sandstone ground stone materials. The construction method comprises the steps that (1) white cement is smeared on the bottom faces ofthe sandstone stone materials, the sandstone stone materials are laid on the ground, and a gap between every two adjacent sandstone stone materials is 3-5 mm; (2) protective agents are smeared on thesurfaces of the sandstone stone materials, after the protective agents are absorbed by the sandstone stone materials, waterproof films are laid on the surfaces of the sandstone stone materials in a covering mode, and natural air drying is conducted for at least 10 days; (3) hollowing positions of the sandstone stone materials are subjected to potting treatment; (4) the edges of the sandstone stone materials are cut, and thus the gap between every two adjacent sandstone stone materials is 3-5 mm; and (5) the gap between every two adjacent sandstone stone materials is subjected to caulking treatment through marble glue.</description><subject>BUILDING</subject><subject>FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS</subject><subject>FIXED CONSTRUCTIONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPB0zs8rLikqTS7JzM9TyE0tychPUUjLL1JILqosLknMycmsysxLV8hPUyhOzEspLsnPS1VIL8ovzUtRgHByE0tSizITc4p5GFjTgFQqL5TmZlB0cw1x9tBNLciPTy0uSExOzUstiXf2MzSwMLEwN7UwcjQmRg0AZ2Y1xg</recordid><startdate>20180904</startdate><enddate>20180904</enddate><creator>WANG JIAN</creator><creator>YANG LIANG</creator><creator>GENG XIAOCHAO</creator><scope>EVB</scope></search><sort><creationdate>20180904</creationdate><title>Construction method for crystallizing of sandstone ground stone materials</title><author>WANG JIAN ; YANG LIANG ; GENG XIAOCHAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN108487582A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2018</creationdate><topic>BUILDING</topic><topic>FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS</topic><topic>FIXED CONSTRUCTIONS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG JIAN</creatorcontrib><creatorcontrib>YANG LIANG</creatorcontrib><creatorcontrib>GENG XIAOCHAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG JIAN</au><au>YANG LIANG</au><au>GENG XIAOCHAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Construction method for crystallizing of sandstone ground stone materials</title><date>2018-09-04</date><risdate>2018</risdate><abstract>The invention discloses a construction method for crystallizing of sandstone ground stone materials. The construction method comprises the steps that (1) white cement is smeared on the bottom faces ofthe sandstone stone materials, the sandstone stone materials are laid on the ground, and a gap between every two adjacent sandstone stone materials is 3-5 mm; (2) protective agents are smeared on thesurfaces of the sandstone stone materials, after the protective agents are absorbed by the sandstone stone materials, waterproof films are laid on the surfaces of the sandstone stone materials in a covering mode, and natural air drying is conducted for at least 10 days; (3) hollowing positions of the sandstone stone materials are subjected to potting treatment; (4) the edges of the sandstone stone materials are cut, and thus the gap between every two adjacent sandstone stone materials is 3-5 mm; and (5) the gap between every two adjacent sandstone stone materials is subjected to caulking treatment through marble glue.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN108487582A
source esp@cenet
subjects BUILDING
FINISHING WORK ON BUILDINGS, e.g. STAIRS, FLOORS
FIXED CONSTRUCTIONS
title Construction method for crystallizing of sandstone ground stone materials
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-17T20%3A55%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20JIAN&rft.date=2018-09-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN108487582A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true