Preparation technology for high-performance solvent copolymerization acrylate pressure-sensitive adhesive
Provided is preparation technology for a high-performance solvent copolymerization acrylate pressure-sensitive adhesive. The adhesive comprises the following components, by weight ratio: 65-90% of a soft monomer, 10-30% of a hard monomer, and 3-5% of a crosslinking monomer. The adhesive also compris...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WU PEILONG |
description | Provided is preparation technology for a high-performance solvent copolymerization acrylate pressure-sensitive adhesive. The adhesive comprises the following components, by weight ratio: 65-90% of a soft monomer, 10-30% of a hard monomer, and 3-5% of a crosslinking monomer. The adhesive also comprises a solvent, the weight of which is 10% of the total weight of monomers at an initial reaction stage, is 10-20% of the total weight of monomers at an early stage of a growth stage, is 40-60% of the total weight of monomers at a later stage of the growth stage, and is 138-163% of the total weight of monomers at a final reaction stage, and an initiator, the weight of which is 0.03-0.5% of the total weight of monomers. According to the invention, the copolymerization acrylate is high in average molecular weight and wide in molecular weight distribution. The molecular weight of the copolymerization acrylate can be measured through gel permeation chromatography, and has a weight-average molecular weight in a range of 450-900 kg/mol and a molecular weight distribution index in a range of 4-20. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104845565A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104845565A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104845565A3</originalsourceid><addsrcrecordid>eNqNi7EKwkAQBdNYiPoP5wcEFBOxlaBYiYW9LOdL7uBye-yegfj1BvQDrGaKmXnhb4JEQtlzNBnWRQ7cjaZlMc53rkyQyXuKFkY5DIjZWE4cxh7i39-RrIyBMkwSqL4EpSKqz36AoaeDTrIsZi0FxerHRbE-n-7NpUTiBzSRRUR-NNftpjpUdb2vj7t_mg9fWULE</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation technology for high-performance solvent copolymerization acrylate pressure-sensitive adhesive</title><source>esp@cenet</source><creator>WU PEILONG</creator><creatorcontrib>WU PEILONG</creatorcontrib><description>Provided is preparation technology for a high-performance solvent copolymerization acrylate pressure-sensitive adhesive. The adhesive comprises the following components, by weight ratio: 65-90% of a soft monomer, 10-30% of a hard monomer, and 3-5% of a crosslinking monomer. The adhesive also comprises a solvent, the weight of which is 10% of the total weight of monomers at an initial reaction stage, is 10-20% of the total weight of monomers at an early stage of a growth stage, is 40-60% of the total weight of monomers at a later stage of the growth stage, and is 138-163% of the total weight of monomers at a final reaction stage, and an initiator, the weight of which is 0.03-0.5% of the total weight of monomers. According to the invention, the copolymerization acrylate is high in average molecular weight and wide in molecular weight distribution. The molecular weight of the copolymerization acrylate can be measured through gel permeation chromatography, and has a weight-average molecular weight in a range of 450-900 kg/mol and a molecular weight distribution index in a range of 4-20.</description><language>eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; DYES ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150819&DB=EPODOC&CC=CN&NR=104845565A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150819&DB=EPODOC&CC=CN&NR=104845565A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WU PEILONG</creatorcontrib><title>Preparation technology for high-performance solvent copolymerization acrylate pressure-sensitive adhesive</title><description>Provided is preparation technology for a high-performance solvent copolymerization acrylate pressure-sensitive adhesive. The adhesive comprises the following components, by weight ratio: 65-90% of a soft monomer, 10-30% of a hard monomer, and 3-5% of a crosslinking monomer. The adhesive also comprises a solvent, the weight of which is 10% of the total weight of monomers at an initial reaction stage, is 10-20% of the total weight of monomers at an early stage of a growth stage, is 40-60% of the total weight of monomers at a later stage of the growth stage, and is 138-163% of the total weight of monomers at a final reaction stage, and an initiator, the weight of which is 0.03-0.5% of the total weight of monomers. According to the invention, the copolymerization acrylate is high in average molecular weight and wide in molecular weight distribution. The molecular weight of the copolymerization acrylate can be measured through gel permeation chromatography, and has a weight-average molecular weight in a range of 450-900 kg/mol and a molecular weight distribution index in a range of 4-20.</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>DYES</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi7EKwkAQBdNYiPoP5wcEFBOxlaBYiYW9LOdL7uBye-yegfj1BvQDrGaKmXnhb4JEQtlzNBnWRQ7cjaZlMc53rkyQyXuKFkY5DIjZWE4cxh7i39-RrIyBMkwSqL4EpSKqz36AoaeDTrIsZi0FxerHRbE-n-7NpUTiBzSRRUR-NNftpjpUdb2vj7t_mg9fWULE</recordid><startdate>20150819</startdate><enddate>20150819</enddate><creator>WU PEILONG</creator><scope>EVB</scope></search><sort><creationdate>20150819</creationdate><title>Preparation technology for high-performance solvent copolymerization acrylate pressure-sensitive adhesive</title><author>WU PEILONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104845565A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>DYES</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>WU PEILONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WU PEILONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation technology for high-performance solvent copolymerization acrylate pressure-sensitive adhesive</title><date>2015-08-19</date><risdate>2015</risdate><abstract>Provided is preparation technology for a high-performance solvent copolymerization acrylate pressure-sensitive adhesive. The adhesive comprises the following components, by weight ratio: 65-90% of a soft monomer, 10-30% of a hard monomer, and 3-5% of a crosslinking monomer. The adhesive also comprises a solvent, the weight of which is 10% of the total weight of monomers at an initial reaction stage, is 10-20% of the total weight of monomers at an early stage of a growth stage, is 40-60% of the total weight of monomers at a later stage of the growth stage, and is 138-163% of the total weight of monomers at a final reaction stage, and an initiator, the weight of which is 0.03-0.5% of the total weight of monomers. According to the invention, the copolymerization acrylate is high in average molecular weight and wide in molecular weight distribution. The molecular weight of the copolymerization acrylate can be measured through gel permeation chromatography, and has a weight-average molecular weight in a range of 450-900 kg/mol and a molecular weight distribution index in a range of 4-20.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_CN104845565A |
source | esp@cenet |
subjects | ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ADHESIVES CHEMISTRY COMPOSITIONS BASED THEREON DYES MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ORGANIC MACROMOLECULAR COMPOUNDS PAINTS POLISHES THEIR PREPARATION OR CHEMICAL WORKING-UP USE OF MATERIALS AS ADHESIVES |
title | Preparation technology for high-performance solvent copolymerization acrylate pressure-sensitive adhesive |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T10%3A01%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WU%20PEILONG&rft.date=2015-08-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104845565A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |