Preparation method of rare earth-doped hydrated manganese oxide adsorbent

The invention discloses a preparation method of a rare earth-doped hydrated manganese oxide adsorbent. The preparation method comprises the following steps: firstly preparing a mixed liquid I from a MnSO4.H2O solution with the molar concentration of 2%-5% and a NaCl solution with the molar concentra...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHAO LI'NAN, YANG XIAOSONG, CHEN GUOQIANG, ZHAO SHAOKANG, LIU FENGBIAO, ZHENG XI, LIU YANLI, HU JIANLONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SHAO LI'NAN
YANG XIAOSONG
CHEN GUOQIANG
ZHAO SHAOKANG
LIU FENGBIAO
ZHENG XI
LIU YANLI
HU JIANLONG
description The invention discloses a preparation method of a rare earth-doped hydrated manganese oxide adsorbent. The preparation method comprises the following steps: firstly preparing a mixed liquid I from a MnSO4.H2O solution with the molar concentration of 2%-5% and a NaCl solution with the molar concentration of 2%-10%, and adding a 0.1%-0.5% KMnO4 solution into the mixed liquid I so as to prepare a hydrated manganese dioxide seed crystal mixed liquid; carrying out rare earth-doped crystal particle amplification on the hydrated manganese dioxide seed crystal mixed liquid; carrying out precipitate size grading on a rare earth-doped hydrated manganese oxide mixed liquid, and carrying out filter pressing on precipitates with particle sizes larger than 10 microns so as to obtain adsorbent filter cake; drying the adsorbent filter cake at 50-75 DEG C for 1.5-3 hours until no obvious moisture is left on the surface of the adsorbent filter cake, thereby obtaining the finished adsorbent. The adsorbent is high in adsorption
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104162404A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104162404A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104162404A3</originalsourceid><addsrcrecordid>eNqNyjEOwjAMRuEsDAi4gzlApRYidlSBYEEM7JXBf0klGkdOBrg9HTgA03vDN3fnqyGxcRk00ogSVEh7MjYQ2EqoRBOEwkcmNM3I8ckRGaTvQUAsWe2OWJZu1vMrY_Xrwq2Ph1t7qpC0Q078QETp2ktT-2a38bXfb_8xX_beNM0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of rare earth-doped hydrated manganese oxide adsorbent</title><source>esp@cenet</source><creator>SHAO LI'NAN ; YANG XIAOSONG ; CHEN GUOQIANG ; ZHAO SHAOKANG ; LIU FENGBIAO ; ZHENG XI ; LIU YANLI ; HU JIANLONG</creator><creatorcontrib>SHAO LI'NAN ; YANG XIAOSONG ; CHEN GUOQIANG ; ZHAO SHAOKANG ; LIU FENGBIAO ; ZHENG XI ; LIU YANLI ; HU JIANLONG</creatorcontrib><description>The invention discloses a preparation method of a rare earth-doped hydrated manganese oxide adsorbent. The preparation method comprises the following steps: firstly preparing a mixed liquid I from a MnSO4.H2O solution with the molar concentration of 2%-5% and a NaCl solution with the molar concentration of 2%-10%, and adding a 0.1%-0.5% KMnO4 solution into the mixed liquid I so as to prepare a hydrated manganese dioxide seed crystal mixed liquid; carrying out rare earth-doped crystal particle amplification on the hydrated manganese dioxide seed crystal mixed liquid; carrying out precipitate size grading on a rare earth-doped hydrated manganese oxide mixed liquid, and carrying out filter pressing on precipitates with particle sizes larger than 10 microns so as to obtain adsorbent filter cake; drying the adsorbent filter cake at 50-75 DEG C for 1.5-3 hours until no obvious moisture is left on the surface of the adsorbent filter cake, thereby obtaining the finished adsorbent. The adsorbent is high in adsorption</description><language>chi ; eng</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20141126&amp;DB=EPODOC&amp;CC=CN&amp;NR=104162404A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20141126&amp;DB=EPODOC&amp;CC=CN&amp;NR=104162404A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHAO LI'NAN</creatorcontrib><creatorcontrib>YANG XIAOSONG</creatorcontrib><creatorcontrib>CHEN GUOQIANG</creatorcontrib><creatorcontrib>ZHAO SHAOKANG</creatorcontrib><creatorcontrib>LIU FENGBIAO</creatorcontrib><creatorcontrib>ZHENG XI</creatorcontrib><creatorcontrib>LIU YANLI</creatorcontrib><creatorcontrib>HU JIANLONG</creatorcontrib><title>Preparation method of rare earth-doped hydrated manganese oxide adsorbent</title><description>The invention discloses a preparation method of a rare earth-doped hydrated manganese oxide adsorbent. The preparation method comprises the following steps: firstly preparing a mixed liquid I from a MnSO4.H2O solution with the molar concentration of 2%-5% and a NaCl solution with the molar concentration of 2%-10%, and adding a 0.1%-0.5% KMnO4 solution into the mixed liquid I so as to prepare a hydrated manganese dioxide seed crystal mixed liquid; carrying out rare earth-doped crystal particle amplification on the hydrated manganese dioxide seed crystal mixed liquid; carrying out precipitate size grading on a rare earth-doped hydrated manganese oxide mixed liquid, and carrying out filter pressing on precipitates with particle sizes larger than 10 microns so as to obtain adsorbent filter cake; drying the adsorbent filter cake at 50-75 DEG C for 1.5-3 hours until no obvious moisture is left on the surface of the adsorbent filter cake, thereby obtaining the finished adsorbent. The adsorbent is high in adsorption</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEOwjAMRuEsDAi4gzlApRYidlSBYEEM7JXBf0klGkdOBrg9HTgA03vDN3fnqyGxcRk00ogSVEh7MjYQ2EqoRBOEwkcmNM3I8ckRGaTvQUAsWe2OWJZu1vMrY_Xrwq2Ph1t7qpC0Q078QETp2ktT-2a38bXfb_8xX_beNM0</recordid><startdate>20141126</startdate><enddate>20141126</enddate><creator>SHAO LI'NAN</creator><creator>YANG XIAOSONG</creator><creator>CHEN GUOQIANG</creator><creator>ZHAO SHAOKANG</creator><creator>LIU FENGBIAO</creator><creator>ZHENG XI</creator><creator>LIU YANLI</creator><creator>HU JIANLONG</creator><scope>EVB</scope></search><sort><creationdate>20141126</creationdate><title>Preparation method of rare earth-doped hydrated manganese oxide adsorbent</title><author>SHAO LI'NAN ; YANG XIAOSONG ; CHEN GUOQIANG ; ZHAO SHAOKANG ; LIU FENGBIAO ; ZHENG XI ; LIU YANLI ; HU JIANLONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104162404A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2014</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>SHAO LI'NAN</creatorcontrib><creatorcontrib>YANG XIAOSONG</creatorcontrib><creatorcontrib>CHEN GUOQIANG</creatorcontrib><creatorcontrib>ZHAO SHAOKANG</creatorcontrib><creatorcontrib>LIU FENGBIAO</creatorcontrib><creatorcontrib>ZHENG XI</creatorcontrib><creatorcontrib>LIU YANLI</creatorcontrib><creatorcontrib>HU JIANLONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHAO LI'NAN</au><au>YANG XIAOSONG</au><au>CHEN GUOQIANG</au><au>ZHAO SHAOKANG</au><au>LIU FENGBIAO</au><au>ZHENG XI</au><au>LIU YANLI</au><au>HU JIANLONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of rare earth-doped hydrated manganese oxide adsorbent</title><date>2014-11-26</date><risdate>2014</risdate><abstract>The invention discloses a preparation method of a rare earth-doped hydrated manganese oxide adsorbent. The preparation method comprises the following steps: firstly preparing a mixed liquid I from a MnSO4.H2O solution with the molar concentration of 2%-5% and a NaCl solution with the molar concentration of 2%-10%, and adding a 0.1%-0.5% KMnO4 solution into the mixed liquid I so as to prepare a hydrated manganese dioxide seed crystal mixed liquid; carrying out rare earth-doped crystal particle amplification on the hydrated manganese dioxide seed crystal mixed liquid; carrying out precipitate size grading on a rare earth-doped hydrated manganese oxide mixed liquid, and carrying out filter pressing on precipitates with particle sizes larger than 10 microns so as to obtain adsorbent filter cake; drying the adsorbent filter cake at 50-75 DEG C for 1.5-3 hours until no obvious moisture is left on the surface of the adsorbent filter cake, thereby obtaining the finished adsorbent. The adsorbent is high in adsorption</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN104162404A
source esp@cenet
subjects CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
THEIR RELEVANT APPARATUS
TRANSPORTING
TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE
title Preparation method of rare earth-doped hydrated manganese oxide adsorbent
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T16%3A51%3A25IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHAO%20LI'NAN&rft.date=2014-11-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104162404A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true