Green series titanium alloy micro-arc oxidation coloring solution and preparation method thereof
The invention belongs to the field of metal coloring and dyeing in a surface treatment technology, and in particular, relates to a green series titanium alloy micro-arc oxidation coloring solution and a preparation method thereof, used for solving the defects of an electrolytic colored film. The col...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | TANG HONGCAI |
description | The invention belongs to the field of metal coloring and dyeing in a surface treatment technology, and in particular, relates to a green series titanium alloy micro-arc oxidation coloring solution and a preparation method thereof, used for solving the defects of an electrolytic colored film. The coloring solution comprises a micro-arc oxidation spark discharge introducing agent for producing micro-arc oxidation, a green micro-arc oxidation coloring agent, a green film compactness accelerant, a green micro-arc oxidation film color homogenizing agent, a green film stabilizer and a bath solution stabilizer. By using the solution for micro-arc oxidation coloring, the thickness of the film can reach 22 microns, the film is green as required when the thickness is 3 to 22 microns, and the formed film is stable in color, has the characteristics of touch resistance and abrasion resistance, is compact and does not adsorb dirt. More preferably, the film does not contain organic substances, and can tolerate ultraviolet f |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN103014813A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN103014813A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN103014813A3</originalsourceid><addsrcrecordid>eNqNyj0KwkAQhuE0FqLeYTxAICEWthL8qazs47D5YgY2O8vsBvT2gnoAqxdenmVxPxsQKMEEibJkDjJPxN7riyZxpiWbI31Kz1k0kFOvJuFBSf38ORx6iobI9hUT8qg95REGHdbFYmCfsPl1VWxPx1t7KRG1Q4rsEJC79lpXTVXv9nVzaP4xbyWBPgU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Green series titanium alloy micro-arc oxidation coloring solution and preparation method thereof</title><source>esp@cenet</source><creator>TANG HONGCAI</creator><creatorcontrib>TANG HONGCAI</creatorcontrib><description>The invention belongs to the field of metal coloring and dyeing in a surface treatment technology, and in particular, relates to a green series titanium alloy micro-arc oxidation coloring solution and a preparation method thereof, used for solving the defects of an electrolytic colored film. The coloring solution comprises a micro-arc oxidation spark discharge introducing agent for producing micro-arc oxidation, a green micro-arc oxidation coloring agent, a green film compactness accelerant, a green micro-arc oxidation film color homogenizing agent, a green film stabilizer and a bath solution stabilizer. By using the solution for micro-arc oxidation coloring, the thickness of the film can reach 22 microns, the film is green as required when the thickness is 3 to 22 microns, and the formed film is stable in color, has the characteristics of touch resistance and abrasion resistance, is compact and does not adsorb dirt. More preferably, the film does not contain organic substances, and can tolerate ultraviolet f</description><language>chi ; eng</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130403&DB=EPODOC&CC=CN&NR=103014813A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130403&DB=EPODOC&CC=CN&NR=103014813A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TANG HONGCAI</creatorcontrib><title>Green series titanium alloy micro-arc oxidation coloring solution and preparation method thereof</title><description>The invention belongs to the field of metal coloring and dyeing in a surface treatment technology, and in particular, relates to a green series titanium alloy micro-arc oxidation coloring solution and a preparation method thereof, used for solving the defects of an electrolytic colored film. The coloring solution comprises a micro-arc oxidation spark discharge introducing agent for producing micro-arc oxidation, a green micro-arc oxidation coloring agent, a green film compactness accelerant, a green micro-arc oxidation film color homogenizing agent, a green film stabilizer and a bath solution stabilizer. By using the solution for micro-arc oxidation coloring, the thickness of the film can reach 22 microns, the film is green as required when the thickness is 3 to 22 microns, and the formed film is stable in color, has the characteristics of touch resistance and abrasion resistance, is compact and does not adsorb dirt. More preferably, the film does not contain organic substances, and can tolerate ultraviolet f</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyj0KwkAQhuE0FqLeYTxAICEWthL8qazs47D5YgY2O8vsBvT2gnoAqxdenmVxPxsQKMEEibJkDjJPxN7riyZxpiWbI31Kz1k0kFOvJuFBSf38ORx6iobI9hUT8qg95REGHdbFYmCfsPl1VWxPx1t7KRG1Q4rsEJC79lpXTVXv9nVzaP4xbyWBPgU</recordid><startdate>20130403</startdate><enddate>20130403</enddate><creator>TANG HONGCAI</creator><scope>EVB</scope></search><sort><creationdate>20130403</creationdate><title>Green series titanium alloy micro-arc oxidation coloring solution and preparation method thereof</title><author>TANG HONGCAI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN103014813A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2013</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><toplevel>online_resources</toplevel><creatorcontrib>TANG HONGCAI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TANG HONGCAI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Green series titanium alloy micro-arc oxidation coloring solution and preparation method thereof</title><date>2013-04-03</date><risdate>2013</risdate><abstract>The invention belongs to the field of metal coloring and dyeing in a surface treatment technology, and in particular, relates to a green series titanium alloy micro-arc oxidation coloring solution and a preparation method thereof, used for solving the defects of an electrolytic colored film. The coloring solution comprises a micro-arc oxidation spark discharge introducing agent for producing micro-arc oxidation, a green micro-arc oxidation coloring agent, a green film compactness accelerant, a green micro-arc oxidation film color homogenizing agent, a green film stabilizer and a bath solution stabilizer. By using the solution for micro-arc oxidation coloring, the thickness of the film can reach 22 microns, the film is green as required when the thickness is 3 to 22 microns, and the formed film is stable in color, has the characteristics of touch resistance and abrasion resistance, is compact and does not adsorb dirt. More preferably, the film does not contain organic substances, and can tolerate ultraviolet f</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN103014813A |
source | esp@cenet |
subjects | APPARATUS THEREFOR CHEMISTRY ELECTROFORMING ELECTROLYTIC OR ELECTROPHORETIC PROCESSES METALLURGY PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS |
title | Green series titanium alloy micro-arc oxidation coloring solution and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T23%3A05%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TANG%20HONGCAI&rft.date=2013-04-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN103014813A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |