Preparation method for rosin modified phenolic resin for ink

The invention provides a preparation method for rosin modified phenolic resin for ink. The preparation method comprises the steps that 1, rosin is put into a reaction still, and is heated to 180 DEG C, fumaric acid is added, the temperature continues to rise to 210 DEG C to 215 DEG C, and heat prese...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HU XIAOMING, HUANG HONGXIU, FAN LU, CHEN YUBIN
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HU XIAOMING
HUANG HONGXIU
FAN LU
CHEN YUBIN
description The invention provides a preparation method for rosin modified phenolic resin for ink. The preparation method comprises the steps that 1, rosin is put into a reaction still, and is heated to 180 DEG C, fumaric acid is added, the temperature continues to rise to 210 DEG C to 215 DEG C, and heat preservation is carried out for 1 h to 1.5 h; 2, pentaerythritol and magnesium oxide are added to the reaction still, the temperature is reduced to 160 DEG C to 170 DEG C, dodecyl phenol and nonylphenol are added according to the molar ratio of 1 to 1.02-1.04, then the temperature continues to be reduced to 130 DEG C to 140 DEG C, paraformaldehyde is added according to the phenolic aldehyde molar ratio of 1 to 2.2-2.3, and heat preservation is carried out for 2 h to 2.5 h; 3, the temperature in the reaction still rises to 260 DEG C to 270 DEG C, heat preservation is carried out, an esterification reaction is conducted till the acid value is smaller than 25 mgKOH/g, low-boiling-point substances are distilled out in a decompression mode, and the rosin modified phenolic resin for the ink is obtained. The obtained resin is high in viscosity, good in solubility, large in molecular weight, even in distribution and suitable for slab offset printing ink.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN105037668A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN105037668A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN105037668A3</originalsourceid><addsrcrecordid>eNrjZLAJKEotSCxKLMnMz1PITS3JyE9RSMsvUijKL84ECuSnZKZlpqYoFGSk5uXnZCYrFKWCxEEqMvOyeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGpgbG5mZmFozExagD3IS_g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method for rosin modified phenolic resin for ink</title><source>esp@cenet</source><creator>HU XIAOMING ; HUANG HONGXIU ; FAN LU ; CHEN YUBIN</creator><creatorcontrib>HU XIAOMING ; HUANG HONGXIU ; FAN LU ; CHEN YUBIN</creatorcontrib><description>The invention provides a preparation method for rosin modified phenolic resin for ink. The preparation method comprises the steps that 1, rosin is put into a reaction still, and is heated to 180 DEG C, fumaric acid is added, the temperature continues to rise to 210 DEG C to 215 DEG C, and heat preservation is carried out for 1 h to 1.5 h; 2, pentaerythritol and magnesium oxide are added to the reaction still, the temperature is reduced to 160 DEG C to 170 DEG C, dodecyl phenol and nonylphenol are added according to the molar ratio of 1 to 1.02-1.04, then the temperature continues to be reduced to 130 DEG C to 140 DEG C, paraformaldehyde is added according to the phenolic aldehyde molar ratio of 1 to 2.2-2.3, and heat preservation is carried out for 2 h to 2.5 h; 3, the temperature in the reaction still rises to 260 DEG C to 270 DEG C, heat preservation is carried out, an esterification reaction is conducted till the acid value is smaller than 25 mgKOH/g, low-boiling-point substances are distilled out in a decompression mode, and the rosin modified phenolic resin for the ink is obtained. The obtained resin is high in viscosity, good in solubility, large in molecular weight, even in distribution and suitable for slab offset printing ink.</description><language>eng</language><subject>ADHESIVES ; CHEMICAL PAINT OR INK REMOVERS ; CHEMISTRY ; COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS ; COMPOSITIONS BASED THEREON ; CORRECTING FLUIDS ; DYES ; FILLING PASTES ; INKS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; PASTES OR SOLIDS FOR COLOURING OR PRINTING ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF MATERIALS THEREFOR ; WOODSTAINS</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151111&amp;DB=EPODOC&amp;CC=CN&amp;NR=105037668A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20151111&amp;DB=EPODOC&amp;CC=CN&amp;NR=105037668A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HU XIAOMING</creatorcontrib><creatorcontrib>HUANG HONGXIU</creatorcontrib><creatorcontrib>FAN LU</creatorcontrib><creatorcontrib>CHEN YUBIN</creatorcontrib><title>Preparation method for rosin modified phenolic resin for ink</title><description>The invention provides a preparation method for rosin modified phenolic resin for ink. The preparation method comprises the steps that 1, rosin is put into a reaction still, and is heated to 180 DEG C, fumaric acid is added, the temperature continues to rise to 210 DEG C to 215 DEG C, and heat preservation is carried out for 1 h to 1.5 h; 2, pentaerythritol and magnesium oxide are added to the reaction still, the temperature is reduced to 160 DEG C to 170 DEG C, dodecyl phenol and nonylphenol are added according to the molar ratio of 1 to 1.02-1.04, then the temperature continues to be reduced to 130 DEG C to 140 DEG C, paraformaldehyde is added according to the phenolic aldehyde molar ratio of 1 to 2.2-2.3, and heat preservation is carried out for 2 h to 2.5 h; 3, the temperature in the reaction still rises to 260 DEG C to 270 DEG C, heat preservation is carried out, an esterification reaction is conducted till the acid value is smaller than 25 mgKOH/g, low-boiling-point substances are distilled out in a decompression mode, and the rosin modified phenolic resin for the ink is obtained. The obtained resin is high in viscosity, good in solubility, large in molecular weight, even in distribution and suitable for slab offset printing ink.</description><subject>ADHESIVES</subject><subject>CHEMICAL PAINT OR INK REMOVERS</subject><subject>CHEMISTRY</subject><subject>COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>CORRECTING FLUIDS</subject><subject>DYES</subject><subject>FILLING PASTES</subject><subject>INKS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>PASTES OR SOLIDS FOR COLOURING OR PRINTING</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF MATERIALS THEREFOR</subject><subject>WOODSTAINS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAJKEotSCxKLMnMz1PITS3JyE9RSMsvUijKL84ECuSnZKZlpqYoFGSk5uXnZCYrFKWCxEEqMvOyeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGpgbG5mZmFozExagD3IS_g</recordid><startdate>20151111</startdate><enddate>20151111</enddate><creator>HU XIAOMING</creator><creator>HUANG HONGXIU</creator><creator>FAN LU</creator><creator>CHEN YUBIN</creator><scope>EVB</scope></search><sort><creationdate>20151111</creationdate><title>Preparation method for rosin modified phenolic resin for ink</title><author>HU XIAOMING ; HUANG HONGXIU ; FAN LU ; CHEN YUBIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN105037668A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>ADHESIVES</topic><topic>CHEMICAL PAINT OR INK REMOVERS</topic><topic>CHEMISTRY</topic><topic>COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>CORRECTING FLUIDS</topic><topic>DYES</topic><topic>FILLING PASTES</topic><topic>INKS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>PASTES OR SOLIDS FOR COLOURING OR PRINTING</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF MATERIALS THEREFOR</topic><topic>WOODSTAINS</topic><toplevel>online_resources</toplevel><creatorcontrib>HU XIAOMING</creatorcontrib><creatorcontrib>HUANG HONGXIU</creatorcontrib><creatorcontrib>FAN LU</creatorcontrib><creatorcontrib>CHEN YUBIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HU XIAOMING</au><au>HUANG HONGXIU</au><au>FAN LU</au><au>CHEN YUBIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method for rosin modified phenolic resin for ink</title><date>2015-11-11</date><risdate>2015</risdate><abstract>The invention provides a preparation method for rosin modified phenolic resin for ink. The preparation method comprises the steps that 1, rosin is put into a reaction still, and is heated to 180 DEG C, fumaric acid is added, the temperature continues to rise to 210 DEG C to 215 DEG C, and heat preservation is carried out for 1 h to 1.5 h; 2, pentaerythritol and magnesium oxide are added to the reaction still, the temperature is reduced to 160 DEG C to 170 DEG C, dodecyl phenol and nonylphenol are added according to the molar ratio of 1 to 1.02-1.04, then the temperature continues to be reduced to 130 DEG C to 140 DEG C, paraformaldehyde is added according to the phenolic aldehyde molar ratio of 1 to 2.2-2.3, and heat preservation is carried out for 2 h to 2.5 h; 3, the temperature in the reaction still rises to 260 DEG C to 270 DEG C, heat preservation is carried out, an esterification reaction is conducted till the acid value is smaller than 25 mgKOH/g, low-boiling-point substances are distilled out in a decompression mode, and the rosin modified phenolic resin for the ink is obtained. The obtained resin is high in viscosity, good in solubility, large in molecular weight, even in distribution and suitable for slab offset printing ink.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN105037668A
source esp@cenet
subjects ADHESIVES
CHEMICAL PAINT OR INK REMOVERS
CHEMISTRY
COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS
COMPOSITIONS BASED THEREON
CORRECTING FLUIDS
DYES
FILLING PASTES
INKS
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
ORGANIC MACROMOLECULAR COMPOUNDS
PAINTS
PASTES OR SOLIDS FOR COLOURING OR PRINTING
POLISHES
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF MATERIALS THEREFOR
WOODSTAINS
title Preparation method for rosin modified phenolic resin for ink
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T05%3A09%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HU%20XIAOMING&rft.date=2015-11-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN105037668A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true