Method for producing -shaped antiskid safety glass cup

The invention relates to the field of glassware, and aims at providing a method for producing a *-shaped antiskid safety glass cup. The method comprises the following steps: a, heating glass to 1400 to 2000 DEG C to ensure that the glass becomes liquid; b, removing the impurities in the glass liquid...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: WANG ZUGANG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG ZUGANG
description The invention relates to the field of glassware, and aims at providing a method for producing a *-shaped antiskid safety glass cup. The method comprises the following steps: a, heating glass to 1400 to 2000 DEG C to ensure that the glass becomes liquid; b, removing the impurities in the glass liquid obtained in the step a and pouring the glass liquid into a high temperature resistant grinding tool, wherein the high temperature resistant grinding tool comprises a plurality of round holes the same as the cup bottom in the aspect of size and the bottoms of the round holes are provided with fine *-shaped grooves which extend from the center to the circumference; c, pouring the glass liquid obtained in the step a into a glass tube, wherein the glass tube is made of a grinding tool sleeve tube, and the size of the glass tube is the same as the diameter of the cup opening of the cup body of the glass cup; d, when the glass liquid flows uniformly to fill the round holes, scraping the glass liquid at the round holes by using a high temperature resistant flat scraper; e, adhering a layer of high temperature resistant explosion-proof membrane on the outer wall of the glass tube obtained in the step c and cutting into the length size required by the cup body. After the *-shaped antiskid safety glass cup is broken, the fragments do not puncture the hands during the sweeping, so that the injury is avoided.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104337349A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104337349A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104337349A3</originalsourceid><addsrcrecordid>eNrjZDDzTS3JyE9RSMsvUigoyk8pTc7MS1fQLc5ILEhNUUjMK8kszs5MUShOTEstqVRIz0ksLlZILi3gYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBibGxubGJpaOxsSoAQCFGy1b</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for producing -shaped antiskid safety glass cup</title><source>esp@cenet</source><creator>WANG ZUGANG</creator><creatorcontrib>WANG ZUGANG</creatorcontrib><description>The invention relates to the field of glassware, and aims at providing a method for producing a *-shaped antiskid safety glass cup. The method comprises the following steps: a, heating glass to 1400 to 2000 DEG C to ensure that the glass becomes liquid; b, removing the impurities in the glass liquid obtained in the step a and pouring the glass liquid into a high temperature resistant grinding tool, wherein the high temperature resistant grinding tool comprises a plurality of round holes the same as the cup bottom in the aspect of size and the bottoms of the round holes are provided with fine *-shaped grooves which extend from the center to the circumference; c, pouring the glass liquid obtained in the step a into a glass tube, wherein the glass tube is made of a grinding tool sleeve tube, and the size of the glass tube is the same as the diameter of the cup opening of the cup body of the glass cup; d, when the glass liquid flows uniformly to fill the round holes, scraping the glass liquid at the round holes by using a high temperature resistant flat scraper; e, adhering a layer of high temperature resistant explosion-proof membrane on the outer wall of the glass tube obtained in the step c and cutting into the length size required by the cup body. After the *-shaped antiskid safety glass cup is broken, the fragments do not puncture the hands during the sweeping, so that the injury is avoided.</description><language>eng</language><subject>COFFEE MILLS ; DOMESTIC ARTICLES OR APPLIANCES ; FURNITURE ; HOUSEHOLD OR TABLE EQUIPMENT ; HUMAN NECESSITIES ; SPICE MILLS ; SUCTION CLEANERS IN GENERAL</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150211&amp;DB=EPODOC&amp;CC=CN&amp;NR=104337349A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150211&amp;DB=EPODOC&amp;CC=CN&amp;NR=104337349A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG ZUGANG</creatorcontrib><title>Method for producing -shaped antiskid safety glass cup</title><description>The invention relates to the field of glassware, and aims at providing a method for producing a *-shaped antiskid safety glass cup. The method comprises the following steps: a, heating glass to 1400 to 2000 DEG C to ensure that the glass becomes liquid; b, removing the impurities in the glass liquid obtained in the step a and pouring the glass liquid into a high temperature resistant grinding tool, wherein the high temperature resistant grinding tool comprises a plurality of round holes the same as the cup bottom in the aspect of size and the bottoms of the round holes are provided with fine *-shaped grooves which extend from the center to the circumference; c, pouring the glass liquid obtained in the step a into a glass tube, wherein the glass tube is made of a grinding tool sleeve tube, and the size of the glass tube is the same as the diameter of the cup opening of the cup body of the glass cup; d, when the glass liquid flows uniformly to fill the round holes, scraping the glass liquid at the round holes by using a high temperature resistant flat scraper; e, adhering a layer of high temperature resistant explosion-proof membrane on the outer wall of the glass tube obtained in the step c and cutting into the length size required by the cup body. After the *-shaped antiskid safety glass cup is broken, the fragments do not puncture the hands during the sweeping, so that the injury is avoided.</description><subject>COFFEE MILLS</subject><subject>DOMESTIC ARTICLES OR APPLIANCES</subject><subject>FURNITURE</subject><subject>HOUSEHOLD OR TABLE EQUIPMENT</subject><subject>HUMAN NECESSITIES</subject><subject>SPICE MILLS</subject><subject>SUCTION CLEANERS IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDzTS3JyE9RSMsvUigoyk8pTc7MS1fQLc5ILEhNUUjMK8kszs5MUShOTEstqVRIz0ksLlZILi3gYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBibGxubGJpaOxsSoAQCFGy1b</recordid><startdate>20150211</startdate><enddate>20150211</enddate><creator>WANG ZUGANG</creator><scope>EVB</scope></search><sort><creationdate>20150211</creationdate><title>Method for producing -shaped antiskid safety glass cup</title><author>WANG ZUGANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104337349A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>COFFEE MILLS</topic><topic>DOMESTIC ARTICLES OR APPLIANCES</topic><topic>FURNITURE</topic><topic>HOUSEHOLD OR TABLE EQUIPMENT</topic><topic>HUMAN NECESSITIES</topic><topic>SPICE MILLS</topic><topic>SUCTION CLEANERS IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG ZUGANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG ZUGANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for producing -shaped antiskid safety glass cup</title><date>2015-02-11</date><risdate>2015</risdate><abstract>The invention relates to the field of glassware, and aims at providing a method for producing a *-shaped antiskid safety glass cup. The method comprises the following steps: a, heating glass to 1400 to 2000 DEG C to ensure that the glass becomes liquid; b, removing the impurities in the glass liquid obtained in the step a and pouring the glass liquid into a high temperature resistant grinding tool, wherein the high temperature resistant grinding tool comprises a plurality of round holes the same as the cup bottom in the aspect of size and the bottoms of the round holes are provided with fine *-shaped grooves which extend from the center to the circumference; c, pouring the glass liquid obtained in the step a into a glass tube, wherein the glass tube is made of a grinding tool sleeve tube, and the size of the glass tube is the same as the diameter of the cup opening of the cup body of the glass cup; d, when the glass liquid flows uniformly to fill the round holes, scraping the glass liquid at the round holes by using a high temperature resistant flat scraper; e, adhering a layer of high temperature resistant explosion-proof membrane on the outer wall of the glass tube obtained in the step c and cutting into the length size required by the cup body. After the *-shaped antiskid safety glass cup is broken, the fragments do not puncture the hands during the sweeping, so that the injury is avoided.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN104337349A
source esp@cenet
subjects COFFEE MILLS
DOMESTIC ARTICLES OR APPLIANCES
FURNITURE
HOUSEHOLD OR TABLE EQUIPMENT
HUMAN NECESSITIES
SPICE MILLS
SUCTION CLEANERS IN GENERAL
title Method for producing -shaped antiskid safety glass cup
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T23%3A16%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20ZUGANG&rft.date=2015-02-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104337349A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true