Preparation method of polydopamine-based modified composite polymer diaphragm
The invention relates to a polydopamine-based modified composite polymer diaphragm which is characterized in that a preparation method specifically comprises the following steps: (a) soaking nonwoven fabric with the size of 10cm*15cm in 10mmol/L dopamine solution for 24h to obtain polydopamine-pretr...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YU LI'NA ZHANG KEJIN CAO TINGTING RONG CHANGRU WANG DAN ZHAO ZHONGLING DIAO HONGJUN MA QIANLI |
description | The invention relates to a polydopamine-based modified composite polymer diaphragm which is characterized in that a preparation method specifically comprises the following steps: (a) soaking nonwoven fabric with the size of 10cm*15cm in 10mmol/L dopamine solution for 24h to obtain polydopamine-pretreated nonwoven fabric; (b) meanwhile, treating the polydopamine-pretreated nonwoven fabric with a mixed system containing water, polymer particles and a water-based binder to obtain a diaphragm, wherein the ratio of the water-based binder to the water to the polymer particles is (0.5-5g):50g:(0.1-0.5g); and (c) performing vacuum drying on the diaphragm at 70-85 DEG C to obtain a polydopamine-based modified composite polymer particle diaphragm. Aiming at the shortcomings of an existing diaphragm, after the nonwoven fabric is treated by dopamine, the diaphragm surface is in a hydrophilic state from a hydrophobic state, and the adopted water-based binder is environmentally-friendly; the added polymer particles can imp |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104051691A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104051691A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104051691A3</originalsourceid><addsrcrecordid>eNrjZPANKEotSCxKLMnMz1PITS3JyE9RyE9TKMjPqUzJL0jMzcxL1U1KLE5NUcjNT8lMywQykvNzC_KLM0tSwapyU4sUUjITCzKKEtNzeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGJgamhmaWhozExagA6Szbr</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of polydopamine-based modified composite polymer diaphragm</title><source>esp@cenet</source><creator>YU LI'NA ; ZHANG KEJIN ; CAO TINGTING ; RONG CHANGRU ; WANG DAN ; ZHAO ZHONGLING ; DIAO HONGJUN ; MA QIANLI</creator><creatorcontrib>YU LI'NA ; ZHANG KEJIN ; CAO TINGTING ; RONG CHANGRU ; WANG DAN ; ZHAO ZHONGLING ; DIAO HONGJUN ; MA QIANLI</creatorcontrib><description>The invention relates to a polydopamine-based modified composite polymer diaphragm which is characterized in that a preparation method specifically comprises the following steps: (a) soaking nonwoven fabric with the size of 10cm*15cm in 10mmol/L dopamine solution for 24h to obtain polydopamine-pretreated nonwoven fabric; (b) meanwhile, treating the polydopamine-pretreated nonwoven fabric with a mixed system containing water, polymer particles and a water-based binder to obtain a diaphragm, wherein the ratio of the water-based binder to the water to the polymer particles is (0.5-5g):50g:(0.1-0.5g); and (c) performing vacuum drying on the diaphragm at 70-85 DEG C to obtain a polydopamine-based modified composite polymer particle diaphragm. Aiming at the shortcomings of an existing diaphragm, after the nonwoven fabric is treated by dopamine, the diaphragm surface is in a hydrophilic state from a hydrophobic state, and the adopted water-based binder is environmentally-friendly; the added polymer particles can imp</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140917&DB=EPODOC&CC=CN&NR=104051691A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140917&DB=EPODOC&CC=CN&NR=104051691A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YU LI'NA</creatorcontrib><creatorcontrib>ZHANG KEJIN</creatorcontrib><creatorcontrib>CAO TINGTING</creatorcontrib><creatorcontrib>RONG CHANGRU</creatorcontrib><creatorcontrib>WANG DAN</creatorcontrib><creatorcontrib>ZHAO ZHONGLING</creatorcontrib><creatorcontrib>DIAO HONGJUN</creatorcontrib><creatorcontrib>MA QIANLI</creatorcontrib><title>Preparation method of polydopamine-based modified composite polymer diaphragm</title><description>The invention relates to a polydopamine-based modified composite polymer diaphragm which is characterized in that a preparation method specifically comprises the following steps: (a) soaking nonwoven fabric with the size of 10cm*15cm in 10mmol/L dopamine solution for 24h to obtain polydopamine-pretreated nonwoven fabric; (b) meanwhile, treating the polydopamine-pretreated nonwoven fabric with a mixed system containing water, polymer particles and a water-based binder to obtain a diaphragm, wherein the ratio of the water-based binder to the water to the polymer particles is (0.5-5g):50g:(0.1-0.5g); and (c) performing vacuum drying on the diaphragm at 70-85 DEG C to obtain a polydopamine-based modified composite polymer particle diaphragm. Aiming at the shortcomings of an existing diaphragm, after the nonwoven fabric is treated by dopamine, the diaphragm surface is in a hydrophilic state from a hydrophobic state, and the adopted water-based binder is environmentally-friendly; the added polymer particles can imp</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPANKEotSCxKLMnMz1PITS3JyE9RyE9TKMjPqUzJL0jMzcxL1U1KLE5NUcjNT8lMywQykvNzC_KLM0tSwapyU4sUUjITCzKKEtNzeRhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoYGJgamhmaWhozExagA6Szbr</recordid><startdate>20140917</startdate><enddate>20140917</enddate><creator>YU LI'NA</creator><creator>ZHANG KEJIN</creator><creator>CAO TINGTING</creator><creator>RONG CHANGRU</creator><creator>WANG DAN</creator><creator>ZHAO ZHONGLING</creator><creator>DIAO HONGJUN</creator><creator>MA QIANLI</creator><scope>EVB</scope></search><sort><creationdate>20140917</creationdate><title>Preparation method of polydopamine-based modified composite polymer diaphragm</title><author>YU LI'NA ; ZHANG KEJIN ; CAO TINGTING ; RONG CHANGRU ; WANG DAN ; ZHAO ZHONGLING ; DIAO HONGJUN ; MA QIANLI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104051691A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2014</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>YU LI'NA</creatorcontrib><creatorcontrib>ZHANG KEJIN</creatorcontrib><creatorcontrib>CAO TINGTING</creatorcontrib><creatorcontrib>RONG CHANGRU</creatorcontrib><creatorcontrib>WANG DAN</creatorcontrib><creatorcontrib>ZHAO ZHONGLING</creatorcontrib><creatorcontrib>DIAO HONGJUN</creatorcontrib><creatorcontrib>MA QIANLI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YU LI'NA</au><au>ZHANG KEJIN</au><au>CAO TINGTING</au><au>RONG CHANGRU</au><au>WANG DAN</au><au>ZHAO ZHONGLING</au><au>DIAO HONGJUN</au><au>MA QIANLI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of polydopamine-based modified composite polymer diaphragm</title><date>2014-09-17</date><risdate>2014</risdate><abstract>The invention relates to a polydopamine-based modified composite polymer diaphragm which is characterized in that a preparation method specifically comprises the following steps: (a) soaking nonwoven fabric with the size of 10cm*15cm in 10mmol/L dopamine solution for 24h to obtain polydopamine-pretreated nonwoven fabric; (b) meanwhile, treating the polydopamine-pretreated nonwoven fabric with a mixed system containing water, polymer particles and a water-based binder to obtain a diaphragm, wherein the ratio of the water-based binder to the water to the polymer particles is (0.5-5g):50g:(0.1-0.5g); and (c) performing vacuum drying on the diaphragm at 70-85 DEG C to obtain a polydopamine-based modified composite polymer particle diaphragm. Aiming at the shortcomings of an existing diaphragm, after the nonwoven fabric is treated by dopamine, the diaphragm surface is in a hydrophilic state from a hydrophobic state, and the adopted water-based binder is environmentally-friendly; the added polymer particles can imp</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN104051691A |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS ELECTRICITY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
title | Preparation method of polydopamine-based modified composite polymer diaphragm |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T04%3A26%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YU%20LI'NA&rft.date=2014-09-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104051691A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |