Preparation method of dephosphorizing modified gravel adsorbent
The invention belongs to the technical field of sewage treatment and particularly relates to a preparation method of a dephosphorizing modified iron gravel adsorbent. The method comprises the following steps: firstly washing gravels with water and drying the gravels at the temperature of 80-90 DEG C...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LU YING LI HAOJUN GUO JIAHUA GAO JUNQI LI JIHUA WU JIANGTAO ZHENG ZHENG HUANG WEI ZHANG LIANGJIE LUO XINGZHANG |
description | The invention belongs to the technical field of sewage treatment and particularly relates to a preparation method of a dephosphorizing modified iron gravel adsorbent. The method comprises the following steps: firstly washing gravels with water and drying the gravels at the temperature of 80-90 DEG C; grinding the gravels into powder by a grinder; mixing gravel powder with an inorganic iron salt solution to obtain a mixture, oscillating the mixture at constant temperature, filtering the mixture, and performing drying, thereby obtaining the high-efficiency dephosphorizing modified iron gravel adsorbent rich in iron oxides. Compared with the prior art, the method has the advantages of moderate preparation conditions, strong operability, and high efficiency of treatment on phosphorus wastewater, and is simple, easy to implement and capable of lowering the purification cost. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104190351A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104190351A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104190351A3</originalsourceid><addsrcrecordid>eNrjZLAPKEotSCxKLMnMz1PITS3JyE9RyE9TSEktyMgvBuKizKrMvHSF3PyUzLTM1BSF9KLEstQchcSU4vyipNS8Eh4G1rTEnOJUXijNzaDo5hri7KGbWpAfn1pckJicmpdaEu_sZ2hgYmhpYGxq6GhMjBoA5e0xkg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of dephosphorizing modified gravel adsorbent</title><source>esp@cenet</source><creator>LU YING ; LI HAOJUN ; GUO JIAHUA ; GAO JUNQI ; LI JIHUA ; WU JIANGTAO ; ZHENG ZHENG ; HUANG WEI ; ZHANG LIANGJIE ; LUO XINGZHANG</creator><creatorcontrib>LU YING ; LI HAOJUN ; GUO JIAHUA ; GAO JUNQI ; LI JIHUA ; WU JIANGTAO ; ZHENG ZHENG ; HUANG WEI ; ZHANG LIANGJIE ; LUO XINGZHANG</creatorcontrib><description>The invention belongs to the technical field of sewage treatment and particularly relates to a preparation method of a dephosphorizing modified iron gravel adsorbent. The method comprises the following steps: firstly washing gravels with water and drying the gravels at the temperature of 80-90 DEG C; grinding the gravels into powder by a grinder; mixing gravel powder with an inorganic iron salt solution to obtain a mixture, oscillating the mixture at constant temperature, filtering the mixture, and performing drying, thereby obtaining the high-efficiency dephosphorizing modified iron gravel adsorbent rich in iron oxides. Compared with the prior art, the method has the advantages of moderate preparation conditions, strong operability, and high efficiency of treatment on phosphorus wastewater, and is simple, easy to implement and capable of lowering the purification cost.</description><language>chi ; eng</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20141210&DB=EPODOC&CC=CN&NR=104190351A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20141210&DB=EPODOC&CC=CN&NR=104190351A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LU YING</creatorcontrib><creatorcontrib>LI HAOJUN</creatorcontrib><creatorcontrib>GUO JIAHUA</creatorcontrib><creatorcontrib>GAO JUNQI</creatorcontrib><creatorcontrib>LI JIHUA</creatorcontrib><creatorcontrib>WU JIANGTAO</creatorcontrib><creatorcontrib>ZHENG ZHENG</creatorcontrib><creatorcontrib>HUANG WEI</creatorcontrib><creatorcontrib>ZHANG LIANGJIE</creatorcontrib><creatorcontrib>LUO XINGZHANG</creatorcontrib><title>Preparation method of dephosphorizing modified gravel adsorbent</title><description>The invention belongs to the technical field of sewage treatment and particularly relates to a preparation method of a dephosphorizing modified iron gravel adsorbent. The method comprises the following steps: firstly washing gravels with water and drying the gravels at the temperature of 80-90 DEG C; grinding the gravels into powder by a grinder; mixing gravel powder with an inorganic iron salt solution to obtain a mixture, oscillating the mixture at constant temperature, filtering the mixture, and performing drying, thereby obtaining the high-efficiency dephosphorizing modified iron gravel adsorbent rich in iron oxides. Compared with the prior art, the method has the advantages of moderate preparation conditions, strong operability, and high efficiency of treatment on phosphorus wastewater, and is simple, easy to implement and capable of lowering the purification cost.</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAPKEotSCxKLMnMz1PITS3JyE9RyE9TSEktyMgvBuKizKrMvHSF3PyUzLTM1BSF9KLEstQchcSU4vyipNS8Eh4G1rTEnOJUXijNzaDo5hri7KGbWpAfn1pckJicmpdaEu_sZ2hgYmhpYGxq6GhMjBoA5e0xkg</recordid><startdate>20141210</startdate><enddate>20141210</enddate><creator>LU YING</creator><creator>LI HAOJUN</creator><creator>GUO JIAHUA</creator><creator>GAO JUNQI</creator><creator>LI JIHUA</creator><creator>WU JIANGTAO</creator><creator>ZHENG ZHENG</creator><creator>HUANG WEI</creator><creator>ZHANG LIANGJIE</creator><creator>LUO XINGZHANG</creator><scope>EVB</scope></search><sort><creationdate>20141210</creationdate><title>Preparation method of dephosphorizing modified gravel adsorbent</title><author>LU YING ; LI HAOJUN ; GUO JIAHUA ; GAO JUNQI ; LI JIHUA ; WU JIANGTAO ; ZHENG ZHENG ; HUANG WEI ; ZHANG LIANGJIE ; LUO XINGZHANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104190351A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2014</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>LU YING</creatorcontrib><creatorcontrib>LI HAOJUN</creatorcontrib><creatorcontrib>GUO JIAHUA</creatorcontrib><creatorcontrib>GAO JUNQI</creatorcontrib><creatorcontrib>LI JIHUA</creatorcontrib><creatorcontrib>WU JIANGTAO</creatorcontrib><creatorcontrib>ZHENG ZHENG</creatorcontrib><creatorcontrib>HUANG WEI</creatorcontrib><creatorcontrib>ZHANG LIANGJIE</creatorcontrib><creatorcontrib>LUO XINGZHANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LU YING</au><au>LI HAOJUN</au><au>GUO JIAHUA</au><au>GAO JUNQI</au><au>LI JIHUA</au><au>WU JIANGTAO</au><au>ZHENG ZHENG</au><au>HUANG WEI</au><au>ZHANG LIANGJIE</au><au>LUO XINGZHANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of dephosphorizing modified gravel adsorbent</title><date>2014-12-10</date><risdate>2014</risdate><abstract>The invention belongs to the technical field of sewage treatment and particularly relates to a preparation method of a dephosphorizing modified iron gravel adsorbent. The method comprises the following steps: firstly washing gravels with water and drying the gravels at the temperature of 80-90 DEG C; grinding the gravels into powder by a grinder; mixing gravel powder with an inorganic iron salt solution to obtain a mixture, oscillating the mixture at constant temperature, filtering the mixture, and performing drying, thereby obtaining the high-efficiency dephosphorizing modified iron gravel adsorbent rich in iron oxides. Compared with the prior art, the method has the advantages of moderate preparation conditions, strong operability, and high efficiency of treatment on phosphorus wastewater, and is simple, easy to implement and capable of lowering the purification cost.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN104190351A |
source | esp@cenet |
subjects | CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY CHEMISTRY METALLURGY PERFORMING OPERATIONS PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL THEIR RELEVANT APPARATUS TRANSPORTING TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE |
title | Preparation method of dephosphorizing modified gravel adsorbent |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-23T13%3A32%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LU%20YING&rft.date=2014-12-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104190351A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |