Method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process

The invention discloses a method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process, comprising the following steps: adding soda and additives into primary tungsten autoclaving slag, carrying out secondary autoclaving at high temperature and press...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JIANG WENWEI, ZHANG ZHANFEI, LIANG WEIDONG, LI JIANHUI, WEN BAIKAI, ZENG XINRONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator JIANG WENWEI
ZHANG ZHANFEI
LIANG WEIDONG
LI JIANHUI
WEN BAIKAI
ZENG XINRONG
description The invention discloses a method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process, comprising the following steps: adding soda and additives into primary tungsten autoclaving slag, carrying out secondary autoclaving at high temperature and pressure; separating the leaching solution from the slag; carrying out primary autoclaving to the tungsten by the leaching solution; separating the primary autoclaving slag from the crude sodium tungstate solution, wherein the primary autoclaving slag is used as the raw material; and mixing the tungstate with the secondary autoclaving leaching solution to prepare slurry. The liquid-solid ratio is controlled to be (3-5):1 in the step of adding the soda and the additives into the primary autoclaving slag and mixing to prepare the slurry, and the soda has the excess coefficient of 2.0-2.5. The liquid-solid ratio is controlled to be (3-5):1 in the step of mixing the tungstate with the secondary autoclaving leaching solution
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102747223A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102747223A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102747223A3</originalsourceid><addsrcrecordid>eNqNizEKwkAQRdNYiHqH8QABTQRrCYqNVvZh3J1kA8nMMrMBvb1GBFurz3u8P8_4QimIh0YU6JEUXeq4hTRya4kYGpXhR0PHpNjD_QmjTZ2JR0D2gF7i5xm6NuRRyWxUgp7QhUlHFfd2y2zWYG-0-u4iW5-Ot-qcU5SaLKIjplRX1-2m2O_2RVEeyn-aFxYrQys</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process</title><source>esp@cenet</source><creator>JIANG WENWEI ; ZHANG ZHANFEI ; LIANG WEIDONG ; LI JIANHUI ; WEN BAIKAI ; ZENG XINRONG</creator><creatorcontrib>JIANG WENWEI ; ZHANG ZHANFEI ; LIANG WEIDONG ; LI JIANHUI ; WEN BAIKAI ; ZENG XINRONG</creatorcontrib><description>The invention discloses a method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process, comprising the following steps: adding soda and additives into primary tungsten autoclaving slag, carrying out secondary autoclaving at high temperature and pressure; separating the leaching solution from the slag; carrying out primary autoclaving to the tungsten by the leaching solution; separating the primary autoclaving slag from the crude sodium tungstate solution, wherein the primary autoclaving slag is used as the raw material; and mixing the tungstate with the secondary autoclaving leaching solution to prepare slurry. The liquid-solid ratio is controlled to be (3-5):1 in the step of adding the soda and the additives into the primary autoclaving slag and mixing to prepare the slurry, and the soda has the excess coefficient of 2.0-2.5. The liquid-solid ratio is controlled to be (3-5):1 in the step of mixing the tungstate with the secondary autoclaving leaching solution</description><language>chi ; eng</language><subject>CHEMISTRY ; CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20121024&amp;DB=EPODOC&amp;CC=CN&amp;NR=102747223A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20121024&amp;DB=EPODOC&amp;CC=CN&amp;NR=102747223A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>JIANG WENWEI</creatorcontrib><creatorcontrib>ZHANG ZHANFEI</creatorcontrib><creatorcontrib>LIANG WEIDONG</creatorcontrib><creatorcontrib>LI JIANHUI</creatorcontrib><creatorcontrib>WEN BAIKAI</creatorcontrib><creatorcontrib>ZENG XINRONG</creatorcontrib><title>Method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process</title><description>The invention discloses a method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process, comprising the following steps: adding soda and additives into primary tungsten autoclaving slag, carrying out secondary autoclaving at high temperature and pressure; separating the leaching solution from the slag; carrying out primary autoclaving to the tungsten by the leaching solution; separating the primary autoclaving slag from the crude sodium tungstate solution, wherein the primary autoclaving slag is used as the raw material; and mixing the tungstate with the secondary autoclaving leaching solution to prepare slurry. The liquid-solid ratio is controlled to be (3-5):1 in the step of adding the soda and the additives into the primary autoclaving slag and mixing to prepare the slurry, and the soda has the excess coefficient of 2.0-2.5. The liquid-solid ratio is controlled to be (3-5):1 in the step of mixing the tungstate with the secondary autoclaving leaching solution</description><subject>CHEMISTRY</subject><subject>CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNizEKwkAQRdNYiHqH8QABTQRrCYqNVvZh3J1kA8nMMrMBvb1GBFurz3u8P8_4QimIh0YU6JEUXeq4hTRya4kYGpXhR0PHpNjD_QmjTZ2JR0D2gF7i5xm6NuRRyWxUgp7QhUlHFfd2y2zWYG-0-u4iW5-Ot-qcU5SaLKIjplRX1-2m2O_2RVEeyn-aFxYrQys</recordid><startdate>20121024</startdate><enddate>20121024</enddate><creator>JIANG WENWEI</creator><creator>ZHANG ZHANFEI</creator><creator>LIANG WEIDONG</creator><creator>LI JIANHUI</creator><creator>WEN BAIKAI</creator><creator>ZENG XINRONG</creator><scope>EVB</scope></search><sort><creationdate>20121024</creationdate><title>Method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process</title><author>JIANG WENWEI ; ZHANG ZHANFEI ; LIANG WEIDONG ; LI JIANHUI ; WEN BAIKAI ; ZENG XINRONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102747223A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2012</creationdate><topic>CHEMISTRY</topic><topic>CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>JIANG WENWEI</creatorcontrib><creatorcontrib>ZHANG ZHANFEI</creatorcontrib><creatorcontrib>LIANG WEIDONG</creatorcontrib><creatorcontrib>LI JIANHUI</creatorcontrib><creatorcontrib>WEN BAIKAI</creatorcontrib><creatorcontrib>ZENG XINRONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>JIANG WENWEI</au><au>ZHANG ZHANFEI</au><au>LIANG WEIDONG</au><au>LI JIANHUI</au><au>WEN BAIKAI</au><au>ZENG XINRONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process</title><date>2012-10-24</date><risdate>2012</risdate><abstract>The invention discloses a method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process, comprising the following steps: adding soda and additives into primary tungsten autoclaving slag, carrying out secondary autoclaving at high temperature and pressure; separating the leaching solution from the slag; carrying out primary autoclaving to the tungsten by the leaching solution; separating the primary autoclaving slag from the crude sodium tungstate solution, wherein the primary autoclaving slag is used as the raw material; and mixing the tungstate with the secondary autoclaving leaching solution to prepare slurry. The liquid-solid ratio is controlled to be (3-5):1 in the step of adding the soda and the additives into the primary autoclaving slag and mixing to prepare the slurry, and the soda has the excess coefficient of 2.0-2.5. The liquid-solid ratio is controlled to be (3-5):1 in the step of mixing the tungstate with the secondary autoclaving leaching solution</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN102747223A
source esp@cenet
subjects CHEMISTRY
CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION ORPROCESSING OF GOODS
FERROUS OR NON-FERROUS ALLOYS
GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINSTCLIMATE CHANGE
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Method for extracting tungsten from tungsten mineral by using soda and adopting high-pressure leaching process
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T10%3A55%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=JIANG%20WENWEI&rft.date=2012-10-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102747223A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true