Strip steel coiling tension control method and device

The invention relates to the field of steel rolling, in particular to a trip steel coiling tension control method. The method comprises the steps that when the strip steel head enters a belt wrapper,the coiling tension value is controlled to 35 to 65 MPa; when the belt wrapper descends and delays fo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU WANHUI, WAN JUN, TANG WEI, WANG FEI, REN QIUHONG, QI HAIFENG, LI JING, WANG DONGYANG, WANG SHAOFEI, WANG XISHUO, REN XINYI, MENG FANTONG, LIU YUQI, DOU AIMIN, QI JINCHAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU WANHUI
WAN JUN
TANG WEI
WANG FEI
REN QIUHONG
QI HAIFENG
LI JING
WANG DONGYANG
WANG SHAOFEI
WANG XISHUO
REN XINYI
MENG FANTONG
LIU YUQI
DOU AIMIN
QI JINCHAO
description The invention relates to the field of steel rolling, in particular to a trip steel coiling tension control method. The method comprises the steps that when the strip steel head enters a belt wrapper,the coiling tension value is controlled to 35 to 65 MPa; when the belt wrapper descends and delays for 4 to 5 seconds, the coiling tension value is controlled to be stepped to 50.05 to 92.95 MPa, then, the value is gradually reduced to 38.5 to 71.5 MPa; when the length of coiled strip steel reaches 1/5 of the total length of the strip steel, the coiling tension value is controlled to be graduallyreduced to 35 to 65 MPa; when the length of the coiled strip steel reaches 3/5 of the total length of the strip steel, the coiling tension value is controlled to be kept 35 to 65 MPa; when the lengthof the coiled strip steel reaches 4/5 of the total length of the strip steel, the coiling tension value is controlled to be gradually increased to 36.75 to 68.25 MPa until strip steel coiling is finished. According to the coili
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN108405653A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN108405653A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN108405653A3</originalsourceid><addsrcrecordid>eNrjZDANLinKLFAoLklNzVFIzs_MycxLVyhJzSvOzM8D8vNKivJzFHJTSzLyUxQS81IUUlLLMpNTeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGFiYGpmamxozExagBwrS01</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Strip steel coiling tension control method and device</title><source>esp@cenet</source><creator>LIU WANHUI ; WAN JUN ; TANG WEI ; WANG FEI ; REN QIUHONG ; QI HAIFENG ; LI JING ; WANG DONGYANG ; WANG SHAOFEI ; WANG XISHUO ; REN XINYI ; MENG FANTONG ; LIU YUQI ; DOU AIMIN ; QI JINCHAO</creator><creatorcontrib>LIU WANHUI ; WAN JUN ; TANG WEI ; WANG FEI ; REN QIUHONG ; QI HAIFENG ; LI JING ; WANG DONGYANG ; WANG SHAOFEI ; WANG XISHUO ; REN XINYI ; MENG FANTONG ; LIU YUQI ; DOU AIMIN ; QI JINCHAO</creatorcontrib><description>The invention relates to the field of steel rolling, in particular to a trip steel coiling tension control method. The method comprises the steps that when the strip steel head enters a belt wrapper,the coiling tension value is controlled to 35 to 65 MPa; when the belt wrapper descends and delays for 4 to 5 seconds, the coiling tension value is controlled to be stepped to 50.05 to 92.95 MPa, then, the value is gradually reduced to 38.5 to 71.5 MPa; when the length of coiled strip steel reaches 1/5 of the total length of the strip steel, the coiling tension value is controlled to be graduallyreduced to 35 to 65 MPa; when the length of the coiled strip steel reaches 3/5 of the total length of the strip steel, the coiling tension value is controlled to be kept 35 to 65 MPa; when the lengthof the coiled strip steel reaches 4/5 of the total length of the strip steel, the coiling tension value is controlled to be gradually increased to 36.75 to 68.25 MPa until strip steel coiling is finished. According to the coili</description><language>chi ; eng</language><subject>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL ; MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; TRANSPORTING</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180817&amp;DB=EPODOC&amp;CC=CN&amp;NR=108405653A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180817&amp;DB=EPODOC&amp;CC=CN&amp;NR=108405653A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU WANHUI</creatorcontrib><creatorcontrib>WAN JUN</creatorcontrib><creatorcontrib>TANG WEI</creatorcontrib><creatorcontrib>WANG FEI</creatorcontrib><creatorcontrib>REN QIUHONG</creatorcontrib><creatorcontrib>QI HAIFENG</creatorcontrib><creatorcontrib>LI JING</creatorcontrib><creatorcontrib>WANG DONGYANG</creatorcontrib><creatorcontrib>WANG SHAOFEI</creatorcontrib><creatorcontrib>WANG XISHUO</creatorcontrib><creatorcontrib>REN XINYI</creatorcontrib><creatorcontrib>MENG FANTONG</creatorcontrib><creatorcontrib>LIU YUQI</creatorcontrib><creatorcontrib>DOU AIMIN</creatorcontrib><creatorcontrib>QI JINCHAO</creatorcontrib><title>Strip steel coiling tension control method and device</title><description>The invention relates to the field of steel rolling, in particular to a trip steel coiling tension control method. The method comprises the steps that when the strip steel head enters a belt wrapper,the coiling tension value is controlled to 35 to 65 MPa; when the belt wrapper descends and delays for 4 to 5 seconds, the coiling tension value is controlled to be stepped to 50.05 to 92.95 MPa, then, the value is gradually reduced to 38.5 to 71.5 MPa; when the length of coiled strip steel reaches 1/5 of the total length of the strip steel, the coiling tension value is controlled to be graduallyreduced to 35 to 65 MPa; when the length of the coiled strip steel reaches 3/5 of the total length of the strip steel, the coiling tension value is controlled to be kept 35 to 65 MPa; when the lengthof the coiled strip steel reaches 4/5 of the total length of the strip steel, the coiling tension value is controlled to be gradually increased to 36.75 to 68.25 MPa until strip steel coiling is finished. According to the coili</description><subject>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL</subject><subject>MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDANLinKLFAoLklNzVFIzs_MycxLVyhJzSvOzM8D8vNKivJzFHJTSzLyUxQS81IUUlLLMpNTeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGFiYGpmamxozExagBwrS01</recordid><startdate>20180817</startdate><enddate>20180817</enddate><creator>LIU WANHUI</creator><creator>WAN JUN</creator><creator>TANG WEI</creator><creator>WANG FEI</creator><creator>REN QIUHONG</creator><creator>QI HAIFENG</creator><creator>LI JING</creator><creator>WANG DONGYANG</creator><creator>WANG SHAOFEI</creator><creator>WANG XISHUO</creator><creator>REN XINYI</creator><creator>MENG FANTONG</creator><creator>LIU YUQI</creator><creator>DOU AIMIN</creator><creator>QI JINCHAO</creator><scope>EVB</scope></search><sort><creationdate>20180817</creationdate><title>Strip steel coiling tension control method and device</title><author>LIU WANHUI ; WAN JUN ; TANG WEI ; WANG FEI ; REN QIUHONG ; QI HAIFENG ; LI JING ; WANG DONGYANG ; WANG SHAOFEI ; WANG XISHUO ; REN XINYI ; MENG FANTONG ; LIU YUQI ; DOU AIMIN ; QI JINCHAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN108405653A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2018</creationdate><topic>AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL</topic><topic>MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU WANHUI</creatorcontrib><creatorcontrib>WAN JUN</creatorcontrib><creatorcontrib>TANG WEI</creatorcontrib><creatorcontrib>WANG FEI</creatorcontrib><creatorcontrib>REN QIUHONG</creatorcontrib><creatorcontrib>QI HAIFENG</creatorcontrib><creatorcontrib>LI JING</creatorcontrib><creatorcontrib>WANG DONGYANG</creatorcontrib><creatorcontrib>WANG SHAOFEI</creatorcontrib><creatorcontrib>WANG XISHUO</creatorcontrib><creatorcontrib>REN XINYI</creatorcontrib><creatorcontrib>MENG FANTONG</creatorcontrib><creatorcontrib>LIU YUQI</creatorcontrib><creatorcontrib>DOU AIMIN</creatorcontrib><creatorcontrib>QI JINCHAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU WANHUI</au><au>WAN JUN</au><au>TANG WEI</au><au>WANG FEI</au><au>REN QIUHONG</au><au>QI HAIFENG</au><au>LI JING</au><au>WANG DONGYANG</au><au>WANG SHAOFEI</au><au>WANG XISHUO</au><au>REN XINYI</au><au>MENG FANTONG</au><au>LIU YUQI</au><au>DOU AIMIN</au><au>QI JINCHAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Strip steel coiling tension control method and device</title><date>2018-08-17</date><risdate>2018</risdate><abstract>The invention relates to the field of steel rolling, in particular to a trip steel coiling tension control method. The method comprises the steps that when the strip steel head enters a belt wrapper,the coiling tension value is controlled to 35 to 65 MPa; when the belt wrapper descends and delays for 4 to 5 seconds, the coiling tension value is controlled to be stepped to 50.05 to 92.95 MPa, then, the value is gradually reduced to 38.5 to 71.5 MPa; when the length of coiled strip steel reaches 1/5 of the total length of the strip steel, the coiling tension value is controlled to be graduallyreduced to 35 to 65 MPa; when the length of the coiled strip steel reaches 3/5 of the total length of the strip steel, the coiling tension value is controlled to be kept 35 to 65 MPa; when the lengthof the coiled strip steel reaches 4/5 of the total length of the strip steel, the coiling tension value is controlled to be gradually increased to 36.75 to 68.25 MPa until strip steel coiling is finished. According to the coili</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN108405653A
source esp@cenet
subjects AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKINGWITHOUT ESSENTIALLY REMOVING MATERIAL
MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES OR PROFILES,OTHERWISE THAN BY ROLLING
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
PUNCHING METAL
TRANSPORTING
title Strip steel coiling tension control method and device
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T17%3A23%3A56IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20WANHUI&rft.date=2018-08-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN108405653A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true