Medium-high voltage electronic aluminum foil corrosion pretreatment method

A medium-high voltage electronic aluminum foil corrosion pretreatment method comprises the following steps: placing an aluminum foil into pure water or aqueous solution containing ammonia water or amine at the temperature between 70 and 100 DEG C for treatment, performing proper heat treatment after...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG XIAOFEI, PENG NING, HE YEDONG, LI YINGRI, LIANG LIBO, XIONG CHUANYONG, SONG HONGZHOU, CAI XIAOYU
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANG XIAOFEI
PENG NING
HE YEDONG
LI YINGRI
LIANG LIBO
XIONG CHUANYONG
SONG HONGZHOU
CAI XIAOYU
description A medium-high voltage electronic aluminum foil corrosion pretreatment method comprises the following steps: placing an aluminum foil into pure water or aqueous solution containing ammonia water or amine at the temperature between 70 and 100 DEG C for treatment, performing proper heat treatment after treatment, and generating a hydrated oxidation film with uniformly distributed defects on the surface of the aluminum foil after treatment. During pitting corrosion, Cl is easily transmitted to the surface of the aluminum foil through water and defects in the hydrated oxidation film, so that the pitting uniformity of a high-voltage aluminum foil can be improved, the possibility of hole combination is reduced, and the specific capacitance of the aluminum foil is obviously improved on the premise of not reducing the mechanical strength and the bending performance of the aluminum foil.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102915847A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102915847A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102915847A3</originalsourceid><addsrcrecordid>eNqNyj0KAjEQBtA0FqLeYTzAgusPaimLIoJW9kvIfrsJJJmQTDy_jQewes2bq8cTg6uhsW6y9GEvegLBw0jm6AxpX4OLNdDIzpPhnLk4jpQyJENLQBQKEMvDUs1G7QtWPxdqfbu-u3uDxD1K0gYR0nevdrM9t4fT_njZ_XO-fmg17w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Medium-high voltage electronic aluminum foil corrosion pretreatment method</title><source>esp@cenet</source><creator>YANG XIAOFEI ; PENG NING ; HE YEDONG ; LI YINGRI ; LIANG LIBO ; XIONG CHUANYONG ; SONG HONGZHOU ; CAI XIAOYU</creator><creatorcontrib>YANG XIAOFEI ; PENG NING ; HE YEDONG ; LI YINGRI ; LIANG LIBO ; XIONG CHUANYONG ; SONG HONGZHOU ; CAI XIAOYU</creatorcontrib><description>A medium-high voltage electronic aluminum foil corrosion pretreatment method comprises the following steps: placing an aluminum foil into pure water or aqueous solution containing ammonia water or amine at the temperature between 70 and 100 DEG C for treatment, performing proper heat treatment after treatment, and generating a hydrated oxidation film with uniformly distributed defects on the surface of the aluminum foil after treatment. During pitting corrosion, Cl&lt;-&gt; is easily transmitted to the surface of the aluminum foil through water and defects in the hydrated oxidation film, so that the pitting uniformity of a high-voltage aluminum foil can be improved, the possibility of hole combination is reduced, and the specific capacitance of the aluminum foil is obviously improved on the premise of not reducing the mechanical strength and the bending performance of the aluminum foil.</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; CAPACITORS ; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE ; ELECTRICITY</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130206&amp;DB=EPODOC&amp;CC=CN&amp;NR=102915847A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130206&amp;DB=EPODOC&amp;CC=CN&amp;NR=102915847A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANG XIAOFEI</creatorcontrib><creatorcontrib>PENG NING</creatorcontrib><creatorcontrib>HE YEDONG</creatorcontrib><creatorcontrib>LI YINGRI</creatorcontrib><creatorcontrib>LIANG LIBO</creatorcontrib><creatorcontrib>XIONG CHUANYONG</creatorcontrib><creatorcontrib>SONG HONGZHOU</creatorcontrib><creatorcontrib>CAI XIAOYU</creatorcontrib><title>Medium-high voltage electronic aluminum foil corrosion pretreatment method</title><description>A medium-high voltage electronic aluminum foil corrosion pretreatment method comprises the following steps: placing an aluminum foil into pure water or aqueous solution containing ammonia water or amine at the temperature between 70 and 100 DEG C for treatment, performing proper heat treatment after treatment, and generating a hydrated oxidation film with uniformly distributed defects on the surface of the aluminum foil after treatment. During pitting corrosion, Cl&lt;-&gt; is easily transmitted to the surface of the aluminum foil through water and defects in the hydrated oxidation film, so that the pitting uniformity of a high-voltage aluminum foil can be improved, the possibility of hole combination is reduced, and the specific capacitance of the aluminum foil is obviously improved on the premise of not reducing the mechanical strength and the bending performance of the aluminum foil.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CAPACITORS</subject><subject>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</subject><subject>ELECTRICITY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyj0KAjEQBtA0FqLeYTzAgusPaimLIoJW9kvIfrsJJJmQTDy_jQewes2bq8cTg6uhsW6y9GEvegLBw0jm6AxpX4OLNdDIzpPhnLk4jpQyJENLQBQKEMvDUs1G7QtWPxdqfbu-u3uDxD1K0gYR0nevdrM9t4fT_njZ_XO-fmg17w</recordid><startdate>20130206</startdate><enddate>20130206</enddate><creator>YANG XIAOFEI</creator><creator>PENG NING</creator><creator>HE YEDONG</creator><creator>LI YINGRI</creator><creator>LIANG LIBO</creator><creator>XIONG CHUANYONG</creator><creator>SONG HONGZHOU</creator><creator>CAI XIAOYU</creator><scope>EVB</scope></search><sort><creationdate>20130206</creationdate><title>Medium-high voltage electronic aluminum foil corrosion pretreatment method</title><author>YANG XIAOFEI ; PENG NING ; HE YEDONG ; LI YINGRI ; LIANG LIBO ; XIONG CHUANYONG ; SONG HONGZHOU ; CAI XIAOYU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102915847A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2013</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CAPACITORS</topic><topic>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</topic><topic>ELECTRICITY</topic><toplevel>online_resources</toplevel><creatorcontrib>YANG XIAOFEI</creatorcontrib><creatorcontrib>PENG NING</creatorcontrib><creatorcontrib>HE YEDONG</creatorcontrib><creatorcontrib>LI YINGRI</creatorcontrib><creatorcontrib>LIANG LIBO</creatorcontrib><creatorcontrib>XIONG CHUANYONG</creatorcontrib><creatorcontrib>SONG HONGZHOU</creatorcontrib><creatorcontrib>CAI XIAOYU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANG XIAOFEI</au><au>PENG NING</au><au>HE YEDONG</au><au>LI YINGRI</au><au>LIANG LIBO</au><au>XIONG CHUANYONG</au><au>SONG HONGZHOU</au><au>CAI XIAOYU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Medium-high voltage electronic aluminum foil corrosion pretreatment method</title><date>2013-02-06</date><risdate>2013</risdate><abstract>A medium-high voltage electronic aluminum foil corrosion pretreatment method comprises the following steps: placing an aluminum foil into pure water or aqueous solution containing ammonia water or amine at the temperature between 70 and 100 DEG C for treatment, performing proper heat treatment after treatment, and generating a hydrated oxidation film with uniformly distributed defects on the surface of the aluminum foil after treatment. During pitting corrosion, Cl&lt;-&gt; is easily transmitted to the surface of the aluminum foil through water and defects in the hydrated oxidation film, so that the pitting uniformity of a high-voltage aluminum foil can be improved, the possibility of hole combination is reduced, and the specific capacitance of the aluminum foil is obviously improved on the premise of not reducing the mechanical strength and the bending performance of the aluminum foil.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN102915847A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CAPACITORS
CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE
ELECTRICITY
title Medium-high voltage electronic aluminum foil corrosion pretreatment method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T22%3A32%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANG%20XIAOFEI&rft.date=2013-02-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102915847A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true