Non-oriented silicon steel used for frequency conversion high efficiency compressor and production method thereof

The invention relates to a non-oriented silicon steel used for a frequency conversion high efficiency compressor, which comprises the following components by weight percentage: less than or equal to 0.005% of C, 3.1-3.4% of Si, 0.03-0.1% of Mn, less than or equal to 0.01% of Als, less than or equal...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FENG DAJUN, SHI WENMIN, YANG GUANG, LUO ZHONGHAN, OUYANG YEXIAN, MAO JIONGHUI, WANG XIANGXIN, CHEN SHENGLIN, DU GUANGLIANG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FENG DAJUN
SHI WENMIN
YANG GUANG
LUO ZHONGHAN
OUYANG YEXIAN
MAO JIONGHUI
WANG XIANGXIN
CHEN SHENGLIN
DU GUANGLIANG
description The invention relates to a non-oriented silicon steel used for a frequency conversion high efficiency compressor, which comprises the following components by weight percentage: less than or equal to 0.005% of C, 3.1-3.4% of Si, 0.03-0.1% of Mn, less than or equal to 0.01% of Als, less than or equal to 0.05% of P, greater than 0 and less than or equal to 0.0025%, less than or equal to 0.06%, 0.04-0.06% of Sn, less than or equal to 0.0025%. The method comprises the following steps: smelting according to clean steel and performing continuous casting to obtain a blank; heating the continuous casting and insulating; performing hot rolling; reeling; naturally cooling to room temperature; normalizing; pickling and employing a single cold-reduced method for rolling, annealing the finished product; cooling, coating and finishing. On basis of silicon content level of the current high grade non-oriented silicon steel, the Als content is strictly controlled below 0.01%, magnetic induction is increased to no less than 1.7T from no more than 1.67T of B50 by employing the single cold-reduced method, power frequency iron loss is reduced to no more than 2.35W/kg from no less than 2.6W/kg of P1.5/50, intermediate frequency iron loss is reduced to no more than 17.5W/kg from no less than 20W/kg of P1.0/400, product hardness HV5 is 170-190, and the ratio of percentage elongation A and hardness can be satisfied at 0.13-0.17, and the performance, punching sheet and automatic riveted joint requirement of the frequency conversion high efficiency compressor can be simultaneously satisfied.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104328342A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104328342A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104328342A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAUheEuDqK-w_UBCtp2cJWiOHVyLyU5MYE2N81NBd_eCH0ApwPn_7bF3LEvOTr4BE3iRqfYkyRgpEXyZTiSiZgXePWhHN-I4rKx7mUJxjjl1jSFCJHsB68pRNaLSj85IVnWlCwi2OyLjRlGwWHdXXG8357to0TgHhIGBY_Ut9351NTVpW6qa_2P-QIij0So</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Non-oriented silicon steel used for frequency conversion high efficiency compressor and production method thereof</title><source>esp@cenet</source><creator>FENG DAJUN ; SHI WENMIN ; YANG GUANG ; LUO ZHONGHAN ; OUYANG YEXIAN ; MAO JIONGHUI ; WANG XIANGXIN ; CHEN SHENGLIN ; DU GUANGLIANG</creator><creatorcontrib>FENG DAJUN ; SHI WENMIN ; YANG GUANG ; LUO ZHONGHAN ; OUYANG YEXIAN ; MAO JIONGHUI ; WANG XIANGXIN ; CHEN SHENGLIN ; DU GUANGLIANG</creatorcontrib><description>The invention relates to a non-oriented silicon steel used for a frequency conversion high efficiency compressor, which comprises the following components by weight percentage: less than or equal to 0.005% of C, 3.1-3.4% of Si, 0.03-0.1% of Mn, less than or equal to 0.01% of Als, less than or equal to 0.05% of P, greater than 0 and less than or equal to 0.0025%, less than or equal to 0.06%, 0.04-0.06% of Sn, less than or equal to 0.0025%. The method comprises the following steps: smelting according to clean steel and performing continuous casting to obtain a blank; heating the continuous casting and insulating; performing hot rolling; reeling; naturally cooling to room temperature; normalizing; pickling and employing a single cold-reduced method for rolling, annealing the finished product; cooling, coating and finishing. On basis of silicon content level of the current high grade non-oriented silicon steel, the Als content is strictly controlled below 0.01%, magnetic induction is increased to no less than 1.7T from no more than 1.67T of B50 by employing the single cold-reduced method, power frequency iron loss is reduced to no more than 2.35W/kg from no less than 2.6W/kg of P1.5/50, intermediate frequency iron loss is reduced to no more than 17.5W/kg from no less than 20W/kg of P1.0/400, product hardness HV5 is 170-190, and the ratio of percentage elongation A and hardness can be satisfied at 0.13-0.17, and the performance, punching sheet and automatic riveted joint requirement of the frequency conversion high efficiency compressor can be simultaneously satisfied.</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150204&amp;DB=EPODOC&amp;CC=CN&amp;NR=104328342A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20150204&amp;DB=EPODOC&amp;CC=CN&amp;NR=104328342A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FENG DAJUN</creatorcontrib><creatorcontrib>SHI WENMIN</creatorcontrib><creatorcontrib>YANG GUANG</creatorcontrib><creatorcontrib>LUO ZHONGHAN</creatorcontrib><creatorcontrib>OUYANG YEXIAN</creatorcontrib><creatorcontrib>MAO JIONGHUI</creatorcontrib><creatorcontrib>WANG XIANGXIN</creatorcontrib><creatorcontrib>CHEN SHENGLIN</creatorcontrib><creatorcontrib>DU GUANGLIANG</creatorcontrib><title>Non-oriented silicon steel used for frequency conversion high efficiency compressor and production method thereof</title><description>The invention relates to a non-oriented silicon steel used for a frequency conversion high efficiency compressor, which comprises the following components by weight percentage: less than or equal to 0.005% of C, 3.1-3.4% of Si, 0.03-0.1% of Mn, less than or equal to 0.01% of Als, less than or equal to 0.05% of P, greater than 0 and less than or equal to 0.0025%, less than or equal to 0.06%, 0.04-0.06% of Sn, less than or equal to 0.0025%. The method comprises the following steps: smelting according to clean steel and performing continuous casting to obtain a blank; heating the continuous casting and insulating; performing hot rolling; reeling; naturally cooling to room temperature; normalizing; pickling and employing a single cold-reduced method for rolling, annealing the finished product; cooling, coating and finishing. On basis of silicon content level of the current high grade non-oriented silicon steel, the Als content is strictly controlled below 0.01%, magnetic induction is increased to no less than 1.7T from no more than 1.67T of B50 by employing the single cold-reduced method, power frequency iron loss is reduced to no more than 2.35W/kg from no less than 2.6W/kg of P1.5/50, intermediate frequency iron loss is reduced to no more than 17.5W/kg from no less than 20W/kg of P1.0/400, product hardness HV5 is 170-190, and the ratio of percentage elongation A and hardness can be satisfied at 0.13-0.17, and the performance, punching sheet and automatic riveted joint requirement of the frequency conversion high efficiency compressor can be simultaneously satisfied.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAUheEuDqK-w_UBCtp2cJWiOHVyLyU5MYE2N81NBd_eCH0ApwPn_7bF3LEvOTr4BE3iRqfYkyRgpEXyZTiSiZgXePWhHN-I4rKx7mUJxjjl1jSFCJHsB68pRNaLSj85IVnWlCwi2OyLjRlGwWHdXXG8357to0TgHhIGBY_Ut9351NTVpW6qa_2P-QIij0So</recordid><startdate>20150204</startdate><enddate>20150204</enddate><creator>FENG DAJUN</creator><creator>SHI WENMIN</creator><creator>YANG GUANG</creator><creator>LUO ZHONGHAN</creator><creator>OUYANG YEXIAN</creator><creator>MAO JIONGHUI</creator><creator>WANG XIANGXIN</creator><creator>CHEN SHENGLIN</creator><creator>DU GUANGLIANG</creator><scope>EVB</scope></search><sort><creationdate>20150204</creationdate><title>Non-oriented silicon steel used for frequency conversion high efficiency compressor and production method thereof</title><author>FENG DAJUN ; SHI WENMIN ; YANG GUANG ; LUO ZHONGHAN ; OUYANG YEXIAN ; MAO JIONGHUI ; WANG XIANGXIN ; CHEN SHENGLIN ; DU GUANGLIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104328342A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>FENG DAJUN</creatorcontrib><creatorcontrib>SHI WENMIN</creatorcontrib><creatorcontrib>YANG GUANG</creatorcontrib><creatorcontrib>LUO ZHONGHAN</creatorcontrib><creatorcontrib>OUYANG YEXIAN</creatorcontrib><creatorcontrib>MAO JIONGHUI</creatorcontrib><creatorcontrib>WANG XIANGXIN</creatorcontrib><creatorcontrib>CHEN SHENGLIN</creatorcontrib><creatorcontrib>DU GUANGLIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FENG DAJUN</au><au>SHI WENMIN</au><au>YANG GUANG</au><au>LUO ZHONGHAN</au><au>OUYANG YEXIAN</au><au>MAO JIONGHUI</au><au>WANG XIANGXIN</au><au>CHEN SHENGLIN</au><au>DU GUANGLIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Non-oriented silicon steel used for frequency conversion high efficiency compressor and production method thereof</title><date>2015-02-04</date><risdate>2015</risdate><abstract>The invention relates to a non-oriented silicon steel used for a frequency conversion high efficiency compressor, which comprises the following components by weight percentage: less than or equal to 0.005% of C, 3.1-3.4% of Si, 0.03-0.1% of Mn, less than or equal to 0.01% of Als, less than or equal to 0.05% of P, greater than 0 and less than or equal to 0.0025%, less than or equal to 0.06%, 0.04-0.06% of Sn, less than or equal to 0.0025%. The method comprises the following steps: smelting according to clean steel and performing continuous casting to obtain a blank; heating the continuous casting and insulating; performing hot rolling; reeling; naturally cooling to room temperature; normalizing; pickling and employing a single cold-reduced method for rolling, annealing the finished product; cooling, coating and finishing. On basis of silicon content level of the current high grade non-oriented silicon steel, the Als content is strictly controlled below 0.01%, magnetic induction is increased to no less than 1.7T from no more than 1.67T of B50 by employing the single cold-reduced method, power frequency iron loss is reduced to no more than 2.35W/kg from no less than 2.6W/kg of P1.5/50, intermediate frequency iron loss is reduced to no more than 17.5W/kg from no less than 20W/kg of P1.0/400, product hardness HV5 is 170-190, and the ratio of percentage elongation A and hardness can be satisfied at 0.13-0.17, and the performance, punching sheet and automatic riveted joint requirement of the frequency conversion high efficiency compressor can be simultaneously satisfied.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN104328342A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Non-oriented silicon steel used for frequency conversion high efficiency compressor and production method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T05%3A11%3A56IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FENG%20DAJUN&rft.date=2015-02-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104328342A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true