Moderate-temperature brazing filler metal for graphite-base composite material connection and preparation method thereof
The invention provides a moderate-temperature brazing filler metal for graphite-base composite material connection and a preparation method thereof, and relates to a moderate-temperature brazing filler metal and a preparation method thereof. The moderate-temperature brazing filler metal is used for...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHANG LIXIA LI HONGWEI FENG JICAI SHI JUNMIAO TIAN XIAOYU CAO JIAN |
description | The invention provides a moderate-temperature brazing filler metal for graphite-base composite material connection and a preparation method thereof, and relates to a moderate-temperature brazing filler metal and a preparation method thereof. The moderate-temperature brazing filler metal is used for solving the problems that the existing graphite-base composite material is poor in low temperature brazing effect. The moderate-temperature brazing filler metal comprises the following ingredients in parts by weight: 48-53 parts of Ag, 19-32 parts of Cu, 10-28 parts of Sn and 0.1-7 parts of Ti. The method comprises the following steps of 1, weighting all the ingredients, putting the ingredients into a graphite crucible at a ball-to-ingredient mass ratio of (12-16):1, and performing ball milling for 2-6 hours at room temperature and the rotation rate of 280-320r/min (revolutions per minute) in the presence of argon, so as to obtain mixed powder; and 2, pressurizing the mixed powder for 6-10t to obtain foil, performi |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102699571A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102699571A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102699571A3</originalsourceid><addsrcrecordid>eNqNjEsKwkAQBbNxIeod2gME_KCSpQTFja7ch07ykgxMpoeeEcTTOwEP4Oq9gqLm2fsuLZQj8ojRT--loFr5Y1xPnbEWSiMiW-pEqVf2g0l2zQHUyOglJKQxFdQkqRHn0EQjjti15BWeU3TiVBmkpThAId0ym3VsA1a_XWTr6-VZ3nJ4qRA8N3CIVfnYbnbHojictuf9P84XX9hHdA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Moderate-temperature brazing filler metal for graphite-base composite material connection and preparation method thereof</title><source>esp@cenet</source><creator>ZHANG LIXIA ; LI HONGWEI ; FENG JICAI ; SHI JUNMIAO ; TIAN XIAOYU ; CAO JIAN</creator><creatorcontrib>ZHANG LIXIA ; LI HONGWEI ; FENG JICAI ; SHI JUNMIAO ; TIAN XIAOYU ; CAO JIAN</creatorcontrib><description>The invention provides a moderate-temperature brazing filler metal for graphite-base composite material connection and a preparation method thereof, and relates to a moderate-temperature brazing filler metal and a preparation method thereof. The moderate-temperature brazing filler metal is used for solving the problems that the existing graphite-base composite material is poor in low temperature brazing effect. The moderate-temperature brazing filler metal comprises the following ingredients in parts by weight: 48-53 parts of Ag, 19-32 parts of Cu, 10-28 parts of Sn and 0.1-7 parts of Ti. The method comprises the following steps of 1, weighting all the ingredients, putting the ingredients into a graphite crucible at a ball-to-ingredient mass ratio of (12-16):1, and performing ball milling for 2-6 hours at room temperature and the rotation rate of 280-320r/min (revolutions per minute) in the presence of argon, so as to obtain mixed powder; and 2, pressurizing the mixed powder for 6-10t to obtain foil, performi</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20121003&DB=EPODOC&CC=CN&NR=102699571A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20121003&DB=EPODOC&CC=CN&NR=102699571A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG LIXIA</creatorcontrib><creatorcontrib>LI HONGWEI</creatorcontrib><creatorcontrib>FENG JICAI</creatorcontrib><creatorcontrib>SHI JUNMIAO</creatorcontrib><creatorcontrib>TIAN XIAOYU</creatorcontrib><creatorcontrib>CAO JIAN</creatorcontrib><title>Moderate-temperature brazing filler metal for graphite-base composite material connection and preparation method thereof</title><description>The invention provides a moderate-temperature brazing filler metal for graphite-base composite material connection and a preparation method thereof, and relates to a moderate-temperature brazing filler metal and a preparation method thereof. The moderate-temperature brazing filler metal is used for solving the problems that the existing graphite-base composite material is poor in low temperature brazing effect. The moderate-temperature brazing filler metal comprises the following ingredients in parts by weight: 48-53 parts of Ag, 19-32 parts of Cu, 10-28 parts of Sn and 0.1-7 parts of Ti. The method comprises the following steps of 1, weighting all the ingredients, putting the ingredients into a graphite crucible at a ball-to-ingredient mass ratio of (12-16):1, and performing ball milling for 2-6 hours at room temperature and the rotation rate of 280-320r/min (revolutions per minute) in the presence of argon, so as to obtain mixed powder; and 2, pressurizing the mixed powder for 6-10t to obtain foil, performi</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEsKwkAQBbNxIeod2gME_KCSpQTFja7ch07ykgxMpoeeEcTTOwEP4Oq9gqLm2fsuLZQj8ojRT--loFr5Y1xPnbEWSiMiW-pEqVf2g0l2zQHUyOglJKQxFdQkqRHn0EQjjti15BWeU3TiVBmkpThAId0ym3VsA1a_XWTr6-VZ3nJ4qRA8N3CIVfnYbnbHojictuf9P84XX9hHdA</recordid><startdate>20121003</startdate><enddate>20121003</enddate><creator>ZHANG LIXIA</creator><creator>LI HONGWEI</creator><creator>FENG JICAI</creator><creator>SHI JUNMIAO</creator><creator>TIAN XIAOYU</creator><creator>CAO JIAN</creator><scope>EVB</scope></search><sort><creationdate>20121003</creationdate><title>Moderate-temperature brazing filler metal for graphite-base composite material connection and preparation method thereof</title><author>ZHANG LIXIA ; LI HONGWEI ; FENG JICAI ; SHI JUNMIAO ; TIAN XIAOYU ; CAO JIAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102699571A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2012</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG LIXIA</creatorcontrib><creatorcontrib>LI HONGWEI</creatorcontrib><creatorcontrib>FENG JICAI</creatorcontrib><creatorcontrib>SHI JUNMIAO</creatorcontrib><creatorcontrib>TIAN XIAOYU</creatorcontrib><creatorcontrib>CAO JIAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG LIXIA</au><au>LI HONGWEI</au><au>FENG JICAI</au><au>SHI JUNMIAO</au><au>TIAN XIAOYU</au><au>CAO JIAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Moderate-temperature brazing filler metal for graphite-base composite material connection and preparation method thereof</title><date>2012-10-03</date><risdate>2012</risdate><abstract>The invention provides a moderate-temperature brazing filler metal for graphite-base composite material connection and a preparation method thereof, and relates to a moderate-temperature brazing filler metal and a preparation method thereof. The moderate-temperature brazing filler metal is used for solving the problems that the existing graphite-base composite material is poor in low temperature brazing effect. The moderate-temperature brazing filler metal comprises the following ingredients in parts by weight: 48-53 parts of Ag, 19-32 parts of Cu, 10-28 parts of Sn and 0.1-7 parts of Ti. The method comprises the following steps of 1, weighting all the ingredients, putting the ingredients into a graphite crucible at a ball-to-ingredient mass ratio of (12-16):1, and performing ball milling for 2-6 hours at room temperature and the rotation rate of 280-320r/min (revolutions per minute) in the presence of argon, so as to obtain mixed powder; and 2, pressurizing the mixed powder for 6-10t to obtain foil, performi</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN102699571A |
source | esp@cenet |
subjects | CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR PERFORMING OPERATIONS SOLDERING OR UNSOLDERING TRANSPORTING WELDING WORKING BY LASER BEAM |
title | Moderate-temperature brazing filler metal for graphite-base composite material connection and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T23%3A53%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20LIXIA&rft.date=2012-10-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102699571A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |