Continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for lithium battery
The invention provides a continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for a lithium battery. The continuous synthesis method is used for manufacturing nickel-cobalt-manganese ternary hydroxide through processes of nucleus growth and particle growth. The nucleus growth pro...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | QIU PING YANG PING JIANG XIAOFENG WANG ZHAOZHE WU JING LIU JINCAI JIANG MINGXI WANG JUANHUI CHANG QUANZHONG WAN YUNYUN |
description | The invention provides a continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for a lithium battery. The continuous synthesis method is used for manufacturing nickel-cobalt-manganese ternary hydroxide through processes of nucleus growth and particle growth. The nucleus growth process is that the reaction is performed in a crystal nucleus generation kettle, and the nucleus generation is controlled in a way that the online detected pH value is 10.0-11.5; the particle growth process is that the primary growth of nucleus is performed in a primary reaction kettle, the optimized growth is performed in an optimization reaction kettle to improve the particle size distribution and morphology of particles, and a particle growth solution containing the nucleus formed in the nucleus growth process is controlled in a way that the online detected pH value is 9.5-11.0. The continuous synthesis method enables the generated nickel-cobalt-manganese ternary hydroxide to be narrower and more homogeneous in the particle size distribution, and can form particles regular in shape and size. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104795558A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104795558A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104795558A3</originalsourceid><addsrcrecordid>eNqNyrEKwkAMANAuDqL-Q_yAgqJFHaUoTk6OQknbtHd4TcolBe_vdfADnN7y5tmzFDbPk0wKmtgcqVcYyJy0IB2wb14U8kZqDJYPyD0yKYFRZIwJXGqjvH1L0EmE4M35aYAa7RvSMpt1GJRWPxfZ-np5lLecRqlIR2yIyaryvt3sD6eiKI7n3T_nA0cJPPk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for lithium battery</title><source>esp@cenet</source><creator>QIU PING ; YANG PING ; JIANG XIAOFENG ; WANG ZHAOZHE ; WU JING ; LIU JINCAI ; JIANG MINGXI ; WANG JUANHUI ; CHANG QUANZHONG ; WAN YUNYUN</creator><creatorcontrib>QIU PING ; YANG PING ; JIANG XIAOFENG ; WANG ZHAOZHE ; WU JING ; LIU JINCAI ; JIANG MINGXI ; WANG JUANHUI ; CHANG QUANZHONG ; WAN YUNYUN</creatorcontrib><description>The invention provides a continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for a lithium battery. The continuous synthesis method is used for manufacturing nickel-cobalt-manganese ternary hydroxide through processes of nucleus growth and particle growth. The nucleus growth process is that the reaction is performed in a crystal nucleus generation kettle, and the nucleus generation is controlled in a way that the online detected pH value is 10.0-11.5; the particle growth process is that the primary growth of nucleus is performed in a primary reaction kettle, the optimized growth is performed in an optimization reaction kettle to improve the particle size distribution and morphology of particles, and a particle growth solution containing the nucleus formed in the nucleus growth process is controlled in a way that the online detected pH value is 9.5-11.0. The continuous synthesis method enables the generated nickel-cobalt-manganese ternary hydroxide to be narrower and more homogeneous in the particle size distribution, and can form particles regular in shape and size.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150722&DB=EPODOC&CC=CN&NR=104795558A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150722&DB=EPODOC&CC=CN&NR=104795558A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>QIU PING</creatorcontrib><creatorcontrib>YANG PING</creatorcontrib><creatorcontrib>JIANG XIAOFENG</creatorcontrib><creatorcontrib>WANG ZHAOZHE</creatorcontrib><creatorcontrib>WU JING</creatorcontrib><creatorcontrib>LIU JINCAI</creatorcontrib><creatorcontrib>JIANG MINGXI</creatorcontrib><creatorcontrib>WANG JUANHUI</creatorcontrib><creatorcontrib>CHANG QUANZHONG</creatorcontrib><creatorcontrib>WAN YUNYUN</creatorcontrib><title>Continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for lithium battery</title><description>The invention provides a continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for a lithium battery. The continuous synthesis method is used for manufacturing nickel-cobalt-manganese ternary hydroxide through processes of nucleus growth and particle growth. The nucleus growth process is that the reaction is performed in a crystal nucleus generation kettle, and the nucleus generation is controlled in a way that the online detected pH value is 10.0-11.5; the particle growth process is that the primary growth of nucleus is performed in a primary reaction kettle, the optimized growth is performed in an optimization reaction kettle to improve the particle size distribution and morphology of particles, and a particle growth solution containing the nucleus formed in the nucleus growth process is controlled in a way that the online detected pH value is 9.5-11.0. The continuous synthesis method enables the generated nickel-cobalt-manganese ternary hydroxide to be narrower and more homogeneous in the particle size distribution, and can form particles regular in shape and size.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwkAMANAuDqL-Q_yAgqJFHaUoTk6OQknbtHd4TcolBe_vdfADnN7y5tmzFDbPk0wKmtgcqVcYyJy0IB2wb14U8kZqDJYPyD0yKYFRZIwJXGqjvH1L0EmE4M35aYAa7RvSMpt1GJRWPxfZ-np5lLecRqlIR2yIyaryvt3sD6eiKI7n3T_nA0cJPPk</recordid><startdate>20150722</startdate><enddate>20150722</enddate><creator>QIU PING</creator><creator>YANG PING</creator><creator>JIANG XIAOFENG</creator><creator>WANG ZHAOZHE</creator><creator>WU JING</creator><creator>LIU JINCAI</creator><creator>JIANG MINGXI</creator><creator>WANG JUANHUI</creator><creator>CHANG QUANZHONG</creator><creator>WAN YUNYUN</creator><scope>EVB</scope></search><sort><creationdate>20150722</creationdate><title>Continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for lithium battery</title><author>QIU PING ; YANG PING ; JIANG XIAOFENG ; WANG ZHAOZHE ; WU JING ; LIU JINCAI ; JIANG MINGXI ; WANG JUANHUI ; CHANG QUANZHONG ; WAN YUNYUN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104795558A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>QIU PING</creatorcontrib><creatorcontrib>YANG PING</creatorcontrib><creatorcontrib>JIANG XIAOFENG</creatorcontrib><creatorcontrib>WANG ZHAOZHE</creatorcontrib><creatorcontrib>WU JING</creatorcontrib><creatorcontrib>LIU JINCAI</creatorcontrib><creatorcontrib>JIANG MINGXI</creatorcontrib><creatorcontrib>WANG JUANHUI</creatorcontrib><creatorcontrib>CHANG QUANZHONG</creatorcontrib><creatorcontrib>WAN YUNYUN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>QIU PING</au><au>YANG PING</au><au>JIANG XIAOFENG</au><au>WANG ZHAOZHE</au><au>WU JING</au><au>LIU JINCAI</au><au>JIANG MINGXI</au><au>WANG JUANHUI</au><au>CHANG QUANZHONG</au><au>WAN YUNYUN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for lithium battery</title><date>2015-07-22</date><risdate>2015</risdate><abstract>The invention provides a continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for a lithium battery. The continuous synthesis method is used for manufacturing nickel-cobalt-manganese ternary hydroxide through processes of nucleus growth and particle growth. The nucleus growth process is that the reaction is performed in a crystal nucleus generation kettle, and the nucleus generation is controlled in a way that the online detected pH value is 10.0-11.5; the particle growth process is that the primary growth of nucleus is performed in a primary reaction kettle, the optimized growth is performed in an optimization reaction kettle to improve the particle size distribution and morphology of particles, and a particle growth solution containing the nucleus formed in the nucleus growth process is controlled in a way that the online detected pH value is 9.5-11.0. The continuous synthesis method enables the generated nickel-cobalt-manganese ternary hydroxide to be narrower and more homogeneous in the particle size distribution, and can form particles regular in shape and size.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_CN104795558A |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS ELECTRICITY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
title | Continuous synthesis method of nickel-cobalt-manganese ternary hydroxide for lithium battery |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T02%3A36%3A59IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=QIU%20PING&rft.date=2015-07-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104795558A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |