Preparation method of full spin-coating type flexible hybrid piezoelectric generator

The invention relates to the technical field of nanometer generator preparation, in particular to a preparation method of a full spin-coating type flexible hybrid piezoelectric generator. The preparation method comprises the steps that firstly, surface treatment is conducted on nanometer zinc oxide...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HAN JING, LI YINGCHUN, WANG WENSHENG, ZHAO CHUNMAO, LI JIE, WANG WENHAO, XIA KAI, LI DONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HAN JING
LI YINGCHUN
WANG WENSHENG
ZHAO CHUNMAO
LI JIE
WANG WENHAO
XIA KAI
LI DONG
description The invention relates to the technical field of nanometer generator preparation, in particular to a preparation method of a full spin-coating type flexible hybrid piezoelectric generator. The preparation method comprises the steps that firstly, surface treatment is conducted on nanometer zinc oxide with a dispersing agent and a surface modifying agent so as to improve the compatibility between a base material and nanometer filler, improve the nucleation capacity of the nanometer zinc oxide and obtain a high-crystallinity composite film; secondly, a full spin-coating technology is provided, wherein in the first spin-coating process, the film suffers from shear stress, so that polyvinylidene fluoride-trifluoroethylene molecular chains are induced to be directionally aligned, and the formation of a beta phase is facilitated; in the second spin-coating process, spin-coated conductive macromolecular poly(3,4-ethylenedioxythiophene): polystyrene sulfonate serves as a top electrode, the problem about interlayer matc
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN107732004A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN107732004A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN107732004A3</originalsourceid><addsrcrecordid>eNqNjLEKwjAYBrM4iPoOvw9QiFboLEVxEofuJU2_tIGYPyQRrE9vBh_A6YY7bi26R0RQUWXLnp7IM4_EhszLOUrB-kpzcX6ivASQcXjbwYHmZYh2pGDxYTjoHK2mCR7lxHErVka5hN2PG7G_Xrr2ViFwjxSULmXu2_tBNk19lPJ0rv9pvuZSOW0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of full spin-coating type flexible hybrid piezoelectric generator</title><source>esp@cenet</source><creator>HAN JING ; LI YINGCHUN ; WANG WENSHENG ; ZHAO CHUNMAO ; LI JIE ; WANG WENHAO ; XIA KAI ; LI DONG</creator><creatorcontrib>HAN JING ; LI YINGCHUN ; WANG WENSHENG ; ZHAO CHUNMAO ; LI JIE ; WANG WENHAO ; XIA KAI ; LI DONG</creatorcontrib><description>The invention relates to the technical field of nanometer generator preparation, in particular to a preparation method of a full spin-coating type flexible hybrid piezoelectric generator. The preparation method comprises the steps that firstly, surface treatment is conducted on nanometer zinc oxide with a dispersing agent and a surface modifying agent so as to improve the compatibility between a base material and nanometer filler, improve the nucleation capacity of the nanometer zinc oxide and obtain a high-crystallinity composite film; secondly, a full spin-coating technology is provided, wherein in the first spin-coating process, the film suffers from shear stress, so that polyvinylidene fluoride-trifluoroethylene molecular chains are induced to be directionally aligned, and the formation of a beta phase is facilitated; in the second spin-coating process, spin-coated conductive macromolecular poly(3,4-ethylenedioxythiophene): polystyrene sulfonate serves as a top electrode, the problem about interlayer matc</description><language>chi ; eng</language><subject>ELECTRICITY</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180223&amp;DB=EPODOC&amp;CC=CN&amp;NR=107732004A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180223&amp;DB=EPODOC&amp;CC=CN&amp;NR=107732004A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HAN JING</creatorcontrib><creatorcontrib>LI YINGCHUN</creatorcontrib><creatorcontrib>WANG WENSHENG</creatorcontrib><creatorcontrib>ZHAO CHUNMAO</creatorcontrib><creatorcontrib>LI JIE</creatorcontrib><creatorcontrib>WANG WENHAO</creatorcontrib><creatorcontrib>XIA KAI</creatorcontrib><creatorcontrib>LI DONG</creatorcontrib><title>Preparation method of full spin-coating type flexible hybrid piezoelectric generator</title><description>The invention relates to the technical field of nanometer generator preparation, in particular to a preparation method of a full spin-coating type flexible hybrid piezoelectric generator. The preparation method comprises the steps that firstly, surface treatment is conducted on nanometer zinc oxide with a dispersing agent and a surface modifying agent so as to improve the compatibility between a base material and nanometer filler, improve the nucleation capacity of the nanometer zinc oxide and obtain a high-crystallinity composite film; secondly, a full spin-coating technology is provided, wherein in the first spin-coating process, the film suffers from shear stress, so that polyvinylidene fluoride-trifluoroethylene molecular chains are induced to be directionally aligned, and the formation of a beta phase is facilitated; in the second spin-coating process, spin-coated conductive macromolecular poly(3,4-ethylenedioxythiophene): polystyrene sulfonate serves as a top electrode, the problem about interlayer matc</description><subject>ELECTRICITY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLEKwjAYBrM4iPoOvw9QiFboLEVxEofuJU2_tIGYPyQRrE9vBh_A6YY7bi26R0RQUWXLnp7IM4_EhszLOUrB-kpzcX6ivASQcXjbwYHmZYh2pGDxYTjoHK2mCR7lxHErVka5hN2PG7G_Xrr2ViFwjxSULmXu2_tBNk19lPJ0rv9pvuZSOW0</recordid><startdate>20180223</startdate><enddate>20180223</enddate><creator>HAN JING</creator><creator>LI YINGCHUN</creator><creator>WANG WENSHENG</creator><creator>ZHAO CHUNMAO</creator><creator>LI JIE</creator><creator>WANG WENHAO</creator><creator>XIA KAI</creator><creator>LI DONG</creator><scope>EVB</scope></search><sort><creationdate>20180223</creationdate><title>Preparation method of full spin-coating type flexible hybrid piezoelectric generator</title><author>HAN JING ; LI YINGCHUN ; WANG WENSHENG ; ZHAO CHUNMAO ; LI JIE ; WANG WENHAO ; XIA KAI ; LI DONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN107732004A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2018</creationdate><topic>ELECTRICITY</topic><toplevel>online_resources</toplevel><creatorcontrib>HAN JING</creatorcontrib><creatorcontrib>LI YINGCHUN</creatorcontrib><creatorcontrib>WANG WENSHENG</creatorcontrib><creatorcontrib>ZHAO CHUNMAO</creatorcontrib><creatorcontrib>LI JIE</creatorcontrib><creatorcontrib>WANG WENHAO</creatorcontrib><creatorcontrib>XIA KAI</creatorcontrib><creatorcontrib>LI DONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HAN JING</au><au>LI YINGCHUN</au><au>WANG WENSHENG</au><au>ZHAO CHUNMAO</au><au>LI JIE</au><au>WANG WENHAO</au><au>XIA KAI</au><au>LI DONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of full spin-coating type flexible hybrid piezoelectric generator</title><date>2018-02-23</date><risdate>2018</risdate><abstract>The invention relates to the technical field of nanometer generator preparation, in particular to a preparation method of a full spin-coating type flexible hybrid piezoelectric generator. The preparation method comprises the steps that firstly, surface treatment is conducted on nanometer zinc oxide with a dispersing agent and a surface modifying agent so as to improve the compatibility between a base material and nanometer filler, improve the nucleation capacity of the nanometer zinc oxide and obtain a high-crystallinity composite film; secondly, a full spin-coating technology is provided, wherein in the first spin-coating process, the film suffers from shear stress, so that polyvinylidene fluoride-trifluoroethylene molecular chains are induced to be directionally aligned, and the formation of a beta phase is facilitated; in the second spin-coating process, spin-coated conductive macromolecular poly(3,4-ethylenedioxythiophene): polystyrene sulfonate serves as a top electrode, the problem about interlayer matc</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN107732004A
source esp@cenet
subjects ELECTRICITY
title Preparation method of full spin-coating type flexible hybrid piezoelectric generator
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-25T15%3A33%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HAN%20JING&rft.date=2018-02-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN107732004A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true