Heat-resisting alloy for 700-DEG C ultra-supercritical steam turbine rotor and preparation method thereof

The invention relates to heat-resisting alloy for a 700-DEG C ultra-supercritical steam turbine rotor and a preparation method thereof, and belongs to the technical field of heat-resisting alloy. The alloy comprises the following ingredients by weight percent: 0.04 to 0.06 percent of C, 19 to 21 per...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BAO HANSHENG, HE XIKOU, YANG GONGXIAN, YANG GANG, WANG LIMIN, LIU ZHENGDONG, WANG ZHIGANG, TIAN ZHONGLIANG, CHEN ZHENGZONG, JIANG SENBAO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator BAO HANSHENG
HE XIKOU
YANG GONGXIAN
YANG GANG
WANG LIMIN
LIU ZHENGDONG
WANG ZHIGANG
TIAN ZHONGLIANG
CHEN ZHENGZONG
JIANG SENBAO
description The invention relates to heat-resisting alloy for a 700-DEG C ultra-supercritical steam turbine rotor and a preparation method thereof, and belongs to the technical field of heat-resisting alloy. The alloy comprises the following ingredients by weight percent: 0.04 to 0.06 percent of C, 19 to 21 percent of Cr, 8.6 to 9.0 percent of Mo, 11 to 13 percent of Co, 0.40 to 0.80 percent of W, 1.10 to 1.30 percent of Al, 1.20 to 1.40 percent of Ti, 0.20 to 0.50 percent of Nb, less than or equal to 0.15 percent of Fe, 30 to 50ppm of B, 0.01 percent of Zr, 0.002 percent of Mg and the balance of Ni and impurities; wherein, the content of Al and Ti needs to satisfy the following condition: (Al+Ti) is more than or equal to 2.5 percent and less than or equal to 2.6 percent, and Ti/Al is more than or equal to 1.0 or less than or equal to 1.1. A VIM, VAR and ESR triplet process is used for smelting the alloy, soft-sheath forging is adopted, and the heat-resisting alloy has advantages that the comprehensive performance is excellent and the alloy is suitable for manufacturing the 700-DEG C ultra-supercritical steam turbine rotor.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105112728A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105112728A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105112728A3</originalsourceid><addsrcrecordid>eNqNyzEOgkAQQFEaC6PeYTzAJoAx2BpEqazsyQiDTLLsbGaHwttr4QGsfvP-OuOW0JxS4mQcXoDeyxtGUajy3F2aG9SweFN0aYmkvbJxjx6SEc5giz45EKjY98AwQFSKqGgsAWaySQawiZRk3GarEX2i3a-bbH9tHnXrKEpHKWJPgayr70V-LIqyKk_nwz_mA7McP-o</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Heat-resisting alloy for 700-DEG C ultra-supercritical steam turbine rotor and preparation method thereof</title><source>esp@cenet</source><creator>BAO HANSHENG ; HE XIKOU ; YANG GONGXIAN ; YANG GANG ; WANG LIMIN ; LIU ZHENGDONG ; WANG ZHIGANG ; TIAN ZHONGLIANG ; CHEN ZHENGZONG ; JIANG SENBAO</creator><creatorcontrib>BAO HANSHENG ; HE XIKOU ; YANG GONGXIAN ; YANG GANG ; WANG LIMIN ; LIU ZHENGDONG ; WANG ZHIGANG ; TIAN ZHONGLIANG ; CHEN ZHENGZONG ; JIANG SENBAO</creatorcontrib><description>The invention relates to heat-resisting alloy for a 700-DEG C ultra-supercritical steam turbine rotor and a preparation method thereof, and belongs to the technical field of heat-resisting alloy. The alloy comprises the following ingredients by weight percent: 0.04 to 0.06 percent of C, 19 to 21 percent of Cr, 8.6 to 9.0 percent of Mo, 11 to 13 percent of Co, 0.40 to 0.80 percent of W, 1.10 to 1.30 percent of Al, 1.20 to 1.40 percent of Ti, 0.20 to 0.50 percent of Nb, less than or equal to 0.15 percent of Fe, 30 to 50ppm of B, 0.01 percent of Zr, 0.002 percent of Mg and the balance of Ni and impurities; wherein, the content of Al and Ti needs to satisfy the following condition: (Al+Ti) is more than or equal to 2.5 percent and less than or equal to 2.6 percent, and Ti/Al is more than or equal to 1.0 or less than or equal to 1.1. A VIM, VAR and ESR triplet process is used for smelting the alloy, soft-sheath forging is adopted, and the heat-resisting alloy has advantages that the comprehensive performance is excellent and the alloy is suitable for manufacturing the 700-DEG C ultra-supercritical steam turbine rotor.</description><language>eng</language><subject>ALLOYS ; BLASTING ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; ENGINE PLANTS IN GENERAL ; FERROUS OR NON-FERROUS ALLOYS ; HEATING ; LIGHTING ; MACHINES OR ENGINES IN GENERAL ; MECHANICAL ENGINEERING ; METALLURGY ; NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAMTURBINES ; STEAM ENGINES ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; WEAPONS</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151202&amp;DB=EPODOC&amp;CC=CN&amp;NR=105112728A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151202&amp;DB=EPODOC&amp;CC=CN&amp;NR=105112728A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BAO HANSHENG</creatorcontrib><creatorcontrib>HE XIKOU</creatorcontrib><creatorcontrib>YANG GONGXIAN</creatorcontrib><creatorcontrib>YANG GANG</creatorcontrib><creatorcontrib>WANG LIMIN</creatorcontrib><creatorcontrib>LIU ZHENGDONG</creatorcontrib><creatorcontrib>WANG ZHIGANG</creatorcontrib><creatorcontrib>TIAN ZHONGLIANG</creatorcontrib><creatorcontrib>CHEN ZHENGZONG</creatorcontrib><creatorcontrib>JIANG SENBAO</creatorcontrib><title>Heat-resisting alloy for 700-DEG C ultra-supercritical steam turbine rotor and preparation method thereof</title><description>The invention relates to heat-resisting alloy for a 700-DEG C ultra-supercritical steam turbine rotor and a preparation method thereof, and belongs to the technical field of heat-resisting alloy. The alloy comprises the following ingredients by weight percent: 0.04 to 0.06 percent of C, 19 to 21 percent of Cr, 8.6 to 9.0 percent of Mo, 11 to 13 percent of Co, 0.40 to 0.80 percent of W, 1.10 to 1.30 percent of Al, 1.20 to 1.40 percent of Ti, 0.20 to 0.50 percent of Nb, less than or equal to 0.15 percent of Fe, 30 to 50ppm of B, 0.01 percent of Zr, 0.002 percent of Mg and the balance of Ni and impurities; wherein, the content of Al and Ti needs to satisfy the following condition: (Al+Ti) is more than or equal to 2.5 percent and less than or equal to 2.6 percent, and Ti/Al is more than or equal to 1.0 or less than or equal to 1.1. A VIM, VAR and ESR triplet process is used for smelting the alloy, soft-sheath forging is adopted, and the heat-resisting alloy has advantages that the comprehensive performance is excellent and the alloy is suitable for manufacturing the 700-DEG C ultra-supercritical steam turbine rotor.</description><subject>ALLOYS</subject><subject>BLASTING</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>ENGINE PLANTS IN GENERAL</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>HEATING</subject><subject>LIGHTING</subject><subject>MACHINES OR ENGINES IN GENERAL</subject><subject>MECHANICAL ENGINEERING</subject><subject>METALLURGY</subject><subject>NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAMTURBINES</subject><subject>STEAM ENGINES</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>WEAPONS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyzEOgkAQQFEaC6PeYTzAJoAx2BpEqazsyQiDTLLsbGaHwttr4QGsfvP-OuOW0JxS4mQcXoDeyxtGUajy3F2aG9SweFN0aYmkvbJxjx6SEc5giz45EKjY98AwQFSKqGgsAWaySQawiZRk3GarEX2i3a-bbH9tHnXrKEpHKWJPgayr70V-LIqyKk_nwz_mA7McP-o</recordid><startdate>20151202</startdate><enddate>20151202</enddate><creator>BAO HANSHENG</creator><creator>HE XIKOU</creator><creator>YANG GONGXIAN</creator><creator>YANG GANG</creator><creator>WANG LIMIN</creator><creator>LIU ZHENGDONG</creator><creator>WANG ZHIGANG</creator><creator>TIAN ZHONGLIANG</creator><creator>CHEN ZHENGZONG</creator><creator>JIANG SENBAO</creator><scope>EVB</scope></search><sort><creationdate>20151202</creationdate><title>Heat-resisting alloy for 700-DEG C ultra-supercritical steam turbine rotor and preparation method thereof</title><author>BAO HANSHENG ; HE XIKOU ; YANG GONGXIAN ; YANG GANG ; WANG LIMIN ; LIU ZHENGDONG ; WANG ZHIGANG ; TIAN ZHONGLIANG ; CHEN ZHENGZONG ; JIANG SENBAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105112728A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>ALLOYS</topic><topic>BLASTING</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>ENGINE PLANTS IN GENERAL</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>HEATING</topic><topic>LIGHTING</topic><topic>MACHINES OR ENGINES IN GENERAL</topic><topic>MECHANICAL ENGINEERING</topic><topic>METALLURGY</topic><topic>NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAMTURBINES</topic><topic>STEAM ENGINES</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>WEAPONS</topic><toplevel>online_resources</toplevel><creatorcontrib>BAO HANSHENG</creatorcontrib><creatorcontrib>HE XIKOU</creatorcontrib><creatorcontrib>YANG GONGXIAN</creatorcontrib><creatorcontrib>YANG GANG</creatorcontrib><creatorcontrib>WANG LIMIN</creatorcontrib><creatorcontrib>LIU ZHENGDONG</creatorcontrib><creatorcontrib>WANG ZHIGANG</creatorcontrib><creatorcontrib>TIAN ZHONGLIANG</creatorcontrib><creatorcontrib>CHEN ZHENGZONG</creatorcontrib><creatorcontrib>JIANG SENBAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BAO HANSHENG</au><au>HE XIKOU</au><au>YANG GONGXIAN</au><au>YANG GANG</au><au>WANG LIMIN</au><au>LIU ZHENGDONG</au><au>WANG ZHIGANG</au><au>TIAN ZHONGLIANG</au><au>CHEN ZHENGZONG</au><au>JIANG SENBAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Heat-resisting alloy for 700-DEG C ultra-supercritical steam turbine rotor and preparation method thereof</title><date>2015-12-02</date><risdate>2015</risdate><abstract>The invention relates to heat-resisting alloy for a 700-DEG C ultra-supercritical steam turbine rotor and a preparation method thereof, and belongs to the technical field of heat-resisting alloy. The alloy comprises the following ingredients by weight percent: 0.04 to 0.06 percent of C, 19 to 21 percent of Cr, 8.6 to 9.0 percent of Mo, 11 to 13 percent of Co, 0.40 to 0.80 percent of W, 1.10 to 1.30 percent of Al, 1.20 to 1.40 percent of Ti, 0.20 to 0.50 percent of Nb, less than or equal to 0.15 percent of Fe, 30 to 50ppm of B, 0.01 percent of Zr, 0.002 percent of Mg and the balance of Ni and impurities; wherein, the content of Al and Ti needs to satisfy the following condition: (Al+Ti) is more than or equal to 2.5 percent and less than or equal to 2.6 percent, and Ti/Al is more than or equal to 1.0 or less than or equal to 1.1. A VIM, VAR and ESR triplet process is used for smelting the alloy, soft-sheath forging is adopted, and the heat-resisting alloy has advantages that the comprehensive performance is excellent and the alloy is suitable for manufacturing the 700-DEG C ultra-supercritical steam turbine rotor.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN105112728A
source esp@cenet
subjects ALLOYS
BLASTING
CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS
CHEMISTRY
ENGINE PLANTS IN GENERAL
FERROUS OR NON-FERROUS ALLOYS
HEATING
LIGHTING
MACHINES OR ENGINES IN GENERAL
MECHANICAL ENGINEERING
METALLURGY
NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAMTURBINES
STEAM ENGINES
TREATMENT OF ALLOYS OR NON-FERROUS METALS
WEAPONS
title Heat-resisting alloy for 700-DEG C ultra-supercritical steam turbine rotor and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T07%3A34%3A24IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BAO%20HANSHENG&rft.date=2015-12-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105112728A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true