Temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method

The invention discloses a temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method. A phase of a composite ceramic comprises Li3Mg2SbO6 phase in a rock salt structure, Ba3 (VO4)2 phase in an orthorhombic structure and a BaSb2O6 in a tril...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GONG YI, REN ZHAOYU, XING HUIYU, LIU NA, FU LONGXI, LIANG BAICHENG, YAO GUOGUANG, PEI CUIJIN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GONG YI
REN ZHAOYU
XING HUIYU
LIU NA
FU LONGXI
LIANG BAICHENG
YAO GUOGUANG
PEI CUIJIN
description The invention discloses a temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method. A phase of a composite ceramic comprises Li3Mg2SbO6 phase in a rock salt structure, Ba3 (VO4)2 phase in an orthorhombic structure and a BaSb2O6 in a trilateral structure, wherein Li3Mg2SbO6 content is 54wt%-78wt%, Ba3 (VO4)2 content is 13wt%-38wt%, and the rest is BaSb2O6. Through adding Ba3 (VO4)2 presintering powder in the Li3Mg2SbO6 main powder body, the composite ceramic inhibits the rupturing of Li3Mg2SbO6, improves its temperature stability, and acquires a new material with good microwave dielectric property; the dielectric constant is 9.0-12.1, the quality factor is 18400-45100 GHz, and the resonate frequency temperature coefficient is -9.0 to +7.0 ppm/DEG C. The preparation method is rich in raw materials, simple in technique, and good for industrial production. 本发明公开了种温度稳定型锑酸镁锂基微波介质复合陶瓷及其制备方法,该复合陶瓷的物相包括岩盐结构的LiMgSbO相、正交结构的Ba(VO)相和三方结构的BaSbO相,其中LiMgSbO的含量为54
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN107235711A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN107235711A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN107235711A3</originalsourceid><addsrcrecordid>eNqNjU0KwjAUhLtxIeodngcQjEW6lqK4ctV9eU1HG2h-SF4t3t4UPICrGYZvZtbF3MAGRJYpgpJwN4LkE0CWXw7JTJbYibHeGQGNRoYl6jhlAv3irdHRz_wGaW-DTwun82LOc7UnI4lCROB8YrzLNRl8vy1WTx4Tdj_dFPvbtanvBwTfIgXWcJC2fqhjdSrPlVKX8h_mCyeMRxI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method</title><source>esp@cenet</source><creator>GONG YI ; REN ZHAOYU ; XING HUIYU ; LIU NA ; FU LONGXI ; LIANG BAICHENG ; YAO GUOGUANG ; PEI CUIJIN</creator><creatorcontrib>GONG YI ; REN ZHAOYU ; XING HUIYU ; LIU NA ; FU LONGXI ; LIANG BAICHENG ; YAO GUOGUANG ; PEI CUIJIN</creatorcontrib><description>The invention discloses a temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method. A phase of a composite ceramic comprises Li3Mg2SbO6 phase in a rock salt structure, Ba3 (VO4)2 phase in an orthorhombic structure and a BaSb2O6 in a trilateral structure, wherein Li3Mg2SbO6 content is 54wt%-78wt%, Ba3 (VO4)2 content is 13wt%-38wt%, and the rest is BaSb2O6. Through adding Ba3 (VO4)2 presintering powder in the Li3Mg2SbO6 main powder body, the composite ceramic inhibits the rupturing of Li3Mg2SbO6, improves its temperature stability, and acquires a new material with good microwave dielectric property; the dielectric constant is 9.0-12.1, the quality factor is 18400-45100 GHz, and the resonate frequency temperature coefficient is -9.0 to +7.0 ppm/DEG C. The preparation method is rich in raw materials, simple in technique, and good for industrial production. 本发明公开了种温度稳定型锑酸镁锂基微波介质复合陶瓷及其制备方法,该复合陶瓷的物相包括岩盐结构的LiMgSbO相、正交结构的Ba(VO)相和三方结构的BaSbO相,其中LiMgSbO的含量为54</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20171010&amp;DB=EPODOC&amp;CC=CN&amp;NR=107235711A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20171010&amp;DB=EPODOC&amp;CC=CN&amp;NR=107235711A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GONG YI</creatorcontrib><creatorcontrib>REN ZHAOYU</creatorcontrib><creatorcontrib>XING HUIYU</creatorcontrib><creatorcontrib>LIU NA</creatorcontrib><creatorcontrib>FU LONGXI</creatorcontrib><creatorcontrib>LIANG BAICHENG</creatorcontrib><creatorcontrib>YAO GUOGUANG</creatorcontrib><creatorcontrib>PEI CUIJIN</creatorcontrib><title>Temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method</title><description>The invention discloses a temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method. A phase of a composite ceramic comprises Li3Mg2SbO6 phase in a rock salt structure, Ba3 (VO4)2 phase in an orthorhombic structure and a BaSb2O6 in a trilateral structure, wherein Li3Mg2SbO6 content is 54wt%-78wt%, Ba3 (VO4)2 content is 13wt%-38wt%, and the rest is BaSb2O6. Through adding Ba3 (VO4)2 presintering powder in the Li3Mg2SbO6 main powder body, the composite ceramic inhibits the rupturing of Li3Mg2SbO6, improves its temperature stability, and acquires a new material with good microwave dielectric property; the dielectric constant is 9.0-12.1, the quality factor is 18400-45100 GHz, and the resonate frequency temperature coefficient is -9.0 to +7.0 ppm/DEG C. The preparation method is rich in raw materials, simple in technique, and good for industrial production. 本发明公开了种温度稳定型锑酸镁锂基微波介质复合陶瓷及其制备方法,该复合陶瓷的物相包括岩盐结构的LiMgSbO相、正交结构的Ba(VO)相和三方结构的BaSbO相,其中LiMgSbO的含量为54</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjU0KwjAUhLtxIeodngcQjEW6lqK4ctV9eU1HG2h-SF4t3t4UPICrGYZvZtbF3MAGRJYpgpJwN4LkE0CWXw7JTJbYibHeGQGNRoYl6jhlAv3irdHRz_wGaW-DTwun82LOc7UnI4lCROB8YrzLNRl8vy1WTx4Tdj_dFPvbtanvBwTfIgXWcJC2fqhjdSrPlVKX8h_mCyeMRxI</recordid><startdate>20171010</startdate><enddate>20171010</enddate><creator>GONG YI</creator><creator>REN ZHAOYU</creator><creator>XING HUIYU</creator><creator>LIU NA</creator><creator>FU LONGXI</creator><creator>LIANG BAICHENG</creator><creator>YAO GUOGUANG</creator><creator>PEI CUIJIN</creator><scope>EVB</scope></search><sort><creationdate>20171010</creationdate><title>Temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method</title><author>GONG YI ; REN ZHAOYU ; XING HUIYU ; LIU NA ; FU LONGXI ; LIANG BAICHENG ; YAO GUOGUANG ; PEI CUIJIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN107235711A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2017</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>GONG YI</creatorcontrib><creatorcontrib>REN ZHAOYU</creatorcontrib><creatorcontrib>XING HUIYU</creatorcontrib><creatorcontrib>LIU NA</creatorcontrib><creatorcontrib>FU LONGXI</creatorcontrib><creatorcontrib>LIANG BAICHENG</creatorcontrib><creatorcontrib>YAO GUOGUANG</creatorcontrib><creatorcontrib>PEI CUIJIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GONG YI</au><au>REN ZHAOYU</au><au>XING HUIYU</au><au>LIU NA</au><au>FU LONGXI</au><au>LIANG BAICHENG</au><au>YAO GUOGUANG</au><au>PEI CUIJIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method</title><date>2017-10-10</date><risdate>2017</risdate><abstract>The invention discloses a temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method. A phase of a composite ceramic comprises Li3Mg2SbO6 phase in a rock salt structure, Ba3 (VO4)2 phase in an orthorhombic structure and a BaSb2O6 in a trilateral structure, wherein Li3Mg2SbO6 content is 54wt%-78wt%, Ba3 (VO4)2 content is 13wt%-38wt%, and the rest is BaSb2O6. Through adding Ba3 (VO4)2 presintering powder in the Li3Mg2SbO6 main powder body, the composite ceramic inhibits the rupturing of Li3Mg2SbO6, improves its temperature stability, and acquires a new material with good microwave dielectric property; the dielectric constant is 9.0-12.1, the quality factor is 18400-45100 GHz, and the resonate frequency temperature coefficient is -9.0 to +7.0 ppm/DEG C. The preparation method is rich in raw materials, simple in technique, and good for industrial production. 本发明公开了种温度稳定型锑酸镁锂基微波介质复合陶瓷及其制备方法,该复合陶瓷的物相包括岩盐结构的LiMgSbO相、正交结构的Ba(VO)相和三方结构的BaSbO相,其中LiMgSbO的含量为54</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN107235711A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Temperature stable type magnesium antimonite lithium base medium microwave composite ceramic and its preparation method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-20T02%3A50%3A34IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GONG%20YI&rft.date=2017-10-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN107235711A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true