Method for preparing natural hydraulic lime by using limestone and quartz powder

The invention relates to a method for preparing natural hydraulic lime by using limestone and quartz powder, and belongs to a building material. The method is implemented by taking limestone as a main raw material through the steps of adding high-purity quartz powder to adjust the ratio of calcium o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LAN MINGZHANG, CUI SUPING, MAO QIANJIN, WANG YALI, MA HAIFENG, WANG ZIMING
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LAN MINGZHANG
CUI SUPING
MAO QIANJIN
WANG YALI
MA HAIFENG
WANG ZIMING
description The invention relates to a method for preparing natural hydraulic lime by using limestone and quartz powder, and belongs to a building material. The method is implemented by taking limestone as a main raw material through the steps of adding high-purity quartz powder to adjust the ratio of calcium oxide and silicon oxide, controlling the content of alumina, carrying out mixed material co-grinding for 6-10 hours by using a ball mill, adding water with a mass accounting for 8% of the mass of a mixed raw material, fully stirring, putting the obtained object into a sealing bag to place for 6-7 hours, pressing the obtained object into a cylinder, drying the cylinder by using a drying oven, putting the cylinder into a muffle furnace to calcinate for 3 hours at a temperature of 1100-1200 DEG C, cooling the calcinated material to room temperature in the air by air cooling, determining the free calcium oxide content of the calcinated product, adding a certain amount of water for slaking into the calcinated product, and after the slaking process is completed, obtaining desirable natural hydraulic lime.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104724953A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104724953A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104724953A3</originalsourceid><addsrcrecordid>eNrjZAjwTS3JyE9RSMsvUigoSi1ILMrMS1fISywpLUrMUcioTClKLM3JTFbIycxNVUiqVCgtBsmDeMUl-XmpCol5KQqFpYlFJVUKBfnlKalFPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0MDE3MjE0tTY0ZgYNQC_8Tes</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing natural hydraulic lime by using limestone and quartz powder</title><source>esp@cenet</source><creator>LAN MINGZHANG ; CUI SUPING ; MAO QIANJIN ; WANG YALI ; MA HAIFENG ; WANG ZIMING</creator><creatorcontrib>LAN MINGZHANG ; CUI SUPING ; MAO QIANJIN ; WANG YALI ; MA HAIFENG ; WANG ZIMING</creatorcontrib><description>The invention relates to a method for preparing natural hydraulic lime by using limestone and quartz powder, and belongs to a building material. The method is implemented by taking limestone as a main raw material through the steps of adding high-purity quartz powder to adjust the ratio of calcium oxide and silicon oxide, controlling the content of alumina, carrying out mixed material co-grinding for 6-10 hours by using a ball mill, adding water with a mass accounting for 8% of the mass of a mixed raw material, fully stirring, putting the obtained object into a sealing bag to place for 6-7 hours, pressing the obtained object into a cylinder, drying the cylinder by using a drying oven, putting the cylinder into a muffle furnace to calcinate for 3 hours at a temperature of 1100-1200 DEG C, cooling the calcinated material to room temperature in the air by air cooling, determining the free calcium oxide content of the calcinated product, adding a certain amount of water for slaking into the calcinated product, and after the slaking process is completed, obtaining desirable natural hydraulic lime.</description><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150624&amp;DB=EPODOC&amp;CC=CN&amp;NR=104724953A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150624&amp;DB=EPODOC&amp;CC=CN&amp;NR=104724953A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LAN MINGZHANG</creatorcontrib><creatorcontrib>CUI SUPING</creatorcontrib><creatorcontrib>MAO QIANJIN</creatorcontrib><creatorcontrib>WANG YALI</creatorcontrib><creatorcontrib>MA HAIFENG</creatorcontrib><creatorcontrib>WANG ZIMING</creatorcontrib><title>Method for preparing natural hydraulic lime by using limestone and quartz powder</title><description>The invention relates to a method for preparing natural hydraulic lime by using limestone and quartz powder, and belongs to a building material. The method is implemented by taking limestone as a main raw material through the steps of adding high-purity quartz powder to adjust the ratio of calcium oxide and silicon oxide, controlling the content of alumina, carrying out mixed material co-grinding for 6-10 hours by using a ball mill, adding water with a mass accounting for 8% of the mass of a mixed raw material, fully stirring, putting the obtained object into a sealing bag to place for 6-7 hours, pressing the obtained object into a cylinder, drying the cylinder by using a drying oven, putting the cylinder into a muffle furnace to calcinate for 3 hours at a temperature of 1100-1200 DEG C, cooling the calcinated material to room temperature in the air by air cooling, determining the free calcium oxide content of the calcinated product, adding a certain amount of water for slaking into the calcinated product, and after the slaking process is completed, obtaining desirable natural hydraulic lime.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZAjwTS3JyE9RSMsvUigoSi1ILMrMS1fISywpLUrMUcioTClKLM3JTFbIycxNVUiqVCgtBsmDeMUl-XmpCol5KQqFpYlFJVUKBfnlKalFPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0MDE3MjE0tTY0ZgYNQC_8Tes</recordid><startdate>20150624</startdate><enddate>20150624</enddate><creator>LAN MINGZHANG</creator><creator>CUI SUPING</creator><creator>MAO QIANJIN</creator><creator>WANG YALI</creator><creator>MA HAIFENG</creator><creator>WANG ZIMING</creator><scope>EVB</scope></search><sort><creationdate>20150624</creationdate><title>Method for preparing natural hydraulic lime by using limestone and quartz powder</title><author>LAN MINGZHANG ; CUI SUPING ; MAO QIANJIN ; WANG YALI ; MA HAIFENG ; WANG ZIMING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104724953A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>LAN MINGZHANG</creatorcontrib><creatorcontrib>CUI SUPING</creatorcontrib><creatorcontrib>MAO QIANJIN</creatorcontrib><creatorcontrib>WANG YALI</creatorcontrib><creatorcontrib>MA HAIFENG</creatorcontrib><creatorcontrib>WANG ZIMING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LAN MINGZHANG</au><au>CUI SUPING</au><au>MAO QIANJIN</au><au>WANG YALI</au><au>MA HAIFENG</au><au>WANG ZIMING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing natural hydraulic lime by using limestone and quartz powder</title><date>2015-06-24</date><risdate>2015</risdate><abstract>The invention relates to a method for preparing natural hydraulic lime by using limestone and quartz powder, and belongs to a building material. The method is implemented by taking limestone as a main raw material through the steps of adding high-purity quartz powder to adjust the ratio of calcium oxide and silicon oxide, controlling the content of alumina, carrying out mixed material co-grinding for 6-10 hours by using a ball mill, adding water with a mass accounting for 8% of the mass of a mixed raw material, fully stirring, putting the obtained object into a sealing bag to place for 6-7 hours, pressing the obtained object into a cylinder, drying the cylinder by using a drying oven, putting the cylinder into a muffle furnace to calcinate for 3 hours at a temperature of 1100-1200 DEG C, cooling the calcinated material to room temperature in the air by air cooling, determining the free calcium oxide content of the calcinated product, adding a certain amount of water for slaking into the calcinated product, and after the slaking process is completed, obtaining desirable natural hydraulic lime.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN104724953A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Method for preparing natural hydraulic lime by using limestone and quartz powder
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T04%3A21%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LAN%20MINGZHANG&rft.date=2015-06-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104724953A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true