Environment-friendly multifunctional brick and preparation method thereof

The invention discloses an environment-friendly multifunctional brick and a preparation method thereof. The environment-friendly multifunctional brick is prepared from the following components in parts by mass: 17 to 20 parts of cement, 5 to 10 parts of emulsion, 0.5 to 2 parts of thin iron wire and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG JIAJUN, TAN XINGUI, LI XUECHENG, ZHAN ZHEHONG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention discloses an environment-friendly multifunctional brick and a preparation method thereof. The environment-friendly multifunctional brick is prepared from the following components in parts by mass: 17 to 20 parts of cement, 5 to 10 parts of emulsion, 0.5 to 2 parts of thin iron wire and/or scrap iron, 0.5 to 2 parts of fly ash, 0.5 to 2 parts of reclaim powder, 18 to 23 parts of fine aggregate, 50 to 60 parts of coarse aggregate and 1 to 5 parts of water. The preparation method comprises the following steps of (1) mixing the raw materials to obtain a mixture; (2) preparing a mold brick; (3) curing the mold brick to obtain the environment-friendly multifunctional brick. The environment-friendly multifunctional brick provided by the invention facilitates solving the problems, such as urban environment pollution, natural resource damage and resource waste, is high in strength, is not easy to damage and crack, can be applied to various urban bricks, meets the requirements of low carbon and environment friendliness, and is simple and convenient in preparation method and low in cost.