Asphalt compositions for roofing applications, methods for making the same, and filled asphalt material comprising the same

Asphalt compositions for roofing applications are provided, as well as filled asphalt material comprising the asphalt compositions and methods for making asphalt compositions and filled asphalt material. More particularly, the asphalt compositions 5 comprise non-oxidized base asphalt; and a low mole...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEM PAUL CHI, HACKER SCOTT MARTIN, RUAN YONGHONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LEM PAUL CHI
HACKER SCOTT MARTIN
RUAN YONGHONG
description Asphalt compositions for roofing applications are provided, as well as filled asphalt material comprising the asphalt compositions and methods for making asphalt compositions and filled asphalt material. More particularly, the asphalt compositions 5 comprise non-oxidized base asphalt; and a low molecular weight polyolefin present in an amount of from about 0.5 to about 15 wt % based on the total weight of the asphalt composition. The asphalt composition has a softening point from about 87.8 to about 160 DEG C (about 190 to about 320 DEG F), a penetration of greater than 12 deci-millimeters DEG @ 25 DEG C, as well as improved stain resistance and heat resistance. 提供用于铺顶应用的沥青组合物,以及包含所述沥青组合物的填充型沥青材料和用于制备沥青组合物和填充型沥青材料的方法。更具体地,所述沥青组合物包含非氧化基料沥青;和基于沥青组合物总重量以约0.5至约15 wt %的量存在的低分子量聚烯烃。所述沥青组合物具有约87.8至约160℃ (约190至约320 °F)的软化点、大于12丝米的针入度@ 25℃、和改善的耐污斑性和耐热性。
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN106574123A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN106574123A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN106574123A3</originalsourceid><addsrcrecordid>eNqNjLsOwjAMRbswIOAfzF4kSnnMVQViYmKvrNYhFkkcxdn4eUTpwMh0h3vOmRevRqNFl6EXH0U5swQFIwmSiOHwAIzRcY_jUYKnbGX4Eh6fHyBbAkVPJWAYwLBzNABOWY-ZEqMb-4n1V1gWM4NOaTXtolhfzvf2uqEoHWnEngLlrr1V2-PhtK92dVP_w7wB1MJHhA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Asphalt compositions for roofing applications, methods for making the same, and filled asphalt material comprising the same</title><source>esp@cenet</source><creator>LEM PAUL CHI ; HACKER SCOTT MARTIN ; RUAN YONGHONG</creator><creatorcontrib>LEM PAUL CHI ; HACKER SCOTT MARTIN ; RUAN YONGHONG</creatorcontrib><description>Asphalt compositions for roofing applications are provided, as well as filled asphalt material comprising the asphalt compositions and methods for making asphalt compositions and filled asphalt material. More particularly, the asphalt compositions 5 comprise non-oxidized base asphalt; and a low molecular weight polyolefin present in an amount of from about 0.5 to about 15 wt % based on the total weight of the asphalt composition. The asphalt composition has a softening point from about 87.8 to about 160 DEG C (about 190 to about 320 DEG F), a penetration of greater than 12 deci-millimeters DEG @ 25 DEG C, as well as improved stain resistance and heat resistance. 提供用于铺顶应用的沥青组合物,以及包含所述沥青组合物的填充型沥青材料和用于制备沥青组合物和填充型沥青材料的方法。更具体地,所述沥青组合物包含非氧化基料沥青;和基于沥青组合物总重量以约0.5至约15 wt %的量存在的低分子量聚烯烃。所述沥青组合物具有约87.8至约160℃ (约190至约320 °F)的软化点、大于12丝米的针入度@ 25℃、和改善的耐污斑性和耐热性。</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170419&amp;DB=EPODOC&amp;CC=CN&amp;NR=106574123A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170419&amp;DB=EPODOC&amp;CC=CN&amp;NR=106574123A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LEM PAUL CHI</creatorcontrib><creatorcontrib>HACKER SCOTT MARTIN</creatorcontrib><creatorcontrib>RUAN YONGHONG</creatorcontrib><title>Asphalt compositions for roofing applications, methods for making the same, and filled asphalt material comprising the same</title><description>Asphalt compositions for roofing applications are provided, as well as filled asphalt material comprising the asphalt compositions and methods for making asphalt compositions and filled asphalt material. More particularly, the asphalt compositions 5 comprise non-oxidized base asphalt; and a low molecular weight polyolefin present in an amount of from about 0.5 to about 15 wt % based on the total weight of the asphalt composition. The asphalt composition has a softening point from about 87.8 to about 160 DEG C (about 190 to about 320 DEG F), a penetration of greater than 12 deci-millimeters DEG @ 25 DEG C, as well as improved stain resistance and heat resistance. 提供用于铺顶应用的沥青组合物,以及包含所述沥青组合物的填充型沥青材料和用于制备沥青组合物和填充型沥青材料的方法。更具体地,所述沥青组合物包含非氧化基料沥青;和基于沥青组合物总重量以约0.5至约15 wt %的量存在的低分子量聚烯烃。所述沥青组合物具有约87.8至约160℃ (约190至约320 °F)的软化点、大于12丝米的针入度@ 25℃、和改善的耐污斑性和耐热性。</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLsOwjAMRbswIOAfzF4kSnnMVQViYmKvrNYhFkkcxdn4eUTpwMh0h3vOmRevRqNFl6EXH0U5swQFIwmSiOHwAIzRcY_jUYKnbGX4Eh6fHyBbAkVPJWAYwLBzNABOWY-ZEqMb-4n1V1gWM4NOaTXtolhfzvf2uqEoHWnEngLlrr1V2-PhtK92dVP_w7wB1MJHhA</recordid><startdate>20170419</startdate><enddate>20170419</enddate><creator>LEM PAUL CHI</creator><creator>HACKER SCOTT MARTIN</creator><creator>RUAN YONGHONG</creator><scope>EVB</scope></search><sort><creationdate>20170419</creationdate><title>Asphalt compositions for roofing applications, methods for making the same, and filled asphalt material comprising the same</title><author>LEM PAUL CHI ; HACKER SCOTT MARTIN ; RUAN YONGHONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN106574123A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2017</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>LEM PAUL CHI</creatorcontrib><creatorcontrib>HACKER SCOTT MARTIN</creatorcontrib><creatorcontrib>RUAN YONGHONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LEM PAUL CHI</au><au>HACKER SCOTT MARTIN</au><au>RUAN YONGHONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Asphalt compositions for roofing applications, methods for making the same, and filled asphalt material comprising the same</title><date>2017-04-19</date><risdate>2017</risdate><abstract>Asphalt compositions for roofing applications are provided, as well as filled asphalt material comprising the asphalt compositions and methods for making asphalt compositions and filled asphalt material. More particularly, the asphalt compositions 5 comprise non-oxidized base asphalt; and a low molecular weight polyolefin present in an amount of from about 0.5 to about 15 wt % based on the total weight of the asphalt composition. The asphalt composition has a softening point from about 87.8 to about 160 DEG C (about 190 to about 320 DEG F), a penetration of greater than 12 deci-millimeters DEG @ 25 DEG C, as well as improved stain resistance and heat resistance. 提供用于铺顶应用的沥青组合物,以及包含所述沥青组合物的填充型沥青材料和用于制备沥青组合物和填充型沥青材料的方法。更具体地,所述沥青组合物包含非氧化基料沥青;和基于沥青组合物总重量以约0.5至约15 wt %的量存在的低分子量聚烯烃。所述沥青组合物具有约87.8至约160℃ (约190至约320 °F)的软化点、大于12丝米的针入度@ 25℃、和改善的耐污斑性和耐热性。</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN106574123A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Asphalt compositions for roofing applications, methods for making the same, and filled asphalt material comprising the same
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-12T11%3A41%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LEM%20PAUL%20CHI&rft.date=2017-04-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN106574123A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true