Modified nylon material and preparing method of modified nylon material
The invention discloses a modified nylon material and a preparing method of the modified nylon material. The modified nylon material comprises the following ingredients in percentage by weight: 45 percent to 55 percent of PA66, 10 percent to 15 percent of red phosphorus flame retardants, 22 percent...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | MU YUN YANG AWEI YANG XIANFU |
description | The invention discloses a modified nylon material and a preparing method of the modified nylon material. The modified nylon material comprises the following ingredients in percentage by weight: 45 percent to 55 percent of PA66, 10 percent to 15 percent of red phosphorus flame retardants, 22 percent to 30 percent of glass fiber, 5 percent to 8 percent of anti-freezing agents, 1 percent to 4.5 percent of mica powder and 0.5 percent to 1.5 percent of assisting agents. The preparing method of the modified nylon material comprises the following steps that: the PA66, the red phosphorus flame retardants, the mica powder and the assisting agents are weighed according to the weight ratio and are mixed; then, the mixture is added into a high-speed stirring pot to be stirred for 3 to 5 minutes at a high speed and is then added into a double-screw extruder; the glass fiber is added from an inlet of the extruder; the temperature is regulated to a specified value; and finally, discharging, water cooling, grain cutting and |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN104004352A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN104004352A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN104004352A3</originalsourceid><addsrcrecordid>eNrjZHD3zU_JTMtMTVHIq8zJz1PITSxJLcpMzFFIzEtRKChKLUgsysxLV8hNLcnIT1HIT1PIxa6eh4E1LTGnOJUXSnMzKLq5hjh76KYW5MenFhckJqfmpZbEO_sZGpgYGJgYmxo5GhOjBgBtPDPl</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Modified nylon material and preparing method of modified nylon material</title><source>esp@cenet</source><creator>MU YUN ; YANG AWEI ; YANG XIANFU</creator><creatorcontrib>MU YUN ; YANG AWEI ; YANG XIANFU</creatorcontrib><description>The invention discloses a modified nylon material and a preparing method of the modified nylon material. The modified nylon material comprises the following ingredients in percentage by weight: 45 percent to 55 percent of PA66, 10 percent to 15 percent of red phosphorus flame retardants, 22 percent to 30 percent of glass fiber, 5 percent to 8 percent of anti-freezing agents, 1 percent to 4.5 percent of mica powder and 0.5 percent to 1.5 percent of assisting agents. The preparing method of the modified nylon material comprises the following steps that: the PA66, the red phosphorus flame retardants, the mica powder and the assisting agents are weighed according to the weight ratio and are mixed; then, the mixture is added into a high-speed stirring pot to be stirred for 3 to 5 minutes at a high speed and is then added into a double-screw extruder; the glass fiber is added from an inlet of the extruder; the temperature is regulated to a specified value; and finally, discharging, water cooling, grain cutting and</description><language>chi ; eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; MAKING GRANULES OR PREFORMS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED ; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140827&DB=EPODOC&CC=CN&NR=104004352A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140827&DB=EPODOC&CC=CN&NR=104004352A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MU YUN</creatorcontrib><creatorcontrib>YANG AWEI</creatorcontrib><creatorcontrib>YANG XIANFU</creatorcontrib><title>Modified nylon material and preparing method of modified nylon material</title><description>The invention discloses a modified nylon material and a preparing method of the modified nylon material. The modified nylon material comprises the following ingredients in percentage by weight: 45 percent to 55 percent of PA66, 10 percent to 15 percent of red phosphorus flame retardants, 22 percent to 30 percent of glass fiber, 5 percent to 8 percent of anti-freezing agents, 1 percent to 4.5 percent of mica powder and 0.5 percent to 1.5 percent of assisting agents. The preparing method of the modified nylon material comprises the following steps that: the PA66, the red phosphorus flame retardants, the mica powder and the assisting agents are weighed according to the weight ratio and are mixed; then, the mixture is added into a high-speed stirring pot to be stirred for 3 to 5 minutes at a high speed and is then added into a double-screw extruder; the glass fiber is added from an inlet of the extruder; the temperature is regulated to a specified value; and finally, discharging, water cooling, grain cutting and</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>MAKING GRANULES OR PREFORMS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</subject><subject>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD3zU_JTMtMTVHIq8zJz1PITSxJLcpMzFFIzEtRKChKLUgsysxLV8hNLcnIT1HIT1PIxa6eh4E1LTGnOJUXSnMzKLq5hjh76KYW5MenFhckJqfmpZbEO_sZGpgYGJgYmxo5GhOjBgBtPDPl</recordid><startdate>20140827</startdate><enddate>20140827</enddate><creator>MU YUN</creator><creator>YANG AWEI</creator><creator>YANG XIANFU</creator><scope>EVB</scope></search><sort><creationdate>20140827</creationdate><title>Modified nylon material and preparing method of modified nylon material</title><author>MU YUN ; YANG AWEI ; YANG XIANFU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN104004352A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2014</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>MAKING GRANULES OR PREFORMS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</topic><topic>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>MU YUN</creatorcontrib><creatorcontrib>YANG AWEI</creatorcontrib><creatorcontrib>YANG XIANFU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MU YUN</au><au>YANG AWEI</au><au>YANG XIANFU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Modified nylon material and preparing method of modified nylon material</title><date>2014-08-27</date><risdate>2014</risdate><abstract>The invention discloses a modified nylon material and a preparing method of the modified nylon material. The modified nylon material comprises the following ingredients in percentage by weight: 45 percent to 55 percent of PA66, 10 percent to 15 percent of red phosphorus flame retardants, 22 percent to 30 percent of glass fiber, 5 percent to 8 percent of anti-freezing agents, 1 percent to 4.5 percent of mica powder and 0.5 percent to 1.5 percent of assisting agents. The preparing method of the modified nylon material comprises the following steps that: the PA66, the red phosphorus flame retardants, the mica powder and the assisting agents are weighed according to the weight ratio and are mixed; then, the mixture is added into a high-speed stirring pot to be stirred for 3 to 5 minutes at a high speed and is then added into a double-screw extruder; the glass fiber is added from an inlet of the extruder; the temperature is regulated to a specified value; and finally, discharging, water cooling, grain cutting and</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN104004352A |
source | esp@cenet |
subjects | AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING CHEMISTRY COMPOSITIONS BASED THEREON COMPOSITIONS OF MACROMOLECULAR COMPOUNDS MAKING GRANULES OR PREFORMS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS PERFORMING OPERATIONS PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR SHAPING OR JOINING OF PLASTICS THEIR PREPARATION OR CHEMICAL WORKING-UP TRANSPORTING USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL |
title | Modified nylon material and preparing method of modified nylon material |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-10T02%3A53%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MU%20YUN&rft.date=2014-08-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN104004352A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |