Flame-retardant slurry

The invention discloses flame-retardant slurry, which belongs to slurry formed through mixing inorganic aggregate and inorganic emulsion, wherein the inorganic aggregate and the inorganic emulsion respectively comprise the following ingredients in percentage by weight: 5 percent of mineral wool, 34...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG DEPING, PAN QUANFU, LI YU, FAN MINGLAN, GENG DACHUN, SONG YAN, LI HUIZHEN, GUO FAYI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG DEPING
PAN QUANFU
LI YU
FAN MINGLAN
GENG DACHUN
SONG YAN
LI HUIZHEN
GUO FAYI
description The invention discloses flame-retardant slurry, which belongs to slurry formed through mixing inorganic aggregate and inorganic emulsion, wherein the inorganic aggregate and the inorganic emulsion respectively comprise the following ingredients in percentage by weight: 5 percent of mineral wool, 34 percent of expanded perlite, 16 percent of hydroxyethyl cellulose with the concentration being 2 percent, 6 percent of rock wool, 5 percent of asbestos plaster, 2 percent of zinc oxide, 3 percent of condensed aluminum phosphate, 20 percent of modified potassium silicate, 9 percent of modified silica sol and 16 percent of hydroxyethyl cellulose with a concentration of 2%. A preparation method comprises the following steps that: firstly, two kinds of inorganic emulsion: the modified potassium silicate and the modified silica sol are respectively added into a container and are uniformly stirred, then, each kind of aggregates and emulsion are respectively added into the container to be mixed into slurry through being s
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN102432264A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN102432264A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN102432264A3</originalsourceid><addsrcrecordid>eNrjZBBzy0nMTdUtSi1JLEpJzCtRKM4pLSqq5GFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgZGJsZGRmYmjsbEqAEAqV4hlQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Flame-retardant slurry</title><source>esp@cenet</source><creator>ZHANG DEPING ; PAN QUANFU ; LI YU ; FAN MINGLAN ; GENG DACHUN ; SONG YAN ; LI HUIZHEN ; GUO FAYI</creator><creatorcontrib>ZHANG DEPING ; PAN QUANFU ; LI YU ; FAN MINGLAN ; GENG DACHUN ; SONG YAN ; LI HUIZHEN ; GUO FAYI</creatorcontrib><description>The invention discloses flame-retardant slurry, which belongs to slurry formed through mixing inorganic aggregate and inorganic emulsion, wherein the inorganic aggregate and the inorganic emulsion respectively comprise the following ingredients in percentage by weight: 5 percent of mineral wool, 34 percent of expanded perlite, 16 percent of hydroxyethyl cellulose with the concentration being 2 percent, 6 percent of rock wool, 5 percent of asbestos plaster, 2 percent of zinc oxide, 3 percent of condensed aluminum phosphate, 20 percent of modified potassium silicate, 9 percent of modified silica sol and 16 percent of hydroxyethyl cellulose with a concentration of 2%. A preparation method comprises the following steps that: firstly, two kinds of inorganic emulsion: the modified potassium silicate and the modified silica sol are respectively added into a container and are uniformly stirred, then, each kind of aggregates and emulsion are respectively added into the container to be mixed into slurry through being s</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120502&amp;DB=EPODOC&amp;CC=CN&amp;NR=102432264A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120502&amp;DB=EPODOC&amp;CC=CN&amp;NR=102432264A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG DEPING</creatorcontrib><creatorcontrib>PAN QUANFU</creatorcontrib><creatorcontrib>LI YU</creatorcontrib><creatorcontrib>FAN MINGLAN</creatorcontrib><creatorcontrib>GENG DACHUN</creatorcontrib><creatorcontrib>SONG YAN</creatorcontrib><creatorcontrib>LI HUIZHEN</creatorcontrib><creatorcontrib>GUO FAYI</creatorcontrib><title>Flame-retardant slurry</title><description>The invention discloses flame-retardant slurry, which belongs to slurry formed through mixing inorganic aggregate and inorganic emulsion, wherein the inorganic aggregate and the inorganic emulsion respectively comprise the following ingredients in percentage by weight: 5 percent of mineral wool, 34 percent of expanded perlite, 16 percent of hydroxyethyl cellulose with the concentration being 2 percent, 6 percent of rock wool, 5 percent of asbestos plaster, 2 percent of zinc oxide, 3 percent of condensed aluminum phosphate, 20 percent of modified potassium silicate, 9 percent of modified silica sol and 16 percent of hydroxyethyl cellulose with a concentration of 2%. A preparation method comprises the following steps that: firstly, two kinds of inorganic emulsion: the modified potassium silicate and the modified silica sol are respectively added into a container and are uniformly stirred, then, each kind of aggregates and emulsion are respectively added into the container to be mixed into slurry through being s</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBBzy0nMTdUtSi1JLEpJzCtRKM4pLSqq5GFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgZGJsZGRmYmjsbEqAEAqV4hlQ</recordid><startdate>20120502</startdate><enddate>20120502</enddate><creator>ZHANG DEPING</creator><creator>PAN QUANFU</creator><creator>LI YU</creator><creator>FAN MINGLAN</creator><creator>GENG DACHUN</creator><creator>SONG YAN</creator><creator>LI HUIZHEN</creator><creator>GUO FAYI</creator><scope>EVB</scope></search><sort><creationdate>20120502</creationdate><title>Flame-retardant slurry</title><author>ZHANG DEPING ; PAN QUANFU ; LI YU ; FAN MINGLAN ; GENG DACHUN ; SONG YAN ; LI HUIZHEN ; GUO FAYI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN102432264A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2012</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG DEPING</creatorcontrib><creatorcontrib>PAN QUANFU</creatorcontrib><creatorcontrib>LI YU</creatorcontrib><creatorcontrib>FAN MINGLAN</creatorcontrib><creatorcontrib>GENG DACHUN</creatorcontrib><creatorcontrib>SONG YAN</creatorcontrib><creatorcontrib>LI HUIZHEN</creatorcontrib><creatorcontrib>GUO FAYI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG DEPING</au><au>PAN QUANFU</au><au>LI YU</au><au>FAN MINGLAN</au><au>GENG DACHUN</au><au>SONG YAN</au><au>LI HUIZHEN</au><au>GUO FAYI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Flame-retardant slurry</title><date>2012-05-02</date><risdate>2012</risdate><abstract>The invention discloses flame-retardant slurry, which belongs to slurry formed through mixing inorganic aggregate and inorganic emulsion, wherein the inorganic aggregate and the inorganic emulsion respectively comprise the following ingredients in percentage by weight: 5 percent of mineral wool, 34 percent of expanded perlite, 16 percent of hydroxyethyl cellulose with the concentration being 2 percent, 6 percent of rock wool, 5 percent of asbestos plaster, 2 percent of zinc oxide, 3 percent of condensed aluminum phosphate, 20 percent of modified potassium silicate, 9 percent of modified silica sol and 16 percent of hydroxyethyl cellulose with a concentration of 2%. A preparation method comprises the following steps that: firstly, two kinds of inorganic emulsion: the modified potassium silicate and the modified silica sol are respectively added into a container and are uniformly stirred, then, each kind of aggregates and emulsion are respectively added into the container to be mixed into slurry through being s</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN102432264A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Flame-retardant slurry
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T23%3A51%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20DEPING&rft.date=2012-05-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN102432264A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true