Three-dimensional graphite alkene/cobaltosic oxide composite material, preparation method thereof and application

The invention discloses a three-dimensional graphite alkene/cobaltosic oxide composite material and a preparation method thereof. The three-dimensional graphite alkene/cobaltosic oxide composite material comprises graphite alkene and cobaltosic oxide and has a three-dimensional micrometer or three-d...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHANG XING, MA PENG, LIU FAN, LIU YILIN, LIN HUALIN, HAN SHENG, WANG CHI, HUANG QI, ZHOU JIAWEI, CHU LEI, XIONG LIPING, WANG XINJING, LI FEI, HANG ZHIJUN, HE ZHONGYI, AI YANI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHANG XING
MA PENG
LIU FAN
LIU YILIN
LIN HUALIN
HAN SHENG
WANG CHI
HUANG QI
ZHOU JIAWEI
CHU LEI
XIONG LIPING
WANG XINJING
LI FEI
HANG ZHIJUN
HE ZHONGYI
AI YANI
description The invention discloses a three-dimensional graphite alkene/cobaltosic oxide composite material and a preparation method thereof. The three-dimensional graphite alkene/cobaltosic oxide composite material comprises graphite alkene and cobaltosic oxide and has a three-dimensional micrometer or three-dimensional nano porous structure, and the cobaltosic oxide is uniformly distributed on the surface of the graphite alkene. The preparation method comprises steps that, an oxidation graphite alkene dispersion liquid and a divalent cobalt salt dispersion liquid are firstly prepared, the oxidation graphite alkene dispersion liquid and the divalent cobalt salt dispersion liquid are then mixed, uniform ultrasonic dispersion is realized, after oil bath temperature control, centrifugation and washing for the mixed oxidation graphite alkene/ divalent cobalt salt liquid are carried out, the oxidation graphite alkene is further added, uniform ultrasonic dispersion is realized to acquire the mixed oxidation graphite alkene/ cobalt hydroxide liquid, hydro-thermal reaction generates, graphite alkene/ cobaltosic oxide hydrogel is obtained, through pre-freezing and freeze-drying treatment, the three-dimensional graphite alkene/cobaltosic oxide composite material having specific capacity up to 748F/g and having good circulation and multiplying power performance is acquired. The preparation method has advantages of simple and reliable operation, low cost and environmental-protection performance.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105161318A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105161318A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105161318A3</originalsourceid><addsrcrecordid>eNqNjbEKAjEQRK-xEPUf1t5Dw6HYyqFYWV1_rMmeCSbZNUnh5xvED7AaHvOYmTevwSai1rhAMTuO6OGRUKwrBOifFGmr-Y6-cHYa-O0MgeYgFasRsFBy6DcgiQQTljoBgYplA8VSIp4AowEU8U5_62Uzm9BnWv1y0awv56G_tiQ8UhbU9bSM_U3t9uqgOnU8df84Hyu7RJs</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Three-dimensional graphite alkene/cobaltosic oxide composite material, preparation method thereof and application</title><source>esp@cenet</source><creator>CHANG XING ; MA PENG ; LIU FAN ; LIU YILIN ; LIN HUALIN ; HAN SHENG ; WANG CHI ; HUANG QI ; ZHOU JIAWEI ; CHU LEI ; XIONG LIPING ; WANG XINJING ; LI FEI ; HANG ZHIJUN ; HE ZHONGYI ; AI YANI</creator><creatorcontrib>CHANG XING ; MA PENG ; LIU FAN ; LIU YILIN ; LIN HUALIN ; HAN SHENG ; WANG CHI ; HUANG QI ; ZHOU JIAWEI ; CHU LEI ; XIONG LIPING ; WANG XINJING ; LI FEI ; HANG ZHIJUN ; HE ZHONGYI ; AI YANI</creatorcontrib><description>The invention discloses a three-dimensional graphite alkene/cobaltosic oxide composite material and a preparation method thereof. The three-dimensional graphite alkene/cobaltosic oxide composite material comprises graphite alkene and cobaltosic oxide and has a three-dimensional micrometer or three-dimensional nano porous structure, and the cobaltosic oxide is uniformly distributed on the surface of the graphite alkene. The preparation method comprises steps that, an oxidation graphite alkene dispersion liquid and a divalent cobalt salt dispersion liquid are firstly prepared, the oxidation graphite alkene dispersion liquid and the divalent cobalt salt dispersion liquid are then mixed, uniform ultrasonic dispersion is realized, after oil bath temperature control, centrifugation and washing for the mixed oxidation graphite alkene/ divalent cobalt salt liquid are carried out, the oxidation graphite alkene is further added, uniform ultrasonic dispersion is realized to acquire the mixed oxidation graphite alkene/ cobalt hydroxide liquid, hydro-thermal reaction generates, graphite alkene/ cobaltosic oxide hydrogel is obtained, through pre-freezing and freeze-drying treatment, the three-dimensional graphite alkene/cobaltosic oxide composite material having specific capacity up to 748F/g and having good circulation and multiplying power performance is acquired. The preparation method has advantages of simple and reliable operation, low cost and environmental-protection performance.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CAPACITORS ; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE ; ELECTRICITY</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151216&amp;DB=EPODOC&amp;CC=CN&amp;NR=105161318A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151216&amp;DB=EPODOC&amp;CC=CN&amp;NR=105161318A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHANG XING</creatorcontrib><creatorcontrib>MA PENG</creatorcontrib><creatorcontrib>LIU FAN</creatorcontrib><creatorcontrib>LIU YILIN</creatorcontrib><creatorcontrib>LIN HUALIN</creatorcontrib><creatorcontrib>HAN SHENG</creatorcontrib><creatorcontrib>WANG CHI</creatorcontrib><creatorcontrib>HUANG QI</creatorcontrib><creatorcontrib>ZHOU JIAWEI</creatorcontrib><creatorcontrib>CHU LEI</creatorcontrib><creatorcontrib>XIONG LIPING</creatorcontrib><creatorcontrib>WANG XINJING</creatorcontrib><creatorcontrib>LI FEI</creatorcontrib><creatorcontrib>HANG ZHIJUN</creatorcontrib><creatorcontrib>HE ZHONGYI</creatorcontrib><creatorcontrib>AI YANI</creatorcontrib><title>Three-dimensional graphite alkene/cobaltosic oxide composite material, preparation method thereof and application</title><description>The invention discloses a three-dimensional graphite alkene/cobaltosic oxide composite material and a preparation method thereof. The three-dimensional graphite alkene/cobaltosic oxide composite material comprises graphite alkene and cobaltosic oxide and has a three-dimensional micrometer or three-dimensional nano porous structure, and the cobaltosic oxide is uniformly distributed on the surface of the graphite alkene. The preparation method comprises steps that, an oxidation graphite alkene dispersion liquid and a divalent cobalt salt dispersion liquid are firstly prepared, the oxidation graphite alkene dispersion liquid and the divalent cobalt salt dispersion liquid are then mixed, uniform ultrasonic dispersion is realized, after oil bath temperature control, centrifugation and washing for the mixed oxidation graphite alkene/ divalent cobalt salt liquid are carried out, the oxidation graphite alkene is further added, uniform ultrasonic dispersion is realized to acquire the mixed oxidation graphite alkene/ cobalt hydroxide liquid, hydro-thermal reaction generates, graphite alkene/ cobaltosic oxide hydrogel is obtained, through pre-freezing and freeze-drying treatment, the three-dimensional graphite alkene/cobaltosic oxide composite material having specific capacity up to 748F/g and having good circulation and multiplying power performance is acquired. The preparation method has advantages of simple and reliable operation, low cost and environmental-protection performance.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CAPACITORS</subject><subject>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</subject><subject>ELECTRICITY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjbEKAjEQRK-xEPUf1t5Dw6HYyqFYWV1_rMmeCSbZNUnh5xvED7AaHvOYmTevwSai1rhAMTuO6OGRUKwrBOifFGmr-Y6-cHYa-O0MgeYgFasRsFBy6DcgiQQTljoBgYplA8VSIp4AowEU8U5_62Uzm9BnWv1y0awv56G_tiQ8UhbU9bSM_U3t9uqgOnU8df84Hyu7RJs</recordid><startdate>20151216</startdate><enddate>20151216</enddate><creator>CHANG XING</creator><creator>MA PENG</creator><creator>LIU FAN</creator><creator>LIU YILIN</creator><creator>LIN HUALIN</creator><creator>HAN SHENG</creator><creator>WANG CHI</creator><creator>HUANG QI</creator><creator>ZHOU JIAWEI</creator><creator>CHU LEI</creator><creator>XIONG LIPING</creator><creator>WANG XINJING</creator><creator>LI FEI</creator><creator>HANG ZHIJUN</creator><creator>HE ZHONGYI</creator><creator>AI YANI</creator><scope>EVB</scope></search><sort><creationdate>20151216</creationdate><title>Three-dimensional graphite alkene/cobaltosic oxide composite material, preparation method thereof and application</title><author>CHANG XING ; MA PENG ; LIU FAN ; LIU YILIN ; LIN HUALIN ; HAN SHENG ; WANG CHI ; HUANG QI ; ZHOU JIAWEI ; CHU LEI ; XIONG LIPING ; WANG XINJING ; LI FEI ; HANG ZHIJUN ; HE ZHONGYI ; AI YANI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105161318A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CAPACITORS</topic><topic>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</topic><topic>ELECTRICITY</topic><toplevel>online_resources</toplevel><creatorcontrib>CHANG XING</creatorcontrib><creatorcontrib>MA PENG</creatorcontrib><creatorcontrib>LIU FAN</creatorcontrib><creatorcontrib>LIU YILIN</creatorcontrib><creatorcontrib>LIN HUALIN</creatorcontrib><creatorcontrib>HAN SHENG</creatorcontrib><creatorcontrib>WANG CHI</creatorcontrib><creatorcontrib>HUANG QI</creatorcontrib><creatorcontrib>ZHOU JIAWEI</creatorcontrib><creatorcontrib>CHU LEI</creatorcontrib><creatorcontrib>XIONG LIPING</creatorcontrib><creatorcontrib>WANG XINJING</creatorcontrib><creatorcontrib>LI FEI</creatorcontrib><creatorcontrib>HANG ZHIJUN</creatorcontrib><creatorcontrib>HE ZHONGYI</creatorcontrib><creatorcontrib>AI YANI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHANG XING</au><au>MA PENG</au><au>LIU FAN</au><au>LIU YILIN</au><au>LIN HUALIN</au><au>HAN SHENG</au><au>WANG CHI</au><au>HUANG QI</au><au>ZHOU JIAWEI</au><au>CHU LEI</au><au>XIONG LIPING</au><au>WANG XINJING</au><au>LI FEI</au><au>HANG ZHIJUN</au><au>HE ZHONGYI</au><au>AI YANI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Three-dimensional graphite alkene/cobaltosic oxide composite material, preparation method thereof and application</title><date>2015-12-16</date><risdate>2015</risdate><abstract>The invention discloses a three-dimensional graphite alkene/cobaltosic oxide composite material and a preparation method thereof. The three-dimensional graphite alkene/cobaltosic oxide composite material comprises graphite alkene and cobaltosic oxide and has a three-dimensional micrometer or three-dimensional nano porous structure, and the cobaltosic oxide is uniformly distributed on the surface of the graphite alkene. The preparation method comprises steps that, an oxidation graphite alkene dispersion liquid and a divalent cobalt salt dispersion liquid are firstly prepared, the oxidation graphite alkene dispersion liquid and the divalent cobalt salt dispersion liquid are then mixed, uniform ultrasonic dispersion is realized, after oil bath temperature control, centrifugation and washing for the mixed oxidation graphite alkene/ divalent cobalt salt liquid are carried out, the oxidation graphite alkene is further added, uniform ultrasonic dispersion is realized to acquire the mixed oxidation graphite alkene/ cobalt hydroxide liquid, hydro-thermal reaction generates, graphite alkene/ cobaltosic oxide hydrogel is obtained, through pre-freezing and freeze-drying treatment, the three-dimensional graphite alkene/cobaltosic oxide composite material having specific capacity up to 748F/g and having good circulation and multiplying power performance is acquired. The preparation method has advantages of simple and reliable operation, low cost and environmental-protection performance.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN105161318A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CAPACITORS
CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE
ELECTRICITY
title Three-dimensional graphite alkene/cobaltosic oxide composite material, preparation method thereof and application
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T12%3A17%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHANG%20XING&rft.date=2015-12-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105161318A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true