Waste rubber powder/waste plastics/SBS composite modified asphalt and preparation method thereof

The invention discloses waste rubber powder/waste plastics/SBS composite modified asphalt and a preparation method thereof, wherein the waste rubber powder/waste plastics/SBS composite modified asphalt comprises the following ingredients in mass percent: 80 to 88 percent of substrate asphalt, 5 to 1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MENG CHAOFENG, PENG YIMIN, DENG JIANRU, MA JIE, HU BO, LUO ZHENYU, CHENG SHENG, KUANG JINGUO, XIAO YUHUI, NIU HAIGANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MENG CHAOFENG
PENG YIMIN
DENG JIANRU
MA JIE
HU BO
LUO ZHENYU
CHENG SHENG
KUANG JINGUO
XIAO YUHUI
NIU HAIGANG
description The invention discloses waste rubber powder/waste plastics/SBS composite modified asphalt and a preparation method thereof, wherein the waste rubber powder/waste plastics/SBS composite modified asphalt comprises the following ingredients in mass percent: 80 to 88 percent of substrate asphalt, 5 to 15 percent of waste rubber powder, 1 to 5 percent of waste plastics, 1 to 3 percent of SBS and 0 to 0.5 percent of cross linking agents. The preparation method comprises the following steps: heating the waste plastics at the temperature between 120 and 150 DEG C to be dissolved into the substrate asphalt; then, raising the temperature to 180 to 200 DEG C; proportionally adding the waste rubber powder, the SBS and the cross linking agents; and stirring and dispersing the materials for 0.5 to 3.0 hours under the simple stirring conditions to obtain the rubber powder/waste plastics/SBS composite modified asphalt. The invention has the advantages of environment protection, energy saving, low cost, simple equipment, easy
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101812234BB</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101812234BB</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101812234BB3</originalsourceid><addsrcrecordid>eNqNysEKgkAURmE3LaJ6h0v7MLVFa6Vo1cagpV2df3BAvZeZCV8_iR6g1YGPs05eTw4R5N9tC08qs4FP56_psMR1Ia3LmjoZVYJbeBTjrIMhDtrzEIknQ-qh7Dk6mWhE7MVQ7OEhdpusLA8Bu183yf56eVS3A1QaBOUOE2JT3bNjds7yvDiVZfHX9AFtIz4m</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Waste rubber powder/waste plastics/SBS composite modified asphalt and preparation method thereof</title><source>esp@cenet</source><creator>MENG CHAOFENG ; PENG YIMIN ; DENG JIANRU ; MA JIE ; HU BO ; LUO ZHENYU ; CHENG SHENG ; KUANG JINGUO ; XIAO YUHUI ; NIU HAIGANG</creator><creatorcontrib>MENG CHAOFENG ; PENG YIMIN ; DENG JIANRU ; MA JIE ; HU BO ; LUO ZHENYU ; CHENG SHENG ; KUANG JINGUO ; XIAO YUHUI ; NIU HAIGANG</creatorcontrib><description>The invention discloses waste rubber powder/waste plastics/SBS composite modified asphalt and a preparation method thereof, wherein the waste rubber powder/waste plastics/SBS composite modified asphalt comprises the following ingredients in mass percent: 80 to 88 percent of substrate asphalt, 5 to 15 percent of waste rubber powder, 1 to 5 percent of waste plastics, 1 to 3 percent of SBS and 0 to 0.5 percent of cross linking agents. The preparation method comprises the following steps: heating the waste plastics at the temperature between 120 and 150 DEG C to be dissolved into the substrate asphalt; then, raising the temperature to 180 to 200 DEG C; proportionally adding the waste rubber powder, the SBS and the cross linking agents; and stirring and dispersing the materials for 0.5 to 3.0 hours under the simple stirring conditions to obtain the rubber powder/waste plastics/SBS composite modified asphalt. The invention has the advantages of environment protection, energy saving, low cost, simple equipment, easy</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20111012&amp;DB=EPODOC&amp;CC=CN&amp;NR=101812234B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20111012&amp;DB=EPODOC&amp;CC=CN&amp;NR=101812234B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MENG CHAOFENG</creatorcontrib><creatorcontrib>PENG YIMIN</creatorcontrib><creatorcontrib>DENG JIANRU</creatorcontrib><creatorcontrib>MA JIE</creatorcontrib><creatorcontrib>HU BO</creatorcontrib><creatorcontrib>LUO ZHENYU</creatorcontrib><creatorcontrib>CHENG SHENG</creatorcontrib><creatorcontrib>KUANG JINGUO</creatorcontrib><creatorcontrib>XIAO YUHUI</creatorcontrib><creatorcontrib>NIU HAIGANG</creatorcontrib><title>Waste rubber powder/waste plastics/SBS composite modified asphalt and preparation method thereof</title><description>The invention discloses waste rubber powder/waste plastics/SBS composite modified asphalt and a preparation method thereof, wherein the waste rubber powder/waste plastics/SBS composite modified asphalt comprises the following ingredients in mass percent: 80 to 88 percent of substrate asphalt, 5 to 15 percent of waste rubber powder, 1 to 5 percent of waste plastics, 1 to 3 percent of SBS and 0 to 0.5 percent of cross linking agents. The preparation method comprises the following steps: heating the waste plastics at the temperature between 120 and 150 DEG C to be dissolved into the substrate asphalt; then, raising the temperature to 180 to 200 DEG C; proportionally adding the waste rubber powder, the SBS and the cross linking agents; and stirring and dispersing the materials for 0.5 to 3.0 hours under the simple stirring conditions to obtain the rubber powder/waste plastics/SBS composite modified asphalt. The invention has the advantages of environment protection, energy saving, low cost, simple equipment, easy</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNysEKgkAURmE3LaJ6h0v7MLVFa6Vo1cagpV2df3BAvZeZCV8_iR6g1YGPs05eTw4R5N9tC08qs4FP56_psMR1Ia3LmjoZVYJbeBTjrIMhDtrzEIknQ-qh7Dk6mWhE7MVQ7OEhdpusLA8Bu183yf56eVS3A1QaBOUOE2JT3bNjds7yvDiVZfHX9AFtIz4m</recordid><startdate>20111012</startdate><enddate>20111012</enddate><creator>MENG CHAOFENG</creator><creator>PENG YIMIN</creator><creator>DENG JIANRU</creator><creator>MA JIE</creator><creator>HU BO</creator><creator>LUO ZHENYU</creator><creator>CHENG SHENG</creator><creator>KUANG JINGUO</creator><creator>XIAO YUHUI</creator><creator>NIU HAIGANG</creator><scope>EVB</scope></search><sort><creationdate>20111012</creationdate><title>Waste rubber powder/waste plastics/SBS composite modified asphalt and preparation method thereof</title><author>MENG CHAOFENG ; PENG YIMIN ; DENG JIANRU ; MA JIE ; HU BO ; LUO ZHENYU ; CHENG SHENG ; KUANG JINGUO ; XIAO YUHUI ; NIU HAIGANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101812234BB3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2011</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>MENG CHAOFENG</creatorcontrib><creatorcontrib>PENG YIMIN</creatorcontrib><creatorcontrib>DENG JIANRU</creatorcontrib><creatorcontrib>MA JIE</creatorcontrib><creatorcontrib>HU BO</creatorcontrib><creatorcontrib>LUO ZHENYU</creatorcontrib><creatorcontrib>CHENG SHENG</creatorcontrib><creatorcontrib>KUANG JINGUO</creatorcontrib><creatorcontrib>XIAO YUHUI</creatorcontrib><creatorcontrib>NIU HAIGANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MENG CHAOFENG</au><au>PENG YIMIN</au><au>DENG JIANRU</au><au>MA JIE</au><au>HU BO</au><au>LUO ZHENYU</au><au>CHENG SHENG</au><au>KUANG JINGUO</au><au>XIAO YUHUI</au><au>NIU HAIGANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Waste rubber powder/waste plastics/SBS composite modified asphalt and preparation method thereof</title><date>2011-10-12</date><risdate>2011</risdate><abstract>The invention discloses waste rubber powder/waste plastics/SBS composite modified asphalt and a preparation method thereof, wherein the waste rubber powder/waste plastics/SBS composite modified asphalt comprises the following ingredients in mass percent: 80 to 88 percent of substrate asphalt, 5 to 15 percent of waste rubber powder, 1 to 5 percent of waste plastics, 1 to 3 percent of SBS and 0 to 0.5 percent of cross linking agents. The preparation method comprises the following steps: heating the waste plastics at the temperature between 120 and 150 DEG C to be dissolved into the substrate asphalt; then, raising the temperature to 180 to 200 DEG C; proportionally adding the waste rubber powder, the SBS and the cross linking agents; and stirring and dispersing the materials for 0.5 to 3.0 hours under the simple stirring conditions to obtain the rubber powder/waste plastics/SBS composite modified asphalt. The invention has the advantages of environment protection, energy saving, low cost, simple equipment, easy</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN101812234BB
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
title Waste rubber powder/waste plastics/SBS composite modified asphalt and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T20%3A30%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MENG%20CHAOFENG&rft.date=2011-10-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101812234BB%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true