Rotating preheating friction micro-welding method

The invention provides a rotating preheating friction micro-welding method and relates to a welding method. The objective of the invention is to solve the problems that when the technologies of soft soldering, hot pressure welding and the like are adopted for connection in the existing micro-connect...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU XIN, WANG PENG, SONG LAIRUI, ZHAO ZHILI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU XIN
WANG PENG
SONG LAIRUI
ZHAO ZHILI
description The invention provides a rotating preheating friction micro-welding method and relates to a welding method. The objective of the invention is to solve the problems that when the technologies of soft soldering, hot pressure welding and the like are adopted for connection in the existing micro-connecting field, connecting temperature is higher than a solder melting point and causes large influence on the thermal impact of a micro-interconnection structure. The method comprises the following steps: firstly, adopting a small-diameter capillary to clamp a drill bit and form a locating hole in a soldier at preset depth; then, adopting the small-diameter capillary to clamp a to-be-welded component, enabling the capillary to drive the to-be-welded component to go into the locating hole at a rotating speed V1 and an axial feeding speed V0, stopping axial feeding when the component reaches depth L1, raising the rotating speed and keeping the rotating speed for S seconds; then, lowering the rotating speed to the origina
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN107498127A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN107498127A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN107498127A3</originalsourceid><addsrcrecordid>eNrjZDAMyi9JLMnMS1coKErNSIUw04oyk0sy8_MUcjOTi_J1y1NzUkDCuaklGfkpPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0MDcxNLC0Mjc0ZgYNQDIgSwl</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Rotating preheating friction micro-welding method</title><source>esp@cenet</source><creator>LIU XIN ; WANG PENG ; SONG LAIRUI ; ZHAO ZHILI</creator><creatorcontrib>LIU XIN ; WANG PENG ; SONG LAIRUI ; ZHAO ZHILI</creatorcontrib><description>The invention provides a rotating preheating friction micro-welding method and relates to a welding method. The objective of the invention is to solve the problems that when the technologies of soft soldering, hot pressure welding and the like are adopted for connection in the existing micro-connecting field, connecting temperature is higher than a solder melting point and causes large influence on the thermal impact of a micro-interconnection structure. The method comprises the following steps: firstly, adopting a small-diameter capillary to clamp a drill bit and form a locating hole in a soldier at preset depth; then, adopting the small-diameter capillary to clamp a to-be-welded component, enabling the capillary to drive the to-be-welded component to go into the locating hole at a rotating speed V1 and an axial feeding speed V0, stopping axial feeding when the component reaches depth L1, raising the rotating speed and keeping the rotating speed for S seconds; then, lowering the rotating speed to the origina</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20171222&amp;DB=EPODOC&amp;CC=CN&amp;NR=107498127A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20171222&amp;DB=EPODOC&amp;CC=CN&amp;NR=107498127A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU XIN</creatorcontrib><creatorcontrib>WANG PENG</creatorcontrib><creatorcontrib>SONG LAIRUI</creatorcontrib><creatorcontrib>ZHAO ZHILI</creatorcontrib><title>Rotating preheating friction micro-welding method</title><description>The invention provides a rotating preheating friction micro-welding method and relates to a welding method. The objective of the invention is to solve the problems that when the technologies of soft soldering, hot pressure welding and the like are adopted for connection in the existing micro-connecting field, connecting temperature is higher than a solder melting point and causes large influence on the thermal impact of a micro-interconnection structure. The method comprises the following steps: firstly, adopting a small-diameter capillary to clamp a drill bit and form a locating hole in a soldier at preset depth; then, adopting the small-diameter capillary to clamp a to-be-welded component, enabling the capillary to drive the to-be-welded component to go into the locating hole at a rotating speed V1 and an axial feeding speed V0, stopping axial feeding when the component reaches depth L1, raising the rotating speed and keeping the rotating speed for S seconds; then, lowering the rotating speed to the origina</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAMyi9JLMnMS1coKErNSIUw04oyk0sy8_MUcjOTi_J1y1NzUkDCuaklGfkpPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0MDcxNLC0Mjc0ZgYNQDIgSwl</recordid><startdate>20171222</startdate><enddate>20171222</enddate><creator>LIU XIN</creator><creator>WANG PENG</creator><creator>SONG LAIRUI</creator><creator>ZHAO ZHILI</creator><scope>EVB</scope></search><sort><creationdate>20171222</creationdate><title>Rotating preheating friction micro-welding method</title><author>LIU XIN ; WANG PENG ; SONG LAIRUI ; ZHAO ZHILI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN107498127A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2017</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU XIN</creatorcontrib><creatorcontrib>WANG PENG</creatorcontrib><creatorcontrib>SONG LAIRUI</creatorcontrib><creatorcontrib>ZHAO ZHILI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU XIN</au><au>WANG PENG</au><au>SONG LAIRUI</au><au>ZHAO ZHILI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Rotating preheating friction micro-welding method</title><date>2017-12-22</date><risdate>2017</risdate><abstract>The invention provides a rotating preheating friction micro-welding method and relates to a welding method. The objective of the invention is to solve the problems that when the technologies of soft soldering, hot pressure welding and the like are adopted for connection in the existing micro-connecting field, connecting temperature is higher than a solder melting point and causes large influence on the thermal impact of a micro-interconnection structure. The method comprises the following steps: firstly, adopting a small-diameter capillary to clamp a drill bit and form a locating hole in a soldier at preset depth; then, adopting the small-diameter capillary to clamp a to-be-welded component, enabling the capillary to drive the to-be-welded component to go into the locating hole at a rotating speed V1 and an axial feeding speed V0, stopping axial feeding when the component reaches depth L1, raising the rotating speed and keeping the rotating speed for S seconds; then, lowering the rotating speed to the origina</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN107498127A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Rotating preheating friction micro-welding method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T07%3A18%3A29IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20XIN&rft.date=2017-12-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN107498127A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true