In-situ uranium leaching and mining treatment method by adding O2 into CO2

The invention provides an in-situ uranium leaching and mining treatment method by adding O2 into CO2. The invention comprises the steps of (1) adding O2 into leaching solution, then injecting an underground mine-water contained layer into a liquid injection pipeline, and preparing the leaching solut...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHENG HONG, NIU YUQING, GUO ZHONGDE, YAO YIXUAN, MA LIANCHUN, YUAN YUAN, LI JIANHUA, WANG XIAODONG, YANG SHAOWU, ZHANG YONGMING, LIU NAIZHONG, ZHANG WANLIANG, LIAO WENSHENG, TAN YAHUI, DU ZHIMING, WANG YUNXIA, SU XUEBIN, CHENG ZONGFANG, SHEN HONGWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHENG HONG
NIU YUQING
GUO ZHONGDE
YAO YIXUAN
MA LIANCHUN
YUAN YUAN
LI JIANHUA
WANG XIAODONG
YANG SHAOWU
ZHANG YONGMING
LIU NAIZHONG
ZHANG WANLIANG
LIAO WENSHENG
TAN YAHUI
DU ZHIMING
WANG YUNXIA
SU XUEBIN
CHENG ZONGFANG
SHEN HONGWEI
description The invention provides an in-situ uranium leaching and mining treatment method by adding O2 into CO2. The invention comprises the steps of (1) adding O2 into leaching solution, then injecting an underground mine-water contained layer into a liquid injection pipeline, and preparing the leaching solution by adopting different oxygenation concentrations according to different underground leaching periods; (2) adding 100-300mg/L of CO2 into the leaching solution containing uranium; (3) conducting ion exchange adsorption on the leaching solution containing uranium, adopting macroporous styrene strong-base anion exchange resin, adsorbing to obtain saturated resin adsorption tail solution; and (4) washing saturated resin by adopting an eluting agent, and then analyzing uranyl carbonate ion solution to obtain Na2U2O7 sediment slurry and sediment mother liquor. According to the method, a high-temperature heating device is eliminated, so that the energy consumption and equipment investment are lowered greatly, the alka
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102900418A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102900418A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102900418A3</originalsourceid><addsrcrecordid>eNrjZPDyzNMtziwpVSgtSszLLM1VyElNTM7IzEtXSMxLUcjNzAMxS4pSE0tyU_NKFHJTSzLyUxSSKhUSU1JAUv5GCpl5JfkKzv5GPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0MDI0sDAxNDC0ZgYNQCePzOz</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>In-situ uranium leaching and mining treatment method by adding O2 into CO2</title><source>esp@cenet</source><creator>CHENG HONG ; NIU YUQING ; GUO ZHONGDE ; YAO YIXUAN ; MA LIANCHUN ; YUAN YUAN ; LI JIANHUA ; WANG XIAODONG ; YANG SHAOWU ; ZHANG YONGMING ; LIU NAIZHONG ; ZHANG WANLIANG ; LIAO WENSHENG ; TAN YAHUI ; DU ZHIMING ; WANG YUNXIA ; SU XUEBIN ; CHENG ZONGFANG ; SHEN HONGWEI</creator><creatorcontrib>CHENG HONG ; NIU YUQING ; GUO ZHONGDE ; YAO YIXUAN ; MA LIANCHUN ; YUAN YUAN ; LI JIANHUA ; WANG XIAODONG ; YANG SHAOWU ; ZHANG YONGMING ; LIU NAIZHONG ; ZHANG WANLIANG ; LIAO WENSHENG ; TAN YAHUI ; DU ZHIMING ; WANG YUNXIA ; SU XUEBIN ; CHENG ZONGFANG ; SHEN HONGWEI</creatorcontrib><description>The invention provides an in-situ uranium leaching and mining treatment method by adding O2 into CO2. The invention comprises the steps of (1) adding O2 into leaching solution, then injecting an underground mine-water contained layer into a liquid injection pipeline, and preparing the leaching solution by adopting different oxygenation concentrations according to different underground leaching periods; (2) adding 100-300mg/L of CO2 into the leaching solution containing uranium; (3) conducting ion exchange adsorption on the leaching solution containing uranium, adopting macroporous styrene strong-base anion exchange resin, adsorbing to obtain saturated resin adsorption tail solution; and (4) washing saturated resin by adopting an eluting agent, and then analyzing uranyl carbonate ion solution to obtain Na2U2O7 sediment slurry and sediment mother liquor. According to the method, a high-temperature heating device is eliminated, so that the energy consumption and equipment investment are lowered greatly, the alka</description><language>chi ; eng</language><subject>EARTH DRILLING ; EARTH DRILLING, e.g. DEEP DRILLING ; FIXED CONSTRUCTIONS ; MINING ; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130130&amp;DB=EPODOC&amp;CC=CN&amp;NR=102900418A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130130&amp;DB=EPODOC&amp;CC=CN&amp;NR=102900418A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHENG HONG</creatorcontrib><creatorcontrib>NIU YUQING</creatorcontrib><creatorcontrib>GUO ZHONGDE</creatorcontrib><creatorcontrib>YAO YIXUAN</creatorcontrib><creatorcontrib>MA LIANCHUN</creatorcontrib><creatorcontrib>YUAN YUAN</creatorcontrib><creatorcontrib>LI JIANHUA</creatorcontrib><creatorcontrib>WANG XIAODONG</creatorcontrib><creatorcontrib>YANG SHAOWU</creatorcontrib><creatorcontrib>ZHANG YONGMING</creatorcontrib><creatorcontrib>LIU NAIZHONG</creatorcontrib><creatorcontrib>ZHANG WANLIANG</creatorcontrib><creatorcontrib>LIAO WENSHENG</creatorcontrib><creatorcontrib>TAN YAHUI</creatorcontrib><creatorcontrib>DU ZHIMING</creatorcontrib><creatorcontrib>WANG YUNXIA</creatorcontrib><creatorcontrib>SU XUEBIN</creatorcontrib><creatorcontrib>CHENG ZONGFANG</creatorcontrib><creatorcontrib>SHEN HONGWEI</creatorcontrib><title>In-situ uranium leaching and mining treatment method by adding O2 into CO2</title><description>The invention provides an in-situ uranium leaching and mining treatment method by adding O2 into CO2. The invention comprises the steps of (1) adding O2 into leaching solution, then injecting an underground mine-water contained layer into a liquid injection pipeline, and preparing the leaching solution by adopting different oxygenation concentrations according to different underground leaching periods; (2) adding 100-300mg/L of CO2 into the leaching solution containing uranium; (3) conducting ion exchange adsorption on the leaching solution containing uranium, adopting macroporous styrene strong-base anion exchange resin, adsorbing to obtain saturated resin adsorption tail solution; and (4) washing saturated resin by adopting an eluting agent, and then analyzing uranyl carbonate ion solution to obtain Na2U2O7 sediment slurry and sediment mother liquor. According to the method, a high-temperature heating device is eliminated, so that the energy consumption and equipment investment are lowered greatly, the alka</description><subject>EARTH DRILLING</subject><subject>EARTH DRILLING, e.g. DEEP DRILLING</subject><subject>FIXED CONSTRUCTIONS</subject><subject>MINING</subject><subject>OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDyzNMtziwpVSgtSszLLM1VyElNTM7IzEtXSMxLUcjNzAMxS4pSE0tyU_NKFHJTSzLyUxSSKhUSU1JAUv5GCpl5JfkKzv5GPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0MDI0sDAxNDC0ZgYNQCePzOz</recordid><startdate>20130130</startdate><enddate>20130130</enddate><creator>CHENG HONG</creator><creator>NIU YUQING</creator><creator>GUO ZHONGDE</creator><creator>YAO YIXUAN</creator><creator>MA LIANCHUN</creator><creator>YUAN YUAN</creator><creator>LI JIANHUA</creator><creator>WANG XIAODONG</creator><creator>YANG SHAOWU</creator><creator>ZHANG YONGMING</creator><creator>LIU NAIZHONG</creator><creator>ZHANG WANLIANG</creator><creator>LIAO WENSHENG</creator><creator>TAN YAHUI</creator><creator>DU ZHIMING</creator><creator>WANG YUNXIA</creator><creator>SU XUEBIN</creator><creator>CHENG ZONGFANG</creator><creator>SHEN HONGWEI</creator><scope>EVB</scope></search><sort><creationdate>20130130</creationdate><title>In-situ uranium leaching and mining treatment method by adding O2 into CO2</title><author>CHENG HONG ; NIU YUQING ; GUO ZHONGDE ; YAO YIXUAN ; MA LIANCHUN ; YUAN YUAN ; LI JIANHUA ; WANG XIAODONG ; YANG SHAOWU ; ZHANG YONGMING ; LIU NAIZHONG ; ZHANG WANLIANG ; LIAO WENSHENG ; TAN YAHUI ; DU ZHIMING ; WANG YUNXIA ; SU XUEBIN ; CHENG ZONGFANG ; SHEN HONGWEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102900418A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2013</creationdate><topic>EARTH DRILLING</topic><topic>EARTH DRILLING, e.g. DEEP DRILLING</topic><topic>FIXED CONSTRUCTIONS</topic><topic>MINING</topic><topic>OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS</topic><toplevel>online_resources</toplevel><creatorcontrib>CHENG HONG</creatorcontrib><creatorcontrib>NIU YUQING</creatorcontrib><creatorcontrib>GUO ZHONGDE</creatorcontrib><creatorcontrib>YAO YIXUAN</creatorcontrib><creatorcontrib>MA LIANCHUN</creatorcontrib><creatorcontrib>YUAN YUAN</creatorcontrib><creatorcontrib>LI JIANHUA</creatorcontrib><creatorcontrib>WANG XIAODONG</creatorcontrib><creatorcontrib>YANG SHAOWU</creatorcontrib><creatorcontrib>ZHANG YONGMING</creatorcontrib><creatorcontrib>LIU NAIZHONG</creatorcontrib><creatorcontrib>ZHANG WANLIANG</creatorcontrib><creatorcontrib>LIAO WENSHENG</creatorcontrib><creatorcontrib>TAN YAHUI</creatorcontrib><creatorcontrib>DU ZHIMING</creatorcontrib><creatorcontrib>WANG YUNXIA</creatorcontrib><creatorcontrib>SU XUEBIN</creatorcontrib><creatorcontrib>CHENG ZONGFANG</creatorcontrib><creatorcontrib>SHEN HONGWEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHENG HONG</au><au>NIU YUQING</au><au>GUO ZHONGDE</au><au>YAO YIXUAN</au><au>MA LIANCHUN</au><au>YUAN YUAN</au><au>LI JIANHUA</au><au>WANG XIAODONG</au><au>YANG SHAOWU</au><au>ZHANG YONGMING</au><au>LIU NAIZHONG</au><au>ZHANG WANLIANG</au><au>LIAO WENSHENG</au><au>TAN YAHUI</au><au>DU ZHIMING</au><au>WANG YUNXIA</au><au>SU XUEBIN</au><au>CHENG ZONGFANG</au><au>SHEN HONGWEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>In-situ uranium leaching and mining treatment method by adding O2 into CO2</title><date>2013-01-30</date><risdate>2013</risdate><abstract>The invention provides an in-situ uranium leaching and mining treatment method by adding O2 into CO2. The invention comprises the steps of (1) adding O2 into leaching solution, then injecting an underground mine-water contained layer into a liquid injection pipeline, and preparing the leaching solution by adopting different oxygenation concentrations according to different underground leaching periods; (2) adding 100-300mg/L of CO2 into the leaching solution containing uranium; (3) conducting ion exchange adsorption on the leaching solution containing uranium, adopting macroporous styrene strong-base anion exchange resin, adsorbing to obtain saturated resin adsorption tail solution; and (4) washing saturated resin by adopting an eluting agent, and then analyzing uranyl carbonate ion solution to obtain Na2U2O7 sediment slurry and sediment mother liquor. According to the method, a high-temperature heating device is eliminated, so that the energy consumption and equipment investment are lowered greatly, the alka</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN102900418A
source esp@cenet
subjects EARTH DRILLING
EARTH DRILLING, e.g. DEEP DRILLING
FIXED CONSTRUCTIONS
MINING
OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR ASLURRY OF MINERALS FROM WELLS
title In-situ uranium leaching and mining treatment method by adding O2 into CO2
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T19%3A18%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHENG%20HONG&rft.date=2013-01-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102900418A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true