Synthetic process of heavy metal chelating agent

The invention belongs to the technical field of chelating agents, and in particular relates to a synthetic process of a heavy metal chelating agent. The method comprises the following steps: firstly, diluting organic amine for 2-10 times by using organic solvents; secondly, adding the enough amount...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG ZHE, ZHANG BIN, LI JIWEN, DUAN HUIWEI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG ZHE
ZHANG BIN
LI JIWEN
DUAN HUIWEI
description The invention belongs to the technical field of chelating agents, and in particular relates to a synthetic process of a heavy metal chelating agent. The method comprises the following steps: firstly, diluting organic amine for 2-10 times by using organic solvents; secondly, adding the enough amount of carbon disulfide into the diluted organic amine by controlling the reaction temperature to be between 30 and 50 DEG C to obtain an intermediate product; and thirdly, adding hydroxide powder into the intermediate product and stirring, performing solid-liquid separation to obtain the heavy metal chelating agent. Compared with the prior art, by reducing the concentration of organic amine, the intense degree of the reaction can be effectively reduced, so that the reaction temperature is increased. A test proves that the quality of the product has no difference from that of the previous product when the temperature is controlled to be between 30 and 50 DEG C; therefore, under a normal condition, normal production can be met by using common circulating water, so that equipment facilities such as refrigerating units for cooling are eliminated, the labor intensity of operation personnel is also reduced, and the cost is greatly reduced.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104528910A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104528910A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104528910A3</originalsourceid><addsrcrecordid>eNrjZDAIrswryUgtyUxWKCjKT04tLlbIT1PISE0sq1TITS1JzFFIzkjNSSzJzEtXSExPzSvhYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBiamRhaWhgaOxsSoAQBo6ytQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Synthetic process of heavy metal chelating agent</title><source>esp@cenet</source><creator>ZHANG ZHE ; ZHANG BIN ; LI JIWEN ; DUAN HUIWEI</creator><creatorcontrib>ZHANG ZHE ; ZHANG BIN ; LI JIWEN ; DUAN HUIWEI</creatorcontrib><description>The invention belongs to the technical field of chelating agents, and in particular relates to a synthetic process of a heavy metal chelating agent. The method comprises the following steps: firstly, diluting organic amine for 2-10 times by using organic solvents; secondly, adding the enough amount of carbon disulfide into the diluted organic amine by controlling the reaction temperature to be between 30 and 50 DEG C to obtain an intermediate product; and thirdly, adding hydroxide powder into the intermediate product and stirring, performing solid-liquid separation to obtain the heavy metal chelating agent. Compared with the prior art, by reducing the concentration of organic amine, the intense degree of the reaction can be effectively reduced, so that the reaction temperature is increased. A test proves that the quality of the product has no difference from that of the previous product when the temperature is controlled to be between 30 and 50 DEG C; therefore, under a normal condition, normal production can be met by using common circulating water, so that equipment facilities such as refrigerating units for cooling are eliminated, the labor intensity of operation personnel is also reduced, and the cost is greatly reduced.</description><language>eng</language><subject>CHEMISTRY ; METALLURGY ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150422&amp;DB=EPODOC&amp;CC=CN&amp;NR=104528910A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150422&amp;DB=EPODOC&amp;CC=CN&amp;NR=104528910A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG ZHE</creatorcontrib><creatorcontrib>ZHANG BIN</creatorcontrib><creatorcontrib>LI JIWEN</creatorcontrib><creatorcontrib>DUAN HUIWEI</creatorcontrib><title>Synthetic process of heavy metal chelating agent</title><description>The invention belongs to the technical field of chelating agents, and in particular relates to a synthetic process of a heavy metal chelating agent. The method comprises the following steps: firstly, diluting organic amine for 2-10 times by using organic solvents; secondly, adding the enough amount of carbon disulfide into the diluted organic amine by controlling the reaction temperature to be between 30 and 50 DEG C to obtain an intermediate product; and thirdly, adding hydroxide powder into the intermediate product and stirring, performing solid-liquid separation to obtain the heavy metal chelating agent. Compared with the prior art, by reducing the concentration of organic amine, the intense degree of the reaction can be effectively reduced, so that the reaction temperature is increased. A test proves that the quality of the product has no difference from that of the previous product when the temperature is controlled to be between 30 and 50 DEG C; therefore, under a normal condition, normal production can be met by using common circulating water, so that equipment facilities such as refrigerating units for cooling are eliminated, the labor intensity of operation personnel is also reduced, and the cost is greatly reduced.</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAIrswryUgtyUxWKCjKT04tLlbIT1PISE0sq1TITS1JzFFIzkjNSSzJzEtXSExPzSvhYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBiamRhaWhgaOxsSoAQBo6ytQ</recordid><startdate>20150422</startdate><enddate>20150422</enddate><creator>ZHANG ZHE</creator><creator>ZHANG BIN</creator><creator>LI JIWEN</creator><creator>DUAN HUIWEI</creator><scope>EVB</scope></search><sort><creationdate>20150422</creationdate><title>Synthetic process of heavy metal chelating agent</title><author>ZHANG ZHE ; ZHANG BIN ; LI JIWEN ; DUAN HUIWEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104528910A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG ZHE</creatorcontrib><creatorcontrib>ZHANG BIN</creatorcontrib><creatorcontrib>LI JIWEN</creatorcontrib><creatorcontrib>DUAN HUIWEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG ZHE</au><au>ZHANG BIN</au><au>LI JIWEN</au><au>DUAN HUIWEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Synthetic process of heavy metal chelating agent</title><date>2015-04-22</date><risdate>2015</risdate><abstract>The invention belongs to the technical field of chelating agents, and in particular relates to a synthetic process of a heavy metal chelating agent. The method comprises the following steps: firstly, diluting organic amine for 2-10 times by using organic solvents; secondly, adding the enough amount of carbon disulfide into the diluted organic amine by controlling the reaction temperature to be between 30 and 50 DEG C to obtain an intermediate product; and thirdly, adding hydroxide powder into the intermediate product and stirring, performing solid-liquid separation to obtain the heavy metal chelating agent. Compared with the prior art, by reducing the concentration of organic amine, the intense degree of the reaction can be effectively reduced, so that the reaction temperature is increased. A test proves that the quality of the product has no difference from that of the previous product when the temperature is controlled to be between 30 and 50 DEG C; therefore, under a normal condition, normal production can be met by using common circulating water, so that equipment facilities such as refrigerating units for cooling are eliminated, the labor intensity of operation personnel is also reduced, and the cost is greatly reduced.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN104528910A
source esp@cenet
subjects CHEMISTRY
METALLURGY
TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE
title Synthetic process of heavy metal chelating agent
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T11%3A21%3A21IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20ZHE&rft.date=2015-04-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104528910A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true