Method for repairing chilling ring of gasifier

The invention relates to a technique of repairing a chilling ring of a waste coal water slurry gasifier. The method for repairing the chilling ring of the gasifier comprises the steps that an original outer ring tube is cut down from the inner ring of a cavity base; lathe turning is carried out on a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CUI LIMING, LI YUYING, HOU SHUBO, HUO CHENGBIN, GAO BO, WANG JINHUI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CUI LIMING
LI YUYING
HOU SHUBO
HUO CHENGBIN
GAO BO
WANG JINHUI
description The invention relates to a technique of repairing a chilling ring of a waste coal water slurry gasifier. The method for repairing the chilling ring of the gasifier comprises the steps that an original outer ring tube is cut down from the inner ring of a cavity base; lathe turning is carried out on a water outlet of a water distribution hole on the inner ring of the cavity base, impurities on the lathe turning surface are removed by abrasive blasting, a thickness removed by the lathe turning is made up by spray welding, and a new water distribution hole is drilled in the inner ring of the cavity base; impurities on washed parts of the outer surface of a water distribution inner ring are removed by the abrasive blasting, and an original size of the water distribution inner ring is recovered through processing and polishing after the spray welding; and a new outer ring tube is fabricated, the outer ring tube is cut into at least three sections which are butt jointed and positioned and fixed to the inner ring of the cavity base, and the outer ring tube is welded on the inner ring of the cavity base. The waste chilling ring is repaired, so an expensive fee for replacing a new chilling ring is saved, production cost of an enterprise is saved, and waste reutilization is realized.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105171330A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105171330A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105171330A3</originalsourceid><addsrcrecordid>eNrjZNDzTS3JyE9RSMsvUihKLUjMLMrMS1dIzsjMyQExwLz8NIX0xOLMtMzUIh4G1rTEnOJUXijNzaDo5hri7KGbWpAfn1pckJicmpdaEu_sZ2hgamhuaGxs4GhMjBoA4fEqQQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for repairing chilling ring of gasifier</title><source>esp@cenet</source><creator>CUI LIMING ; LI YUYING ; HOU SHUBO ; HUO CHENGBIN ; GAO BO ; WANG JINHUI</creator><creatorcontrib>CUI LIMING ; LI YUYING ; HOU SHUBO ; HUO CHENGBIN ; GAO BO ; WANG JINHUI</creatorcontrib><description>The invention relates to a technique of repairing a chilling ring of a waste coal water slurry gasifier. The method for repairing the chilling ring of the gasifier comprises the steps that an original outer ring tube is cut down from the inner ring of a cavity base; lathe turning is carried out on a water outlet of a water distribution hole on the inner ring of the cavity base, impurities on the lathe turning surface are removed by abrasive blasting, a thickness removed by the lathe turning is made up by spray welding, and a new water distribution hole is drilled in the inner ring of the cavity base; impurities on washed parts of the outer surface of a water distribution inner ring are removed by the abrasive blasting, and an original size of the water distribution inner ring is recovered through processing and polishing after the spray welding; and a new outer ring tube is fabricated, the outer ring tube is cut into at least three sections which are butt jointed and positioned and fixed to the inner ring of the cavity base, and the outer ring tube is welded on the inner ring of the cavity base. The waste chilling ring is repaired, so an expensive fee for replacing a new chilling ring is saved, production cost of an enterprise is saved, and waste reutilization is realized.</description><language>eng</language><subject>COMBINED OPERATIONS ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; OTHER WORKING OF METAL ; PERFORMING OPERATIONS ; TRANSPORTING ; UNIVERSAL MACHINE TOOLS</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151223&amp;DB=EPODOC&amp;CC=CN&amp;NR=105171330A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151223&amp;DB=EPODOC&amp;CC=CN&amp;NR=105171330A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CUI LIMING</creatorcontrib><creatorcontrib>LI YUYING</creatorcontrib><creatorcontrib>HOU SHUBO</creatorcontrib><creatorcontrib>HUO CHENGBIN</creatorcontrib><creatorcontrib>GAO BO</creatorcontrib><creatorcontrib>WANG JINHUI</creatorcontrib><title>Method for repairing chilling ring of gasifier</title><description>The invention relates to a technique of repairing a chilling ring of a waste coal water slurry gasifier. The method for repairing the chilling ring of the gasifier comprises the steps that an original outer ring tube is cut down from the inner ring of a cavity base; lathe turning is carried out on a water outlet of a water distribution hole on the inner ring of the cavity base, impurities on the lathe turning surface are removed by abrasive blasting, a thickness removed by the lathe turning is made up by spray welding, and a new water distribution hole is drilled in the inner ring of the cavity base; impurities on washed parts of the outer surface of a water distribution inner ring are removed by the abrasive blasting, and an original size of the water distribution inner ring is recovered through processing and polishing after the spray welding; and a new outer ring tube is fabricated, the outer ring tube is cut into at least three sections which are butt jointed and positioned and fixed to the inner ring of the cavity base, and the outer ring tube is welded on the inner ring of the cavity base. The waste chilling ring is repaired, so an expensive fee for replacing a new chilling ring is saved, production cost of an enterprise is saved, and waste reutilization is realized.</description><subject>COMBINED OPERATIONS</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>OTHER WORKING OF METAL</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>UNIVERSAL MACHINE TOOLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNDzTS3JyE9RSMsvUihKLUjMLMrMS1dIzsjMyQExwLz8NIX0xOLMtMzUIh4G1rTEnOJUXijNzaDo5hri7KGbWpAfn1pckJicmpdaEu_sZ2hgamhuaGxs4GhMjBoA4fEqQQ</recordid><startdate>20151223</startdate><enddate>20151223</enddate><creator>CUI LIMING</creator><creator>LI YUYING</creator><creator>HOU SHUBO</creator><creator>HUO CHENGBIN</creator><creator>GAO BO</creator><creator>WANG JINHUI</creator><scope>EVB</scope></search><sort><creationdate>20151223</creationdate><title>Method for repairing chilling ring of gasifier</title><author>CUI LIMING ; LI YUYING ; HOU SHUBO ; HUO CHENGBIN ; GAO BO ; WANG JINHUI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105171330A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>COMBINED OPERATIONS</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>OTHER WORKING OF METAL</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>UNIVERSAL MACHINE TOOLS</topic><toplevel>online_resources</toplevel><creatorcontrib>CUI LIMING</creatorcontrib><creatorcontrib>LI YUYING</creatorcontrib><creatorcontrib>HOU SHUBO</creatorcontrib><creatorcontrib>HUO CHENGBIN</creatorcontrib><creatorcontrib>GAO BO</creatorcontrib><creatorcontrib>WANG JINHUI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CUI LIMING</au><au>LI YUYING</au><au>HOU SHUBO</au><au>HUO CHENGBIN</au><au>GAO BO</au><au>WANG JINHUI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for repairing chilling ring of gasifier</title><date>2015-12-23</date><risdate>2015</risdate><abstract>The invention relates to a technique of repairing a chilling ring of a waste coal water slurry gasifier. The method for repairing the chilling ring of the gasifier comprises the steps that an original outer ring tube is cut down from the inner ring of a cavity base; lathe turning is carried out on a water outlet of a water distribution hole on the inner ring of the cavity base, impurities on the lathe turning surface are removed by abrasive blasting, a thickness removed by the lathe turning is made up by spray welding, and a new water distribution hole is drilled in the inner ring of the cavity base; impurities on washed parts of the outer surface of a water distribution inner ring are removed by the abrasive blasting, and an original size of the water distribution inner ring is recovered through processing and polishing after the spray welding; and a new outer ring tube is fabricated, the outer ring tube is cut into at least three sections which are butt jointed and positioned and fixed to the inner ring of the cavity base, and the outer ring tube is welded on the inner ring of the cavity base. The waste chilling ring is repaired, so an expensive fee for replacing a new chilling ring is saved, production cost of an enterprise is saved, and waste reutilization is realized.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN105171330A
source esp@cenet
subjects COMBINED OPERATIONS
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
OTHER WORKING OF METAL
PERFORMING OPERATIONS
TRANSPORTING
UNIVERSAL MACHINE TOOLS
title Method for repairing chilling ring of gasifier
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T02%3A57%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CUI%20LIMING&rft.date=2015-12-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105171330A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true