Injection molding method

The invention discloses an injection molding method which comprises the steps of compounding materials and putting the materials in an injection molding machine for injection molding, wherein during material compounding, a dispersing agent consisting of 5-10g Ircoplus 113 hyperdispersant and 2-8g co...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: ZHOU QINXIA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHOU QINXIA
description The invention discloses an injection molding method which comprises the steps of compounding materials and putting the materials in an injection molding machine for injection molding, wherein during material compounding, a dispersing agent consisting of 5-10g Ircoplus 113 hyperdispersant and 2-8g color masterbatch dispersant is added to per kilogram of raw materials; then 2-2.2g toner and 100-200g expanded perlite are added to per kilogram of raw materials; and after the above materials are mixed for 10-20min and are uniform, the injection molding is carried out. Compared with the prior art, the original white oil is replaced by the Ircoplus 113 hyperdispersant and the color masterbatch dispersant, so that the raw materials, color masterbatch and a filling are dispersed more easily during mixing; the chemical stability of the dispersing agent is good, so that the oxidation resistance is good during the injection molding, a product can not produce black spots; due to the own characteristics of the dispersing a
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105538586A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105538586A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105538586A3</originalsourceid><addsrcrecordid>eNrjZJDwzMtKTS7JzM9TyM3PScnMS1fITS3JyE_hYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBqamxhamFmaOxsSoAQD6dyJf</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Injection molding method</title><source>esp@cenet</source><creator>ZHOU QINXIA</creator><creatorcontrib>ZHOU QINXIA</creatorcontrib><description>The invention discloses an injection molding method which comprises the steps of compounding materials and putting the materials in an injection molding machine for injection molding, wherein during material compounding, a dispersing agent consisting of 5-10g Ircoplus 113 hyperdispersant and 2-8g color masterbatch dispersant is added to per kilogram of raw materials; then 2-2.2g toner and 100-200g expanded perlite are added to per kilogram of raw materials; and after the above materials are mixed for 10-20min and are uniform, the injection molding is carried out. Compared with the prior art, the original white oil is replaced by the Ircoplus 113 hyperdispersant and the color masterbatch dispersant, so that the raw materials, color masterbatch and a filling are dispersed more easily during mixing; the chemical stability of the dispersing agent is good, so that the oxidation resistance is good during the injection molding, a product can not produce black spots; due to the own characteristics of the dispersing a</description><language>chi ; eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160504&amp;DB=EPODOC&amp;CC=CN&amp;NR=105538586A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,782,887,25571,76555</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160504&amp;DB=EPODOC&amp;CC=CN&amp;NR=105538586A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHOU QINXIA</creatorcontrib><title>Injection molding method</title><description>The invention discloses an injection molding method which comprises the steps of compounding materials and putting the materials in an injection molding machine for injection molding, wherein during material compounding, a dispersing agent consisting of 5-10g Ircoplus 113 hyperdispersant and 2-8g color masterbatch dispersant is added to per kilogram of raw materials; then 2-2.2g toner and 100-200g expanded perlite are added to per kilogram of raw materials; and after the above materials are mixed for 10-20min and are uniform, the injection molding is carried out. Compared with the prior art, the original white oil is replaced by the Ircoplus 113 hyperdispersant and the color masterbatch dispersant, so that the raw materials, color masterbatch and a filling are dispersed more easily during mixing; the chemical stability of the dispersing agent is good, so that the oxidation resistance is good during the injection molding, a product can not produce black spots; due to the own characteristics of the dispersing a</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJDwzMtKTS7JzM9TyM3PScnMS1fITS3JyE_hYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBqamxhamFmaOxsSoAQD6dyJf</recordid><startdate>20160504</startdate><enddate>20160504</enddate><creator>ZHOU QINXIA</creator><scope>EVB</scope></search><sort><creationdate>20160504</creationdate><title>Injection molding method</title><author>ZHOU QINXIA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105538586A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2016</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHOU QINXIA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHOU QINXIA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Injection molding method</title><date>2016-05-04</date><risdate>2016</risdate><abstract>The invention discloses an injection molding method which comprises the steps of compounding materials and putting the materials in an injection molding machine for injection molding, wherein during material compounding, a dispersing agent consisting of 5-10g Ircoplus 113 hyperdispersant and 2-8g color masterbatch dispersant is added to per kilogram of raw materials; then 2-2.2g toner and 100-200g expanded perlite are added to per kilogram of raw materials; and after the above materials are mixed for 10-20min and are uniform, the injection molding is carried out. Compared with the prior art, the original white oil is replaced by the Ircoplus 113 hyperdispersant and the color masterbatch dispersant, so that the raw materials, color masterbatch and a filling are dispersed more easily during mixing; the chemical stability of the dispersing agent is good, so that the oxidation resistance is good during the injection molding, a product can not produce black spots; due to the own characteristics of the dispersing a</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN105538586A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title Injection molding method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-04T02%3A46%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHOU%20QINXIA&rft.date=2016-05-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105538586A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true