Cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process
The invention discloses a cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process, which comprises the following steps: 1) sequentially adding 2-3 parts by mass of ethyl acetate, 35-70 parts by mass of deionized water, 80-85 parts by mass of neutral cellulase, 2-4 parts by...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | WANG ZHENGQIU |
description | The invention discloses a cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process, which comprises the following steps: 1) sequentially adding 2-3 parts by mass of ethyl acetate, 35-70 parts by mass of deionized water, 80-85 parts by mass of neutral cellulase, 2-4 parts by mass of a deoxidization enzyme, 30-35 parts by mass of alkyl polyoxyethylene ether, 10-15 parts by mass of sucrose and 15-20 parts by mass of sodium chloride into a reaction kettle for mixing at room temperature, stirring for 55 minutes for preparing a knitted fabric-used enzyme additive; 2) pretreating a gray fabric, then washing in 75 DEG C warm water for 25 minutes, then using nitric acid to adjust the pH to neutral, then adding 2g / L of the cotton knitted fabric-used enzyme additive, running at 65 DEG C for 20-25 minutes, dyeing, then washing with water, washing with soap, dehydrating, and drying to obtain a finished product. According to the cotton knitted fabric deoxygenation polishing dyeing-enzyme bath tr |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN103741492A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN103741492A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN103741492A3</originalsourceid><addsrcrecordid>eNqNyrEOgjAURuEuDkZ9h-sDkIiQGEbTaJwcjDsp7Q80wm1D7yA-vQw-gNM3nLNWDx1EAtOLvQgctaaZvCWH8J47sBG_xBgGn3rPHbkZCxn4M4-gxkhPMsHICBaKU7BIaatWrRkSdj83an-9PPUtQww1UjQWDKn1PT8UpzIvq-O5-Of5ApPkOQo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process</title><source>esp@cenet</source><creator>WANG ZHENGQIU</creator><creatorcontrib>WANG ZHENGQIU</creatorcontrib><description>The invention discloses a cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process, which comprises the following steps: 1) sequentially adding 2-3 parts by mass of ethyl acetate, 35-70 parts by mass of deionized water, 80-85 parts by mass of neutral cellulase, 2-4 parts by mass of a deoxidization enzyme, 30-35 parts by mass of alkyl polyoxyethylene ether, 10-15 parts by mass of sucrose and 15-20 parts by mass of sodium chloride into a reaction kettle for mixing at room temperature, stirring for 55 minutes for preparing a knitted fabric-used enzyme additive; 2) pretreating a gray fabric, then washing in 75 DEG C warm water for 25 minutes, then using nitric acid to adjust the pH to neutral, then adding 2g / L of the cotton knitted fabric-used enzyme additive, running at 65 DEG C for 20-25 minutes, dyeing, then washing with water, washing with soap, dehydrating, and drying to obtain a finished product. According to the cotton knitted fabric deoxygenation polishing dyeing-enzyme bath tr</description><language>chi ; eng</language><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; LAUNDERING ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE ; TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140423&DB=EPODOC&CC=CN&NR=103741492A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20140423&DB=EPODOC&CC=CN&NR=103741492A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG ZHENGQIU</creatorcontrib><title>Cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process</title><description>The invention discloses a cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process, which comprises the following steps: 1) sequentially adding 2-3 parts by mass of ethyl acetate, 35-70 parts by mass of deionized water, 80-85 parts by mass of neutral cellulase, 2-4 parts by mass of a deoxidization enzyme, 30-35 parts by mass of alkyl polyoxyethylene ether, 10-15 parts by mass of sucrose and 15-20 parts by mass of sodium chloride into a reaction kettle for mixing at room temperature, stirring for 55 minutes for preparing a knitted fabric-used enzyme additive; 2) pretreating a gray fabric, then washing in 75 DEG C warm water for 25 minutes, then using nitric acid to adjust the pH to neutral, then adding 2g / L of the cotton knitted fabric-used enzyme additive, running at 65 DEG C for 20-25 minutes, dyeing, then washing with water, washing with soap, dehydrating, and drying to obtain a finished product. According to the cotton knitted fabric deoxygenation polishing dyeing-enzyme bath tr</description><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>LAUNDERING</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><subject>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEOgjAURuEuDkZ9h-sDkIiQGEbTaJwcjDsp7Q80wm1D7yA-vQw-gNM3nLNWDx1EAtOLvQgctaaZvCWH8J47sBG_xBgGn3rPHbkZCxn4M4-gxkhPMsHICBaKU7BIaatWrRkSdj83an-9PPUtQww1UjQWDKn1PT8UpzIvq-O5-Of5ApPkOQo</recordid><startdate>20140423</startdate><enddate>20140423</enddate><creator>WANG ZHENGQIU</creator><scope>EVB</scope></search><sort><creationdate>20140423</creationdate><title>Cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process</title><author>WANG ZHENGQIU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN103741492A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2014</creationdate><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>LAUNDERING</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><topic>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG ZHENGQIU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG ZHENGQIU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process</title><date>2014-04-23</date><risdate>2014</risdate><abstract>The invention discloses a cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process, which comprises the following steps: 1) sequentially adding 2-3 parts by mass of ethyl acetate, 35-70 parts by mass of deionized water, 80-85 parts by mass of neutral cellulase, 2-4 parts by mass of a deoxidization enzyme, 30-35 parts by mass of alkyl polyoxyethylene ether, 10-15 parts by mass of sucrose and 15-20 parts by mass of sodium chloride into a reaction kettle for mixing at room temperature, stirring for 55 minutes for preparing a knitted fabric-used enzyme additive; 2) pretreating a gray fabric, then washing in 75 DEG C warm water for 25 minutes, then using nitric acid to adjust the pH to neutral, then adding 2g / L of the cotton knitted fabric-used enzyme additive, running at 65 DEG C for 20-25 minutes, dyeing, then washing with water, washing with soap, dehydrating, and drying to obtain a finished product. According to the cotton knitted fabric deoxygenation polishing dyeing-enzyme bath tr</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN103741492A |
source | esp@cenet |
subjects | FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR LAUNDERING TEXTILES TREATMENT OF TEXTILES OR THE LIKE TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS |
title | Cotton knitted fabric deoxygenation polishing dyeing-enzyme bath treatment process |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-23T19%3A57%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20ZHENGQIU&rft.date=2014-04-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN103741492A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |