High temperature stable water swellable rubber composition

A water swellable rubber composition comprising (a) a non-water swellable base rubber, (b) an ethylene oxide based hydrophilic elastomer having from zero up to and including 20 mole % of a crosslinkable curable functional group, and (c) a water swellable non-elastomeric material. The composition has...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHOI SOO-BUM, JUSTICE LAWRENCE J
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHOI SOO-BUM
JUSTICE LAWRENCE J
description A water swellable rubber composition comprising (a) a non-water swellable base rubber, (b) an ethylene oxide based hydrophilic elastomer having from zero up to and including 20 mole % of a crosslinkable curable functional group, and (c) a water swellable non-elastomeric material. The composition has excellent water swell characteristics under prolonged exposure to high temperature and various electrolyte solutions (strongly saline as well as acid conditions) and is particularly suitable for oil field applications. When the ethylene oxide based hydrophilic elastomer (b) has from zero to less than 5 mole % of crosslinkable functional group, the amount of (b) is between about 30 parts and 300 parts by weight based on 100 parts by weight of the base rubber (a) and the amount of (c) is between about 20 parts and 200 parts by weight based on 100 parts by weight of the base rubber (a), the composition is characterized by good shape retention after undergoing constrained swell, as well as a high degree of constrained
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104246115A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104246115A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104246115A3</originalsourceid><addsrcrecordid>eNrjZLDyyEzPUChJzS1ILUosKS1KVSguSUzKSVUoTyxJLVIoLk_NyQHzi0qTkoACyfm5BfnFmSWZ-Xk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTe2c_QwMTIxMzQ0NTRmBg1ALJCL44</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High temperature stable water swellable rubber composition</title><source>esp@cenet</source><creator>CHOI SOO-BUM ; JUSTICE LAWRENCE J</creator><creatorcontrib>CHOI SOO-BUM ; JUSTICE LAWRENCE J</creatorcontrib><description>A water swellable rubber composition comprising (a) a non-water swellable base rubber, (b) an ethylene oxide based hydrophilic elastomer having from zero up to and including 20 mole % of a crosslinkable curable functional group, and (c) a water swellable non-elastomeric material. The composition has excellent water swell characteristics under prolonged exposure to high temperature and various electrolyte solutions (strongly saline as well as acid conditions) and is particularly suitable for oil field applications. When the ethylene oxide based hydrophilic elastomer (b) has from zero to less than 5 mole % of crosslinkable functional group, the amount of (b) is between about 30 parts and 300 parts by weight based on 100 parts by weight of the base rubber (a) and the amount of (c) is between about 20 parts and 200 parts by weight based on 100 parts by weight of the base rubber (a), the composition is characterized by good shape retention after undergoing constrained swell, as well as a high degree of constrained</description><language>chi ; eng</language><subject>EARTH DRILLING ; EARTH DRILLING, e.g. DEEP DRILLING ; FIXED CONSTRUCTIONS ; MINING ; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20141224&amp;DB=EPODOC&amp;CC=CN&amp;NR=104246115A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20141224&amp;DB=EPODOC&amp;CC=CN&amp;NR=104246115A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHOI SOO-BUM</creatorcontrib><creatorcontrib>JUSTICE LAWRENCE J</creatorcontrib><title>High temperature stable water swellable rubber composition</title><description>A water swellable rubber composition comprising (a) a non-water swellable base rubber, (b) an ethylene oxide based hydrophilic elastomer having from zero up to and including 20 mole % of a crosslinkable curable functional group, and (c) a water swellable non-elastomeric material. The composition has excellent water swell characteristics under prolonged exposure to high temperature and various electrolyte solutions (strongly saline as well as acid conditions) and is particularly suitable for oil field applications. When the ethylene oxide based hydrophilic elastomer (b) has from zero to less than 5 mole % of crosslinkable functional group, the amount of (b) is between about 30 parts and 300 parts by weight based on 100 parts by weight of the base rubber (a) and the amount of (c) is between about 20 parts and 200 parts by weight based on 100 parts by weight of the base rubber (a), the composition is characterized by good shape retention after undergoing constrained swell, as well as a high degree of constrained</description><subject>EARTH DRILLING</subject><subject>EARTH DRILLING, e.g. DEEP DRILLING</subject><subject>FIXED CONSTRUCTIONS</subject><subject>MINING</subject><subject>OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLDyyEzPUChJzS1ILUosKS1KVSguSUzKSVUoTyxJLVIoLk_NyQHzi0qTkoACyfm5BfnFmSWZ-Xk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTe2c_QwMTIxMzQ0NTRmBg1ALJCL44</recordid><startdate>20141224</startdate><enddate>20141224</enddate><creator>CHOI SOO-BUM</creator><creator>JUSTICE LAWRENCE J</creator><scope>EVB</scope></search><sort><creationdate>20141224</creationdate><title>High temperature stable water swellable rubber composition</title><author>CHOI SOO-BUM ; JUSTICE LAWRENCE J</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104246115A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2014</creationdate><topic>EARTH DRILLING</topic><topic>EARTH DRILLING, e.g. DEEP DRILLING</topic><topic>FIXED CONSTRUCTIONS</topic><topic>MINING</topic><topic>OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</topic><toplevel>online_resources</toplevel><creatorcontrib>CHOI SOO-BUM</creatorcontrib><creatorcontrib>JUSTICE LAWRENCE J</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHOI SOO-BUM</au><au>JUSTICE LAWRENCE J</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High temperature stable water swellable rubber composition</title><date>2014-12-24</date><risdate>2014</risdate><abstract>A water swellable rubber composition comprising (a) a non-water swellable base rubber, (b) an ethylene oxide based hydrophilic elastomer having from zero up to and including 20 mole % of a crosslinkable curable functional group, and (c) a water swellable non-elastomeric material. The composition has excellent water swell characteristics under prolonged exposure to high temperature and various electrolyte solutions (strongly saline as well as acid conditions) and is particularly suitable for oil field applications. When the ethylene oxide based hydrophilic elastomer (b) has from zero to less than 5 mole % of crosslinkable functional group, the amount of (b) is between about 30 parts and 300 parts by weight based on 100 parts by weight of the base rubber (a) and the amount of (c) is between about 20 parts and 200 parts by weight based on 100 parts by weight of the base rubber (a), the composition is characterized by good shape retention after undergoing constrained swell, as well as a high degree of constrained</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN104246115A
source esp@cenet
subjects EARTH DRILLING
EARTH DRILLING, e.g. DEEP DRILLING
FIXED CONSTRUCTIONS
MINING
OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS
title High temperature stable water swellable rubber composition
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T06%3A15%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHOI%20SOO-BUM&rft.date=2014-12-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104246115A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true